# US 11,118,015 B2 · Laminate for manufacturing flexible substrate and method for manufacturing flexible substrate by using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,015 B2
- Document ID: US11118015B2
- Status: Granted
- Kind: B2
- Application number: 16/461,619
- Filed: 2018-01-19
- Published: 2020-02-27
- Granted: 2021-09-14
- Earliest claimed: 2017-01-31
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Hye Won Jeong; Cheolmin Yun; Kyungjun Kim; Bora Shin
- Web page: https://patentgrep.com/patent/US11118015B2

## CPC

- C08G 73/1039: {comprising halogen-containing substituents}
- C08G 73/14: Polyamide-imides
- B32B 43/006: {Delaminating}
- C08G 73/1067: {Wholly aromatic polyimides, i.e. having both tetracarboxylic and diamino moieties aromatically bound}
- C09D 179/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

The laminate for manufacturing a flexible substrate according to the present invention is formed by using a polyimide having a high absorbance to a UV laser in an organic sacrificial layer for delaminating a flexible substrate from a carrier substrate. Therefore, it is possible that the laser energy density required in the delaminating process using laser irradiation is reduced and the amount of as generated by the delaminating process is remarkably reduced so that the efficiency of the process, the permeability of the flexible substrate is improved and the reliability of the device is improved.

## Claims

### Claim 1

A laminate for manufacturing a flexible substrate comprising:
a carrier substrate;
an organic sacrificial layer disposed on one side of the carrier substrate and containing a polyimide resin having an amide bond (—C(O)NH—) in the molecular structure; and
a flexible substrate layer disposed on the organic sacrificial layer,
wherein the adhesion of the organic sacrificial layer to the flexible substrate layer is reduced by a UV laser,
wherein the polyimide is formed from at least one diamine selected from the following formulae 3a to 3c and at least one tetracarboxylic anhydride:
in formulae 3a to 3c,
R21 to R29 are each independently a substituent selected from a halogen atom, a thiol group (—SH), a nitro group (—NO2), a cyano group (—CN), an alkyl group having 1 to 10 carbon atoms, a halogenoalkoxy group having 1 to 4 carbon atoms, a halogenoalkyl group having 1 to 10 carbon atoms and an aryl group having 6 to 20 carbon atoms,
b1 to b9 are each independently an integer of 0 to 4, and
wherein an energy density (E/D) of a UV laser at which the adhesion of the organic sacrificial layer to the carrier substrate changes is 220 mJ/cm2 or less.

### Claim 2 (depends on 1)

The laminate for manufacturing a flexible substrate according to claim 1, wherein the organic sacrificial layer containing the polyimide resin has a UV transmittance of 30% or less at a wavelength of 200 nm to 350 nm when the thickness is 100 nm.

### Claim 3 (depends on 1)

The laminate for manufacturing a flexible substrate according to claim 1, wherein the polyimide contained in the organic sacrificial layer comprises at least one repeating structure selected from the following formulae 4a to 4c:

### Claim 4 (depends on 1)

The laminate for manufacturing a flexible substrate according to claim 1, wherein the flexible substrate contains a polyimide.

### Claim 5 (depends on 4)

The laminate for manufacturing a flexible substrate according to claim 4, wherein the polyimide contained in the flexible substrate further comprises a diamine of the following formula 5:
in formula 5,
R31 and R32 are each independently a substituent selected from a halogen atom, a hydroxyl group (—OH), a thiol group (—SH), a nitro group (—NO2), a cyano group, an alkyl group having 1 to 10 carbon atoms, a halogenoalkoxy group having 1 to 4 carbon atoms, a halogenoalkyl group having 1 to 10 carbon atoms and an aryl group having 6 to 20 carbon atoms,
n and m are each independently an integer of 0 to 4, and
Q1 is selected from the group consisting of a single bond, —O—, —CR18R19—, —C(═O)—, —C(═O)O—, —S—, —SO2—, a phenylene group and a combination thereof, wherein R18 and R19 are each independently selected from the group consisting of a hydrogen atom, an alkyl group having 1 to 10 carbon atoms, and a fluoroalkyl group having 1 to 10 carbon atoms.

### Claim 6 (depends on 5)

The laminate for manufacturing a flexible substrate according to claim 5, wherein the polyimide contained in the flexible substrate comprises a repeating structure of the following formula 7:
in formula 7, R31, R32, n, m and Q1 are the same as those defined in formula 5.

### Claim 7 (depends on 1)

The laminate for manufacturing a flexible substrate according to claim 1, wherein the laminate further comprises, on the organic sacrificial layer, at least one functional additional layer selected from the group of a barrier layer and a metal layer.

### Claim 8 (depends on 1)

The laminate for manufacturing a flexible substrate according to claim 1, wherein the polyimide contained in the organic sacrificial layer has a coefficient of thermal expansion (CTE) of 0 to 20 ppm/° C. in the temperature range of 30 to 500° C.

### Claim 9

A method of manufacturing a flexible substrate, comprising the steps of:
applying and coating a polyimide precursor solution comprising an amide bond (—C(O)NH—) in the molecular structure on a carrier substrate to form an organic sacrificial layer containing a polyimide;
forming a flexible substrate layer on the organic sacrificial layer by using a UV laser; and
performing laser lift-off for delaminating the flexible substrate layer from the carrier substrate on which the organic sacrificing layer is formed,
wherein the polyimide is formed from at least one diamine selected from the following formulae 3a to 3c and at least one tetracarboxylic anhydride:
in formulae 3a to 3c,
R21 to R29 are each independently a substituent selected from a halogen atom, a thiol group (—SH), a nitro group (—NO2), a cyano group (—CN), an alkyl group having 1 to 10 carbon atoms, a halogenoalkoxy group having 1 to 4 carbon atoms, a halogenoalkyl group having 1 to 10 carbon atoms and an aryl group having 6 to 20 carbon atoms,
b1 to b9 are each independently an integer of 0 to 4, and
wherein an energy density (E/D) of a UV laser at which the adhesion of the organic sacrificial layer to the carrier substrate changes is 220 mJ/cm2 or less.

### Claim 10 (depends on 9)

The method of manufacturing a flexible substrate according to claim 9, wherein the method further comprises forming, on the organic sacrificial layer, at least one functional additional layer selected from the group of a barrier layer and a metal layer.