# US 11,117,843 B2 · Method for converting a gas comprising carbon monoxide into methane by means of a catalytic material containing praseodymium and nickel on alumina

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,117,843 B2
- Document ID: US11117843B2
- Status: Granted
- Kind: B2
- Application number: 16/757,511
- Filed: 2018-10-22
- Published: 2020-07-30
- Granted: 2021-09-14
- Earliest claimed: 2017-10-20
- Applicants: Engie; Enercat
- Inventors: Arnaud Lahougue; Emmanuel Rohart; Gaëlle Gicquel; Sandra Capela; Yilmaz Kara; Stéphane Fortin; Myriam De Saint Jean
- Web page: https://patentgrep.com/patent/US11117843B2

## CPC

- C07C 1/0435: {containing a metal of group 8 or a compound thereof}
- B01J 8/003: {in a downward flow}
- B01J 8/125: {with multiple sections one above the other separated by distribution aids, e.g. reaction and regeneration sections}
- B01J 8/1827: {the fluidising gas being a reactant}
- B01J 8/1836: {Heating and cooling the reactor (B01J8/42 takes precedence)}
- B01J 8/24: according to "fluidised-bed" technique (B01J8/20 takes precedence)
- B01J 21/04: Alumina
- B01J 23/10: of rare earths
- B01J 23/755: Nickel
- B01J 23/83: with rare earths or actinides
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/613: {10-100 m2/g}
- B01J 35/615: {100-500 m2/g}
- B01J 35/647: {2-50 nm}
- B01J 37/0201: {Impregnation}
- B01J 37/0221: {of particles}
- B01J 37/031: {Precipitation}
- B01J 37/082: {Decomposition and pyrolysis}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 37/16: Reducing
- B01J 37/18: with gases containing free hydrogen
- C07C 1/041: {Reactors}
- C07C 1/042: {Temperature controlling devices; Heat exchangers}
- C07C 1/0445: {Preparation; Activation}
- C07C 1/0485: {Set-up of reactors or accessories; Multi-step processes}
- C07C 1/12: from carbon dioxide with hydrogen
- B01J 2208/00132: Tubes
- B01J 2523/00: Constitutive chemical elements of heterogeneous catalysts
- C07C 2521/04: Alumina
- C07C 2523/10: of rare earths
- C07C 2523/755: Nickel
- C07C 2523/83: with rare earths or actinides
- Y02P 20/52: using catalysts, e.g. selective catalysts
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to a method for converting a gas into methane (CH4) which includes: a step of activating a catalytic material including praseodymium oxide (Pr6O11) associated with nickel oxide (NiO) and alumina (Al2O3), the respective proportions of which are, relative to the total mass of these three compounds: Pr6O11: 1 wt % to 20 wt %, NiO: 1 wt % to 20 wt %, and A12O3: 60 to 98 wt %; and a step of passing a gas including at least one carbon monoxide (CO) over the activated catalytic material.

## Claims

### Claim 1

A method for converting a gas into methane (CH4), that comprises:
a step of activating a catalytic material consisting of praseodymium oxide (Pr6O11) associated with nickel oxide (NiO) and alumina (Al2O3), the respective proportions of which are, relative to the total mass of these three compounds:
Pr6O11: 1 wt % to 20 wt %,
NiO: 1 wt % to 20 wt %, and
Al2O3: 60 wt % to 98 wt %; and
a step of passing a gas including at least carbon monoxide (CO) over the activated catalytic material.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the gas passing over the activated catalytic material also comprises carbon dioxide (CO2).

### Claim 3 (depends on 1)

The method according to claim 1, wherein the proportion of carbon monoxide in the gas reaching the activated catalytic material is higher than five percent by volume in dry gas.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, during the gas passage step, a gas mixture is passed that mainly contains CO, CO2 and H2, with an H2 content higher than that of CO and CO2.

### Claim 5 (depends on 1)

The method according to claim 1, wherein, during the gas passage step, the mean temperature of the catalytic layer is below 300° C.

### Claim 6 (depends on 1)

The method according to claim 1, which further comprises a step of shaping the catalytic material into beads with a mean size of between 100 and 1000 μm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein before the activation step, the catalytic material has respective proportions, relative to the total mass of these three compounds, of:
Pr6O11: 3 wt % to 15 wt %,
NiO: 3 wt % to 15 wt %, and
Al2O3: 70 wt % to 94 wt %.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the alumina has a mesoporosity corresponding to a median diameter of the pores, determined by Hg intrusion porosimetry, of between 3 and 50 nm.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the alumina has a gamma structure.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the catalytic material's specific surface area SStel is between 50 and 300 m2/g.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the catalytic material's specific surface area SStel is between 100 and 250 m2/g.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the step of activating the catalytic material comprises heat treatment in the presence of reducing agents.

### Claim 13 (depends on 2)

The method according to claim 2, wherein the step of activating the catalytic material in the presence of reducing agents is performed in a temperature range of 300-500° C.

### Claim 14 (depends on 1)

The method according to claim 1, which further comprises
a step of the solubilization of salt precursors of nickel and praseodymium, separately or in a mixture;
a step of the surface deposition of metal salts on a carrier based on alumina (Al2O3); and
a step of thermal decomposition in an atmosphere comprising oxygen and in a temperature range of 350-500° C., for a period of between one hour and four hours.

### Claim 15 (depends on 1)

The method according to claim 1, which further comprises, before the gas passage step, a step of constituting the gas comprising at least one of the following steps:
pyrolysis of hydrocarbon materials;
pyro-gasification of hydrocarbon materials;
gasification of hydrocarbon materials;
co-electrolysis of CO2/H2O;
water-Gas-Shift; and
reverse Water-Gas-Shift.

### Claim 16 (depends on 1)

The method according to claim 1, wherein, during the step of passing the gas over the catalytic material, the gas goes through a catalytic layer of activated catalytic material.

### Claim 17 (depends on 16)

The method according to claim 16, wherein, during the step of passing the gas over the catalytic material, the gas goes through a fluidized bed of activated catalytic material.

### Claim 18 (depends on 16)

The method according to claim 16, which further comprises a step of cooling the catalytic layer by at least one heat exchange tube immersed in the catalytic layer.

### Claim 19 (depends on 2)

The method according to claim 2, wherein the step of activating the catalytic material in the presence of reducing agents is performed in a temperature range of 400-500° C.