# US 11,118,019 B2 · Thermoplastic polyurethane particles having low impurity content and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,019 B2
- Document ID: US11118019B2
- Status: Granted
- Kind: B2
- Application number: 16/491,397
- Filed: 2018-03-09
- Published: 2020-01-30
- Granted: 2021-09-14
- Earliest claimed: 2017-03-09
- Assignees: LG Hausys, Ltd.
- Applicants: LG Hausys, Ltd.
- Inventors: Min Gyung Kim; Sung Yong Kang; Kyoung Min Kang; Hee-Jung Lee; Chang-Young Park; Jae Ho Lim; Jun Ho Choi; Jae Han Song; Yu Jin Go
- Web page: https://patentgrep.com/patent/US11118019B2

## CPC

- C08J 3/12: Powdering or granulating
- B01J 2/04: in a gaseous medium {(if combined with suspending the material in a gas, e.g. fluidised beds B01J2/16)}
- B01J 2/20: by expressing the material, e.g. through sieves and fragmenting the extruded length
- B29B 9/10: by moulding the material, i.e. treating it in the molten state
- B29B 9/12: characterised by structure or composition
- C08G 63/06: derived from hydroxycarboxylic acids
- C08G 63/08: Lactones or lactides
- C08L 67/04: Polyesters derived from hydroxycarboxylic acids, e.g. lactones (C08L67/06 takes precedence)
- C08L 75/04: Polyurethanes
- B29B 2009/125: {Micropellets, microgranules, microparticles}
- B29K 2067/046: {PLA, i.e. polylactic acid or polylactide}
- C08J 2367/04: Polyesters derived from hydroxy carboxylic acids, e.g. lactones (C08J2367/06 takes precedence)
- C08J 2375/04: Polyurethanes
- C08L 2203/30: used for thermoforming
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The present invention provides thermoplastic polyurethane particles, which are formed in a continuous matrix phase from a thermoplastic polyurethane resin and have a particle diameter of 200-500 μm. In a differential scanning calorimetry (DSC) curve of the thermoplastic polyurethane particles, derived from the analysis of a temperature rise of 10° C./min by DSC, a peak of the cold crystallization temperature (Tcc) is shown at a temperature between the glass transition temperature (Tg) and the melting point (Tm). The thermoplastic polyurethane particles have a compression degree of 10-20%.

## Claims

### Claim 1

Thermoplastic polyurethane particles which are formed as a continuous matrix from a thermoplastic polyurethane resin and have a particle diameter of 200 to 500 μM, wherein an impurity content of the thermoplastic polyurethane particles is 50 ppm or less.

### Claim 2 (depends on 1)

The thermoplastic polyurethane particles according to claim 1, wherein the thermoplastic polyurethane particles have a peak of cold crystallization temperature (Tcc) at a temperature between a glass transition temperature (Tg) and a melting point (Tm) in the differential scanning calorimetry (DSC) curve derived from temperature rise analysis of 10° C./min by the DSC.

### Claim 3 (depends on 1)

The thermoplastic polyurethane particles according to claim 1, wherein the thermoplastic polyurethane particles have an aspect ratio of 1.00 or more and less than 1.05, calculated by Formula 1 below, and a roundness of 0.95 to 1.00, calculated by Formula 2 below:
Aspect ratio=major axis/minor axis, [Formula 1]
Roundness=4×area/(π×major axis{circumflex over ( )}2). [Formula 2]

### Claim 4 (depends on 1)

The thermoplastic polyurethane particles according to claim 1, wherein the thermoplastic polyurethane particles have a compression degree of 10 to 20%, calculated by Formula 3 below:
Compression degree=(compressed bulk density-relaxed bulk density)/compressed bulk density×100. [Formula 3]

### Claim 5 (depends on 4)

The thermoplastic polyurethane particles according to claim 4, wherein the thermoplastic polyurethane particles have a compressed bulk density of 0.45 to 0.5 g/cm3.

### Claim 6 (depends on 1)

The thermoplastic polyurethane particles according to claim 1, wherein the thermoplastic polyurethane particles have a flow time of 10 to 20 seconds.