# US 11,117,839 B2 · Densification of melt infiltrated ceramic matrix composite (CMC) articles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,117,839 B2
- Document ID: US11117839B2
- Status: Granted
- Kind: B2
- Application number: 16/393,360
- Filed: 2019-04-24
- Published: 2020-10-29
- Granted: 2021-09-14
- Earliest claimed: 2019-04-24
- Assignees: General Electric Company
- Applicants: General Electric Company
- Inventors: Jason Robert Parolini; Canan Uslu Hardwicke; Srikanth Chandrudu Kottilingam; James Joseph Murray, III
- Web page: https://patentgrep.com/patent/US11117839B2

## CPC

- C04B 35/573: obtained by reaction sintering {or recrystallisation}
- C04B 41/4584: {Coating or impregnating of particulate or fibrous ceramic material (C04B20/10, C04B35/628 take precedence)}
- C04B 35/565: based on silicon carbide
- C04B 35/80: Fibres, filaments, whiskers, platelets, or the like
- C04B 2235/428: Silicon
- C04B 2235/5224: Alumina or aluminates
- C04B 2235/5228: Silica and alumina, including aluminosilicates, e.g. mullite
- C04B 2235/524: Non-oxidic, e.g. borides, carbides, silicides or nitrides
- C04B 2235/5244: Silicon carbide
- C04B 2235/5248: Carbon, e.g. graphite
- C04B 2235/616: Liquid infiltration of green bodies or pre-forms
- C04B 2235/6581: Total pressure below 1 atmosphere, e.g. vacuum
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Various embodiments include methods for densifying a melt infiltrated ceramic matrix composite (CMC) article, and a densified melt infiltrated CMC article formed thereby. Particular embodiments include a method including: providing a porous CMC preform within a first region of a casting apparatus; providing a molten densifier within a pressure head area of a second region of the casting apparatus, the first and second regions being operably connected and the molten densifier including at least one source of silicon; and applying a first pressure to the molten densifier within the pressure head, thereby infiltrating voids within the porous CMC preform with the molten densifier and forming a densified melt infiltrated CMC article.

## Claims

### Claim 1

A method for densifying a melt infiltrated ceramic matrix composite (CMC) article, comprising:
providing a porous CMC preform within a first region of a casting apparatus;
providing a molten densifier within a pressure head area of a second region of the casting apparatus, the first and second regions being operably connected and the molten densifier including at least one source of silicon; and
applying a first pressure to the molten densifier within the pressure head, thereby infiltrating voids within the porous CMC preform with the molten densifier and forming a densified melt infiltrated CMC article, wherein the first pressure applied to the molten densifier is atmospheric pressure, and the first and second regions of the casting apparatus are oriented with one another such that a weight of the molten densifier within the pressure head area allows for infiltration of the porous CMC preform with the molten densifier, and
wherein the first region of the casting apparatus includes a die set containing the porous CMC preform, the die set having at least two portions that are capable of moving relative to one another and creating a die opening there between,
further including adjusting an opening width of the die opening during the applying of the first pressure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the adjusting of the opening width of the die opening includes adjusting the opening width to a selected opening width, the selected opening width reducing or inhibiting damage to a porous matrix of the porous CMC preform.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first pressure applied to the molten densifier is greater than atmospheric pressure, and the first and second regions of the casting apparatus are operably coupled with one another such that the infiltrating of the porous CMC preform with the molten densifier at the first pressure greater than atmospheric pressure is performed without damaging the porous matrix of the porous CMC preform.

### Claim 4 (depends on 3)

The method of claim 3, wherein at least one of the first region and the second region of the casting apparatus includes an inlet for passing the molten densifier to the porous CMC preform.

### Claim 5 (depends on 1)

The method of claim 1, wherein the casting apparatus includes a third region, the porous CMC preform spanning between the second and third regions.

### Claim 6 (depends on 5)

The method of claim 5, wherein the first pressure of the second region is greater than a pressure of the third region, and the difference between the first pressure of the second region and the pressure of the third region allows for infiltration of the porous CMC preform with the molten densifier.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first pressure is applied is less than about 3 Bars.

### Claim 8

A method for densifying a melt infiltrated ceramic matrix composite (CMC) article, comprising:
providing a porous CMC preform within a first region of a casting apparatus;
providing a molten densifier within a pressure head area of a second region of the casting apparatus, the first and second regions being operably connected and the molten densifier including at least one source of silicon; and
applying a first pressure to the molten densifier within the pressure head, thereby infiltrating voids within the porous CMC preform with the molten densifier and forming a densified melt infiltrated CMC article, wherein the first pressure is applied is less than about 3 Bars, wherein the first pressure applied to the molten densifier is atmospheric pressure, and the first and second regions of the casting apparatus are oriented with one another such that a weight of the molten densifier within the pressure head area allows for infiltration of the porous CMC preform with the molten densifier, and wherein the first region of the casting apparatus includes a die set containing the porous CMC preform, the die set having at least two portions that are capable of moving relative to one another and creating a die opening there between, and
further including adjusting an opening width of the die opening during the applying of the first pressure.

### Claim 9 (depends on 8)

The method of claim 8, wherein the adjusting of the opening width of the die opening includes adjusting the opening width to a selected opening width, the selected opening width reducing or inhibiting damage to a porous matrix of the porous CMC preform.

### Claim 10 (depends on 8)

The method of claim 8, wherein the first pressure applied to the molten densifier is greater than atmospheric pressure, and the first and second regions of the casting apparatus are operably coupled with one another such that the infiltrating of the porous CMC preform with the molten densifier at the first pressure greater than atmospheric pressure is performed without damaging the porous matrix of the porous CMC preform.

### Claim 11 (depends on 10)