# US 11,117,239 B2 · Chemical mechanical polishing composition and method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,117,239 B2
- Document ID: US11117239B2
- Status: Granted
- Kind: B2
- Application number: 16/025,263
- Filed: 2018-07-02
- Published: 2019-04-04
- Granted: 2021-09-14
- Earliest claimed: 2017-09-29
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Shich-Chang Suen; Kei-Wei Chen; Liang-Guang Chen
- Web page: https://patentgrep.com/patent/US11117239B2

## CPC

- B24B 37/044: {characterised by the composition of the lapping agent}
- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- H10P 52/402: {of semiconductor materials}
- C09K 3/1436: {Composite particles, e.g. coated particles}
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

An abrasive slurry composition for chemical mechanical planarization/polishing (CMP) is provided. The abrasive slurry includes colloidal alumina, a dispersant, and a pH buffer. The colloidal alumina has a particle size of between about 5 nm and about 100 nm. The colloidal alumina may be alpha phase material having a first hardness of about 9 Mohs, or gamma phase material having a second hardness of about 8 Mohs. The abrasive slurry may further include polyacrylic acid (PAA), a down-force enhancer, or a polish-rate inhibitor.

## Claims

### Claim 1

A method comprising:
introducing a slurry to a chemical mechanical polishing pad, the slurry comprising colloidal alumina, wherein the alumina is formed using a sol-gel process, the sol-gel process utilizing β-alanine; and
polishing a semiconductor device layer with the slurry and the chemical mechanical polishing pad.

### Claim 2 (depends on 1)

The method of claim 1, wherein the colloidal alumina has a particle size of between about 5 nm and about 100 nm.

### Claim 3 (depends on 2)

The method of claim 2, wherein the colloidal alumina has a particle size of about 50 nm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the colloidal alumina comprises at least one of an alpha phase material or a gamma phase material.

### Claim 5 (depends on 4)

The method of claim 4, wherein the colloidal alumina comprises the alpha phase material.

### Claim 6 (depends on 4)

The method of claim 4, wherein the colloidal alumina comprises both the gamma phase material and the alpha phase material.

### Claim 7

A method comprising:
forming colloidal alumina using a sol-gel process, the sol-gel process using AlCl3 and Al(NO3)3 as precursors along with β-alanine, wherein the AlCl3 and Al(NO3)3 are in a ratio of 0.1˜5% and wherein a product is hydrothermally treated at a temperature range of between about 600° C. and about 800° C. for a duration of time between about 1 hour and about 2 hours;
attaching a semiconductor device wafer to a chemical mechanical planarization (CMP) carrier head;
introducing a CMP slurry to an exposed surface of the semiconductor device wafer, the CMP slurry comprising the colloidal alumina; and
after introducing the CMP slurry, polishing the exposed surface of the semiconductor device wafer until the semiconductor device wafer has a topological difference spanning a range of about 50 Å.

### Claim 8 (depends on 7)

The method of claim 7, wherein the colloidal alumina has a particle size of between about 5 nm and about 100 nm.

### Claim 9 (depends on 7)

The method of claim 7, wherein the colloidal alumina has a concentration within the CMP slurry of between about 0.1%-wt and about 4%-wt.

### Claim 10 (depends on 7)

The method of claim 7, wherein the colloidal alumina comprises an alpha phase material having a hardness of about 9 Mohs.

### Claim 11 (depends on 10)

The method of claim 10, wherein the colloidal alumina further comprises a gamma phase material having a hardness of about 8 Mohs.

### Claim 12

A method comprising:
forming a chemical mechanical polishing slurry comprising:
placing a reactant into a solvent such that the reactant is present between about 0.001%-wt and about 1.5%-wt;
forming a sol-gel formed colloidal alumina utilizing β-alanine;
placing the a sol-gel formed colloidal alumina into the solvent, wherein the sol-gel formed colloidal alumina is present between about 0.1%-wt and about 4%-wt; and
placing a dispersant into the solvent such that the dispersant is present between about 0.001%-wt and about 0.1%-wt;
placing a pH adjustor into the solvent such that the pH adjustor is present between about 0.001%-wt and about 0.1%-wt;
placing a corrosion inhibitor into the solvent such that the corrosion inhibitor is present between about 0.001%-wt to about 0.1%-wt; and
placing a chelate into the solvent such that the chelate is present between about 0.001%-wt and about 0.01%-wt, wherein the solvent is present between about 95%-wt and about 99%-wt.

### Claim 13 (depends on 12)

The method of claim 12, wherein the colloidal alumina has a particle size of between about 5 nm and about 100 nm.

### Claim 14 (depends on 13)

The method of claim 13, wherein the colloidal alumina has a particle size of about 50 nm.

### Claim 15 (depends on 12)

The method of claim 12, wherein the reactant is an oxidant.

### Claim 16 (depends on 15)

The method of claim 15, wherein the colloidal alumina comprises at least one of an alpha phase material having a first hardness of about 9 Mohs, or a gamma phase material having a second hardness of about 8 Mohs.

### Claim 17 (depends on 16)

The method of claim 16, wherein the alpha phase material has a concentration within the slurry of between about 90% and about 10% and the gamma phase material has a concentration within the slurry of between about 10% and about 90%.

### Claim 18 (depends on 1)

The method of claim 1, wherein the slurry comprises a dispersant, the dispersant having a concentration of between about 0.001%-wt and about 0.1%-wt.

### Claim 19 (depends on 1)

The method of claim 1, wherein the sol-gel process uses AlCl3 and Al(NO3)3 as precursors, wherein the AlCl3 and Al(NO3)3 are in a ratio of 0.1˜5% and wherein a product is hydrothermally treated at a temperature range of between about 600° C. and about 800° C. for a duration of time between about 1 hour and about 2 hours.

### Claim 20 (depends on 7)