# US 11,118,004 B2 · Three-dimensional inkjet printing using ring-opening metathesis polymerization

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,118,004 B2
- Document ID: US11118004B2
- Status: Granted
- Kind: B2
- Application number: 16/095,384
- Filed: 2017-02-05
- Published: 2019-05-02
- Granted: 2021-09-14
- Earliest claimed: 2016-04-26
- Assignees: Stratasys, Inc.
- Applicants: Stratasys Ltd.
- Inventors: Yuval Vidavsky; Ira Yudovin-Farber; Asher Razlan; Lev Kuno; Gilles Recher; Renata Drozdzak-Matusiak
- Web page: https://patentgrep.com/patent/US11118004B2

## CPC

- C08G 61/08: of carbocyclic compounds containing one or more carbon-to-carbon double bonds in the ring
- B29C 64/112: using individual droplets, e.g. from jetting heads
- B33Y 10/00: Processes of additive manufacturing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C08G 2261/418: Ring opening metathesis polymerisation [ROMP]
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING

## Abstract

Methods for fabricating three-dimensional objects by 3D-inkjet printing technology are provided. The methods utilize curable materials that polymerize via ring-opening metathesis polymerization (ROMP) for fabricating the object, in combination with acid-activatable pre-catalyst and an acid generator activator. Kits containing modeling material formulations usable in the methods are also provided.

## Claims

### Claim 1

A method of fabricating a three-dimensional object, the method comprising sequentially forming a plurality of layers in a configured pattern corresponding to the shape of the object, thereby fabricating the object,
wherein said formation of each layer comprises dispensing at least two modeling material formulations by at least two inkjet printing heads, each head jetting one of said at least two modeling material formulations, said at least two modeling material formulations comprising an unsaturated cyclic monomer polymerizable by ring opening metathesis polymerization (ROMP) and a catalyst system for initiating ROMP of said monomer, said catalyst system comprising a pre-catalyst and an activator for chemically activating said catalyst towards initiating ROMP of said monomer, wherein at least one of said modeling material formulations comprises said pre-catalyst and at least another modeling material formulation comprises said activator and is devoid of said pre-catalyst,
wherein said pre-catalyst is an acid-activatable ruthenium-based pre-catalyst and said activator is active towards chemically activating said pre-catalyst,
wherein said pre-catalyst comprises at least two pre-catalysts,
wherein one of said pre-catalysts is
and another one of said pre-catalysts is

### Claim 2 (depends on 1)

The method of claim 1, wherein said activator is represented by Formula:
(R)nSi(Cl)4-n
wherein:
n is 1, 2, or 3, and R is selected from hydrogen, alkyl and aryl, such that when n is 2 or 3, each R can be the same or different,
wherein at least one R is selected from alkyl and aryl.

### Claim 3 (depends on 1)

The method of claim 1, wherein at least one of said modeling material formulations further comprises a toughening agent.

### Claim 4 (depends on 1)

The method of claim 1, wherein a temperature of an inkjet printing head for dispensing said at least one modeling material formulation ranges from 25° C. to 65° C. or from 65° C. to about 85° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein a weight ratio between said pre-catalysts ranges from 90:10 to 10:90.

### Claim 6 (depends on 5)

The method of claim 5, wherein said weight ratio ranges from 60:40 to 40:60.