# US 11,117,804 B2 · Method of synthesizing thickness-controlled graphene through chemical vapor deposition using Cu—Ni thin film laminate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,117,804 B2
- Document ID: US11117804B2
- Status: Granted
- Kind: B2
- Application number: 15/867,913
- Filed: 2018-01-11
- Published: 2018-12-06
- Granted: 2021-09-14
- Earliest claimed: 2017-06-02
- Assignees: Center for Advanced Soft Electronics; Postech Academy-Industry Foundation
- Applicants: Center for Advanced Soft Electronics
- Inventors: Kilwon Cho; Min Seok Yoo; Hyo Chan Lee
- Web page: https://patentgrep.com/patent/US11117804B2

## CPC

- C01B 32/186: by chemical vapour deposition [CVD]
- C23C 14/3442: {using an ion beam}
- C23C 16/0281: {of metallic sub-layers (C23C16/029 takes precedence)}
- C23C 16/04: Coating on selected surface areas, e.g. using masks
- C23C 16/26: Deposition of carbon only
- C01B 2204/04: Specific amount of layers or specific thickness
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Disclosed is a method of synthesizing graphene, wherein a Cu—Ni thin film laminate including a copper thin film and a nickel thin film formed thereon is placed in a chemical vapor depositor, brought into contact with a graphene precursor and subjected to chemical vapor deposition (CVD), thus synthesizing thickness-controlled graphene on the copper thin film, whereby the thickness of multilayer graphene can be easily and reproducibly controlled by adjusting only nickel thickness and CVD time, and a process window for obtaining reproducible results can be widened due to self-limiting properties whereby the maximum thickness of graphene is obtained after a certain synthesis time due to the thickness-controlled nickel thin film. Also, carbon atoms absorbed to the nickel thin film reach the copper thin film opposite thereto through internal diffusion of the metal laminate to thus grow graphene via surface-mediated reaction thereon, thereby improving the uniformity of synthesized graphene.

## Claims

### Claim 1

A method of synthesizing graphene, comprising:
(a) placing a Cu—Ni thin film laminate including a copper thin film comprising a top surface and a bottom surface and a nickel thin film comprising a top surface and a bottom surface formed on the bottom surface of the copper thin film in a chemical vapor depositor; and
(b) bringing a graphene precursor into contact with the Cu—Ni thin film laminate such that the top surface of the copper thin film and the bottom surface of the nickel thin film are exposed to the graphene precursor, and performing chemical vapor deposition (CVD), thus synthesizing Bernal-stacked multilayer graphene on the top surface of the copper thin film,
wherein during the synthesizing step of graphene, a nickel concentration gradient in the copper thin film is generated and a nickel concentration at the bottom surface of the copper thin film is higher than a nickel concentration at the top surface of the copper thin film as a part of nickel of the nickel thin film of the laminate is diffused to interior of the copper thin film,
carbon atoms generated by a decomposition of the graphene precursor are subjected to surface-mediated reaction to form top-layer graphene of the Bernal-stacked multilayer graphene on the top surface of the copper thin film,
the carbon atoms are absorbed to the bottom surface of the nickel thin film and a carbon concentration gradient is formed in the thickness direction of the Cu—Ni thin film laminate,
the carbon atoms absorbed to the bottom surface of the nickel thin film are diffused by the carbon concentration gradient to the copper thin film along the thickness direction of the copper thin film such that the diffused carbon atoms reach the top surface of the copper thin film and form adlayer graphene through surface-mediated reaction between the top-layer graphene and the top surface of the copper thin film,
the chemical vapor deposition is performed at a temperature of 600 to 1,300° C., and
a thickness or a number of layers of the graphene synthesized on the top surface of the copper thin film is controlled by adjusting a thickness of the nickel thin film of the laminate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the nickel thin film has a thickness ranging from 5 to 1,000 nm.

### Claim 3 (depends on 1)

The method of claim 1, wherein a number of layers of the graphene is any one ranging from 2 to 10.

### Claim 4 (depends on 1)

The method of claim 1, wherein a thickness of the nickel thin film is adjusted to a range of 1000 nm or less but exceeding 70 nm in step (a), whereby multilayer graphene is synthesized in step (b).

### Claim 5 (depends on 1)

The method of claim 1, wherein the graphene precursor is a hydrocarbon compound.

### Claim 6 (depends on 5)

The method of claim 5, wherein the hydrocarbon compound is at least one selected from the group consisting of methane, ethane, propane, butane, ethylene, propylene, butylene, benzene, and ethanol.

### Claim 7 (depends on 1)

The method of claim 1, wherein the chemical vapor deposition is performed by supplying the graphene precursor at a rate of 0.1 to 500 sccm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the chemical vapor deposition is performed for 10 to 500 min.

### Claim 9 (depends on 1)

The method of claim 1, wherein the chemical vapor deposition is performed using any one process selected from the group consisting of low-pressure chemical vapor deposition, atmospheric-pressure chemical vapor deposition, plasma-enhanced chemical vapor deposition, Joule-heating chemical vapor deposition, and microwave chemical vapor deposition.

### Claim 10 (depends on 1)

The method of claim 1, wherein the nickel thin film in step (a) is a nickel thin film having a pattern.

### Claim 11 (depends on 10)

The method of claim 10, wherein the pattern includes at least one shape selected from the group consisting of a circular shape, an oval shape, a polygonal shape, a wave shape, a zigzag shape, and a convexo-concave shape.