# US 11,117,825 B2 · Method for activating an inner surface of a hollow glass substrate tube for the manufacturing of an optical fiber preform

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,117,825 B2
- Document ID: US11117825B2
- Status: Granted
- Kind: B2
- Application number: 14/101,705
- Filed: 2013-12-10
- Published: 2014-06-12
- Granted: 2021-09-14
- Earliest claimed: 2012-12-11
- Assignees: Draka Comteq B.V.
- Applicants: Draka Comteq B.V.
- Inventors: Igor Milicevic; Mattheus Jacobus Nicolaas Van Stralen; Johannes Antoon Hartsuiker
- Web page: https://patentgrep.com/patent/US11117825B2

## CPC

- C03B 37/018: by glass deposition on a glass substrate, e.g. by {inside-, modified-, plasma- or plasma modified-} chemical vapour deposition {[ICVD, MCVD, PCVD, PMCVD], i.e. by thin layer coating on the inside or outside of a glass tube or on a glass rod} (C03B37/016 takes precedence; surface treatment of glass by coating with glass C03C17/02)
- C03B 37/0183: {for plasma within a tube substrate}
- C03B 37/01861: {Means for changing or stabilising the diameter or form of tubes or rods}
- C03C 2218/33: by etching
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for activating an inner surface of a hollow glass substrate tube for manufacturing an optical fiber preform including depositing a plurality of activation glass layers on the inner surface of the hollow substrate tube by a PCVD process, wherein a total thickness of the deposited activation glass layers is between 10 microns and 250 microns, and etching the deposited activation glass layers to remove at least 30% of the deposited activation glass layers.

## Claims

### Claim 1

A method of manufacturing a preform for optical fibers comprising the steps of:
(i) providing a hollow substrate tube having an initial or original inner surface, the initial or original inner surface having surface irregularities that predispose the hollow substrate tube to preferential plasma etching, wherein the surface irregularities of the initial or original inner surface of the hollow substrate tube of step (i) that predispose the hollow substrate tube of step (i) to preferential plasma etching comprise a material inhomogeneity relative to other portions of the hollow substrate tube of step (i);
(ii) depositing directly on the initial or original inner surface of the hollow substrate tube a first activation glass layer with PCVD and subsequently depositing a plurality of activation glass layers directly on the first activation glass layer deposited on the initial or original inner surface of the hollow substrate tube with PCVD thereby forming a pretreated hollow glass substrate tube, wherein a total thickness of all activation glass layers deposited in the pretreated hollow substrate tube is at least 10 microns and up to 250 microns and all of the activation glass layers are undoped;
(iii) after step (ii), etching the pretreated hollow substrate tube thereby removing at least 30% of and up to 100% of the activation glass layers thereby forming an etched hollow substrate tube having an inner surface with reduced surface irregularities or without surface irregularities when compared with the surface irregularities of the initial or original inner surface of the hollow substrate tube of step (i);
(iv) after step (iii), supplying doped glass forming gases, undoped glass-forming gases, or a combination thereof into the etched hollow substrate tube and depositing glass layers from the doped glass forming gases, undoped glass-forming gases, or the combination thereof on the inside of the etched hollow substrate tube; and
(v) collapsing the etched hollow substrate tube of step (iv) having deposited glass layers from the doped glass forming gases, undoped glass-forming gases, or the combination thereof on the inside of the etched hollow substrate tube into an optical fiber preform, wherein:
the plurality of activation layers do not contribute to a refractive index profile of the optical fiber preform, and
the doped glass forming gases, undoped glass-forming gases, or a combination thereof of step (iv) provide the refractive index profile of the optical fiber preform.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the etching in step iii) comprises a plasma etching step using an etching gas.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the etching step in step iii) further comprises providing a carrier gas with the etching gas, and
the etching gas is a fluorine-containing etching gas comprising a hydrogen-free fluorinated compound, F2, or a combination thereof.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the carrier gas is selected from the group consisting of oxygen, nitrogen, and argon.

### Claim 5 (depends on 3)

The method according to claim 3, wherein the fluorine-containing etching gas is one or more of C2F6 and SF6 and the carrier gas is O2.

### Claim 6 (depends on 2)

The method according to claim 2, wherein the etching gas includes at least one etching compound selected from the group consisting of CCl2F2, CF4, C2F6, SF6, and SO2F2, and combinations thereof.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the total thickness of the deposited activation glass layers is at least 25 microns.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the total thickness of the deposited activation glass layers is at least 50 microns.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the total thickness of the deposited activation glass layers is at most 125 microns.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the total thickness of the deposited activation glass layers is at most 75 microns.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the plurality of activation layers is undoped.

### Claim 12 (depends on 1)

The method of claim 1, wherein up to 80% of the activation glass layers are removed during step (iii).

### Claim 13 (depends on 1)

The method of claim 1, wherein up to 85% of the activation glass layers are removed during step (iii).

### Claim 14 (depends on 1)

The method of claim 1, wherein up to 90% of the activation glass layers are removed during step (iii).

### Claim 15 (depends on 1)

The method of claim 1, wherein up to 95% of the activation glass layers are removed during step (iii).

### Claim 16 (depends on 1)

The method of claim 1, wherein up to 99% of the activation glass layers are removed during step (iii).