# US 11,118,024 B2 · Method for producing three-dimensional ordered porous microstructure and monolithic column produced thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,024 B2
- Document ID: US11118024B2
- Status: Granted
- Kind: B2
- Application number: 15/699,350
- Filed: 2017-09-08
- Published: 2019-03-14
- Granted: 2021-09-14
- Earliest claimed: 2017-09-08
- Assignees: Tantti Laboratory Inc.
- Applicants: Tantti Laboratory Inc.
- Inventors: Chen-Hung Liao; Yu-Cheng Kuo; Yu Cheng; Shih-Horng Yang
- Web page: https://patentgrep.com/patent/US11118024B2

## CPC

- C08J 9/26: by elimination of a solid phase from a macromolecular composition or article, e.g. leaching out
- B01J 20/28042: {Shaped bodies; Monolithic structures}
- B01J 20/28085: {being more than 50 nm, i.e. macropores}
- B01J 20/28092: {Bimodal, polymodal, different types of pores or different pore size distributions in different parts of the sorbent}
- B01J 20/28095: {Shape or type of pores, voids, channels, ducts}
- B01J 20/3057: {Use of a templating or imprinting material (molecularly imprinted polymers B01J20/268); filling pores of a substrate or matrix followed by the removal of the substrate or matrix}
- B01J 20/3208: {Polymeric carriers, supports or substrates}
- B01J 20/327: {Polymers obtained by reactions involving only carbon to carbon unsaturated bonds}
- B01J 20/3293: {Coatings on a core, the core being particle or fiber shaped, e.g. encapsulated particles, coated fibers}
- B01J 13/14: Polymerisation; cross-linking
- C08J 2201/0462: using organic solvents
- C08J 2201/0464: using water or inorganic fluids
- C08J 2325/14: with unsaturated esters
- C08J 2333/04: esters
- C08J 2351/00: Characterised by the use of graft polymers in which the grafted component is obtained by reactions only involving carbon-to-carbon unsaturated bonds; Derivatives of such polymers
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

The present invention relates to a method for producing a three-dimensional ordered porous microstructure. In the method of the invention where the three-dimensional ordered microstructure is produced using the colloidal crystal templating process, the three-dimensional ordered microstructure thus formed is subjected to heat treatment to soften the particles, so as to effectively increase the contact between orderly arranged particles while removing the solvent used to suspend the particles. The present invention further relates to a monolithic column produced thereby. Compared to the monolithic columns produced by conventional methods, the monolithic column according to the invention is characterized in having a higher aspect ratio and a higher pore regularity, while the connecting pores in the column are relatively large in pore size.

## Claims

### Claim 1

A method for producing a three-dimensional ordered porous microstructure, comprising the steps of:
A. forming a three-dimensional ordered microstructure of substantially spherical particles made of polymeric material selected from the group consisting of a styrene-butyl methacrylate copolymer and a styrene-butyl acrylate copolymer by suspending the particles in a solvent of methanol and water and then allowing the particles to undergo self-assembling, so that interstitial voids are formed between the particles, wherein the particles have a glass transition temperature ranging from 50° C. to 95° C.;
B. heating the substantially spherical particles in the three-dimensional ordered microstructure at a temperature lower than the glass transition temperature by about 3 to 15° C. to soften the particles, so that the respective particles are deformed to have a longest radius R and a shortest radius r, where r/R ratio is greater than √{square root over (3/2)} but smaller than 1, and the solvent is concurrently evaporated from the three-dimensional ordered microstructure, wherein the solvent has a boiling point substantially higher than the temperature at which the particles are heated, so that the solvent is evaporated without being boiled;
C. filling an inverse opal material into the interstitial voids; and
D. removing the three-dimensional ordered microstructure to obtain the three-dimensional ordered porous microstructure.

### Claim 2 (depends on 1)

The method for producing a three-dimensional ordered porous microstructure according to claim 1, wherein the step B comprises heating the three-dimensional ordered microstructure at a temperature lower than the glass transition temperature by about 3 to 10° C.

### Claim 3 (depends on 1)

The method for producing a three-dimensional ordered porous microstructure according to claim 1, wherein the particles are homogeneous spherical particles, and the glass transition temperature is the bulk glass transition temperature of the particles.

### Claim 4 (depends on 1)

The method for producing a three-dimensional ordered porous microstructure according to claim 1, wherein the particles have a core-shell architecture comprising a core and a shell covering the core, with the core and the shell being made of substantially different polymeric materials, and wherein the glass transition temperature is the glass transition temperature of the shell.

### Claim 5 (depends on 1)

The method for producing a three-dimensional ordered porous microstructure according to claim 1, wherein the step D comprises removing the three-dimensional ordered microstructure by a process selected from the group consisting of Soxhlet extraction and supercritical fluid extraction.

### Claim 6 (depends on 1)