# US 11,117,188 B2 · Chromium metal powder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,117,188 B2
- Document ID: US11117188B2
- Status: Granted
- Kind: B2
- Application number: 14/915,785
- Filed: 2014-08-19
- Published: 2016-07-14
- Granted: 2021-09-14
- Earliest claimed: 2013-09-02
- Assignees: Plansee SE
- Applicants: Plansee SE
- Inventors: Michael O'Sullivan; Lorenz Sigl
- Web page: https://patentgrep.com/patent/US11117188B2

## CPC

- B22F 9/22: using gaseous reductors
- A61H 33/065: {with steam generators}
- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- C22C 27/06: Alloys based on chromium
- B22F 2201/013: Hydrogen
- B22F 2202/00: Treatment under specific physical conditions
- B22F 2301/20: Refractory metals
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- A61H: PHYSICAL THERAPY APPARATUS, e.g. DEVICES FOR LOCATING OR STIMULATING REFLEX POINTS IN THE BODY; ARTIFICIAL RESPIRATION; MASSAGE; BATHING DEVICES FOR SPECIAL THERAPEUTIC OR HYGIENIC PURPOSES OR SPECIFIC PARTS OF THE BODY (electrotherapy, magnetotherapy, radiation therapy or ultrasound therapy A61N)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A metal powder has a chromium content of at least 90 Ma %, a nanohardness according to EN ISO 14577-1 of ≤4 GPa and/or a green strength measured according to ASTM B312-09 of at least 7 MPa at a compression pressure of 550 MPa.

## Claims

### Claim 1

A metal powder, comprising:
a chromium content of at least 90 Ma %; and
a nanohardness HIT 0.005/5/1/5 according to EN ISO 14577-1 of ≤4 GPa.

### Claim 2 (depends on 1)

The metal powder according to claim 1, wherein the metal powder is chromium powder having a metallic purity ≥99.0 Ma %.

### Claim 3 (depends on 1)

The metal powder according to claim 1, wherein the metal powder is an alloyed powder or composite powder.

### Claim 4 (depends on 1)

The metal powder according to claim 1, wherein the metal powder is granulated.

### Claim 5 (depends on 1)

The metal powder according to claim 1, which further comprises a surface area according to BET of ≥0.05 m2/g with or without a surface-enlarging operation.

### Claim 6

A method for producing a metal powder, the method comprising the following steps:
reducing at least one compound of the group consisting of chromium oxide and chromium hydroxide, optionally with an admixed solid carbon source, under at least temporary action of hydrogen and hydrocarbon to produce a metal powder having:
a chromium content of at least 90 Ma %; and
a nanohardness HIT 0.005/5/1/5 according to EN ISO 14577-1 of ≤4 GPa.

### Claim 7 (depends on 6)

The method according to claim 6, which further comprises:
heating the compound of the group consisting of chromium oxide and chromium hydroxide, optionally with an admixed solid carbon source, to a temperature TR with 1100° C.≤TR≤1550° C.;
optionally holding the temperature at 1100° C.≤TR≤1550° C.; and
at least temporarily setting the hydrocarbon partial pressure at 5 to 500 mbar at least during the heating step.

### Claim 8 (depends on 6)

The method according to claim 6, wherein the action of hydrogen and hydrocarbon occurs at least in a temperature range of 800 to 1050° C.

### Claim 9 (depends on 8)

The method according to claim 8, which further comprises setting the hydrocarbon partial pressure at 5 to 500 mbar at least in the temperature range of 800 to 1050° C.

### Claim 10 (depends on 8)

The method according to claim 8, which further comprises setting a sum of heating time and holding time in the temperature range of 800° C. to 1050° C. to be at least 45 minutes.

### Claim 11 (depends on 6)

The method according to claim 6, which further comprises setting a total pressure at 0.95 to 2 bar.

### Claim 12 (depends on 6)

The method according to claim 6, which further comprises reducing the compound of the group consisting of chromium oxide and chromium hydroxide under at least temporary action of a H2—CH4 gas mixture.

### Claim 13 (depends on 12)

The method according to claim 12, which further comprises setting a H2/CH4 volume ratio at 1 to 200 or 1.5 to 20.

### Claim 14 (depends on 6)

The method according to claim 6, which further comprises admixing a solid carbon source having at least one component selected from the group consisting of carbon black, activated carbon, graphite, carbon-releasing compound and mixtures thereof.

### Claim 15 (depends on 14)

The method according to claim 14, which further comprises using between 0.75 and 1.25 mol or between 0.90 and 1.05 mol of carbon per mol of oxygen in the chromium oxide or chromium hydroxide.

### Claim 16 (depends on 6)

The method according to claim 6, which further comprises at least partially reacting at least one compound selected from the group consisting of chromium oxide and chromium hydroxide under the action of hydrogen and hydrocarbon to form a chromium carbide selected from the group consisting of Cr3C2, Cr7C3 and Cr23C6.

### Claim 17 (depends on 16)

The method according to claim 16, which further comprises at least partially reacting the chromium carbide with at least one compound selected from the group consisting of chromium oxide and chromium hydroxide to form chromium.

### Claim 18 (depends on 6)

The method according to claim 6, wherein the hydrocarbon is CH4.