# US 11,118,022 B2 · Sizing agent coated carbon fiber, method for producing sizing agent coated carbon fiber, carbon fiber reinforced composite material, and method for producing carbon fiber reinforced composite material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,022 B2
- Document ID: US11118022B2
- Status: Granted
- Kind: B2
- Application number: 15/528,711
- Filed: 2016-01-13
- Published: 2018-12-06
- Granted: 2021-09-14
- Earliest claimed: 2015-03-06
- Assignees: Toray Industries, Inc.
- Applicants: Toray Industries, Inc.
- Inventors: Tomoko Ichikawa; Kazuki Yoshihiro; Hisafumi Mizuta; Makoto Endo
- Web page: https://patentgrep.com/patent/US11118022B2

## CPC

- C08J 5/06: using pretreated fibrous materials
- B32B 5/022: {Non-woven fabric}
- B32B 5/024: {Woven fabric}
- B32B 27/12: next to a fibrous or filamentary layer
- B32B 37/10: characterised by the pressing technique, e.g. using action of vacuum or fluid pressure
- C08J 5/248: {using pre-treated fibres}
- C08J 5/249: {characterised by the additives used in the prepolymer mixture}
- C25D 11/02: Anodisation
- D06M 13/11: Compounds containing epoxy groups or precursors thereof
- D06M 13/148: Polyalcohols, e.g. glycerol {or glucose}
- D06M 13/165: Ethers (D06M13/11 takes precedence)
- D06M 13/52: combined with mechanical treatment
- D06M 15/59: Polyamides; Polyimides
- D06M 15/63: containing sulfur in the main chain, e.g. polysulfones
- D06M 15/70: combined with mechanical treatment
- B32B 2260/023: Two or more layers
- B32B 2260/046: Synthetic resin
- B32B 2262/106: Carbon fibres, e.g. graphite fibres
- B32B 2305/076: Prepregs
- B32B 2305/188: Woven fabrics
- B32B 2305/20: in the form of a non-woven mat
- B32B 2305/74: Partially cured
- B32B 2307/202: Conductive
- B32B 2307/206: Insulating
- B32B 2310/021: using electrical effects (B32B2310/08 and B32B2310/12 take precedence)
- B32B 2310/0418: other than water
- B32B 2313/04: Carbon
- B32B 2363/00: Epoxy resins
- C08J 2381/02: Polythioethers; Polythioether-ethers
- C08J 2381/06: Polysulfones; Polyethersulfones
- D01F 9/12: Carbon filaments; Apparatus specially adapted for the manufacture thereof
- D06M 2101/40: Fibres of carbon
- D06M 2200/40: Reduced friction resistance, lubricant properties; Sizing compositions
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS

## Abstract

Sizing agent coated carbon fibers obtained by coating carbon fibers with a sizing agent comprising at least one of (A) to (C) in a total amount of 80 mass % or more with respect to the whole sizing agent, the carbon fibers each having a surface layer which has a thickness of 10 nm or larger and has an oxygen content of 4% or higher with respect to all the elements, wherein when the sizing agent coated carbon fibers are subjected three times to a 10-minute ultrasonic treatment in an acetone solvent, then the amount of the remaining sizing agent is 0.1-0.25 parts by mass per 100 parts by mass of the sizing agent coated carbon fibers. (A) At least one polymer selected from the group consisting of polyimides, polyetherimides, and polysulfones (B) A compound having a terminal unsaturated group and a polar group in the molecule (C) A polyether-type aliphatic epoxy compound and/or a polyol-type aliphatic epoxy compound which each have an epoxy equivalent of 250 g/eq or less and have two or more epoxy groups in the molecule.

## Claims

### Claim 1

A sizing agent coated carbon fiber comprising a carbon fiber coated with a sizing agent, wherein
the sizing agent coated carbon fiber has a volume-specific resistance of 300 Ωcm or more,
the carbon fiber is polyacrylonitrile-based,
upon subjecting the carbon fiber cross-section to energy-dispersive X-ray spectroscopy, a high oxygen concentration layer is detected wherein
the proportion of oxygen relative to the total of all elements is 4% or more in a thickness of 10 nm or more and 30 nm or less from the carbon fiber surface, and
the proportion of oxygen relative to the total of all elements is less than 4% below the high oxygen concentration layer,
the sizing agent contains (A) to (C) in a total amount of 80 mass % or more relative to the total amount of the sizing agent,
upon subjecting the sizing agent coated carbon fiber to a 10-minute ultrasonic treatment in an acetone solvent three times, the amount of non-eluted sizing agent remaining on the carbon fiber is 0.1 parts by mass or more and 0.25 parts by mass or less per 100 parts by mass of the sizing agent coated carbon fiber, wherein (A), (B) and (C) are as follows:
(A) at least one member selected from the group consisting of polyimide, polyetherimide, and polysulfone,
(B) a compound having a terminal unsaturated group and a polar group in a molecule, and
(C) a polyether-type aliphatic epoxy compound and/or polyol-type aliphatic epoxy compound having an epoxy equivalent of 250 g/eq. or less and having two or more epoxy groups in a molecule, and
wherein the ratio (β)/(α) between the following (α) and (β) is 0.8 or more as determined by X-ray photoelectron spectroscopy using AlKα1,2:
(α): surface oxygen concentration (O/C) that is the ratio of the number of atoms of oxygen (O) to that of carbon (C) on the carbon fiber surface measured at a photoelectron take-off angle of 10°, and
(β): surface oxygen concentration (O/C) that is the ratio of the number of atoms of oxygen (O) to that of carbon (C) on the carbon fiber surface measured at a photoelectron take-off angle of 90°.

### Claim 2 (depends on 1)

The sizing agent coated carbon fiber according to claim 1, wherein the polyether-type aliphatic epoxy compound and/or polyol-type aliphatic epoxy compound (C) is a glycidyl-ether-type epoxy compound obtained by the reaction of at least one member selected from the group consisting of glycerol, diglycerol, polyglycerol, trimethylolpropane, pentaerythritol, sorbitol, and arabitol with epichlorohydrin.

### Claim 3 (depends on 1)

The sizing agent coated carbon fiber according to claim 1, wherein the sizing agent coated carbon fiber has a single-yarn fineness of 0.5 dtex or less.

### Claim 4 (depends on 1)

The sizing agent coated carbon fiber according to claim 1, wherein the twist of the sizing agent coated carbon fiber is not more than 1 turn meter.

### Claim 5 (depends on 1)

A method for producing a sizing agent coated carbon fiber according to claim 1, wherein the method comprises coating a carbon fiber with a sizing agent, followed by a heat treatment at 240° C. or more for 60 to 3,000 seconds.

### Claim 6 (depends on 5)

The method for producing a sizing agent coated carbon fiber according to claim 5, wherein the carbon fiber is subjected to liquid-phase electrolytic oxidation at a current density of 5 A/m2 or less.

### Claim 7 (depends on 6)

The method for producing a sizing agent coated carbon fiber according to claim 6, wherein the liquid-phase electrolytic oxidation is performed at 40° C. or more.

### Claim 8 (depends on 1)

A prepreg obtainable by impregnating the sizing agent coated carbon fiber according to claim 1 with a thermosetting resin.

### Claim 9 (depends on 8)

A carbon fiber reinforced composite material obtainable by curing the prepreg according to claim 8.

### Claim 10 (depends on 1)

A carbon fiber reinforced resin composition comprising:
the sizing agent coated carbon fiber according to claim 1; and
a matrix resin including a thermoplastic resin or a radically polymerizable resin.

### Claim 11 (depends on 10)

The carbon fiber reinforced resin composition according to claim 10, wherein the matrix resin is at least one member selected from a polyimide resin, a polyetherimide resin, a polyarylene sulfide resin, a polycarbonate resin, a polyolefin resin, and a polyamide resin.

### Claim 12 (depends on 5)

A method for producing a carbon fiber reinforced resin composition, comprising:
a step of producing a sizing agent coated carbon fiber by the method according to claim 5; and
a step of blending the sizing agent coated carbon fiber with a matrix resin.

### Claim 13 (depends on 10)

A carbon fiber reinforced resin composition, comprising the carbon fiber reinforced resin composition according to claim 10 and being a molding material in any one of the following forms (D), (E), (F), and (G):
molding material (D): a columnar molding material, in which the carbon fiber is arranged such that the difference in angle between the axial direction thereof and the major axis line of the molding material is 20° or less, the content of carbon fiber having a length of 50% or less of the length of the molding material is 30 mass % or less, and the average two-dimensional orientation angle defined by a single fiber of the carbon fiber forming the molding material and another single fiber of the carbon fiber closest thereto is 10 to 80°,
molding material (E): a molding material, in which the carbon fiber is in the form of a single fiber and substantially two-dimensionally oriented,
molding material (F): a molding material in which the carbon fiber is in the form of a bundle and substantially two-dimensionally oriented,
molding material (G): a prepreg.

### Claim 14 (depends on 13)

The carbon fiber reinforced resin molded article obtainable by molding the carbon fiber reinforced resin composition according to claim 13.

### Claim 15 (depends on 1)

A laminated prepreg comprising:
at least two plies of a carbon fiber layer (b) containing a sizing agent coated carbon fiber (a); and
a layer of a polymer resin (c) disposed between the two plies,
the laminated prepreg being configured such that
(i) the sizing agent coated carbon fiber (a) is the sizing agent coated carbon fiber according to claim 1, and
(ii) a composite material having an interlayer structure obtainable by solidifying the laminated prepreg has a volume-specific resistance of 500 Ω·m or more in the thickness direction of the laminated prepreg.

### Claim 16 (depends on 15)

The laminated prepreg according to claim 15, wherein the ratio T1/T2 between the average thickness T1 of the carbon fiber layer (b) and the average thickness T2 of the layer of a polymer resin (c) in the composite material is 9 or less.

### Claim 17 (depends on 15)

The laminated prepreg according to claim 15, wherein the layer of a polymer resin (c) contains a thermosetting resin and a curing agent in a total amount 50 parts by mass or more per 100 parts by mass of the polymer resin in the layer.

### Claim 18 (depends on 15)

The laminated prepreg according to claim 15, wherein the layer of a polymer resin (c) contains at least one thermoplastic resin selected from the group consisting of particles, fibers, and a film of a thermoplastic resin.

### Claim 19 (depends on 18)

The laminated prepreg according to claim 18, wherein the thermoplastic resin is contained in an amount of 5 to 30 mass % or more relative to the total amount of the polymer resin contained in the laminated prepreg.

### Claim 20 (depends on 15)

The laminated prepreg according to claim 15, wherein the carbon fiber volume fraction in the composite material is 60 to 70%.

### Claim 21 (depends on 15)

A method for producing a laminated prepreg, being a method for producing the laminated prepreg according to claim 15, wherein the sizing agent coated carbon fiber (a) is obtained through a step of coating a carbon fiber with a sizing agent, followed by a heat treatment at 240° C. or more for 60 to 3,000 seconds.

### Claim 22 (depends on 15)

A method for producing a laminated prepreg, being a method for producing the laminated prepreg according to claim 15, wherein the sizing agent coated carbon fiber (a) is obtained through a step of coating a carbon fiber that has been subjected to liquid-phase electrolytic oxidation at a current density of 5 A/m2 or less with a sizing agent.

### Claim 23 (depends on 15)

A method for producing a laminated prepreg, being a method for producing the laminated prepreg according to claim 15, wherein the sizing agent coated carbon fiber (a) is obtained through a step of coating a carbon fiber that has been subjected to liquid-phase electrolytic oxidation at 40° C. or more with a sizing agent.

### Claim 24 (depends on 15)

A method for producing a composite material having an interlayer structure, comprising a step of solidifying the laminated prepreg according to claim 15.

### Claim 25 (depends on 21)

A method for producing a composite material having an interlayer structure, comprising, after obtaining a laminated prepreg by the method according to claim 21, a step of solidifying the laminated prepreg.