# US 11,117,119 B2 · Catalyst for oxidative dehydrogenation and method of preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,117,119 B2
- Document ID: US11117119B2
- Status: Granted
- Kind: B2
- Application number: 15/540,425
- Filed: 2016-11-30
- Published: 2018-11-22
- Granted: 2021-09-14
- Earliest claimed: 2015-12-09
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Myung Ji Suh; Yoon Jae Min; Dong Hyun Ko; Kyong Yong Cha; Se Won Baek; Jun Kyu Han
- Web page: https://patentgrep.com/patent/US11117119B2

## CPC

- B01J 23/8892: {Manganese}
- B01J 21/12: Silica and alumina
- B01J 21/16: Clays or other mineral silicates
- B01J 23/005: {Spinels}
- B01J 23/78: with alkali- or alkaline earth metals
- B01J 23/80: with zinc, cadmium or mercury
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 35/66: Pore distribution
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/0036: {Grinding}
- B01J 37/033: {Using Hydrolysis}
- B01J 37/035: {Precipitation on carriers}
- B01J 37/038: {to form slurries or suspensions, e.g. a washcoat}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C07C 5/48: with oxygen as an acceptor
- B01J 2523/00: Constitutive chemical elements of heterogeneous catalysts
- C07C 2521/12: Silica and alumina
- C07C 2523/78: with alkali- or alkaline earth metals or beryllium
- C07C 2523/80: with zinc, cadmium or mercury
- C07C 2523/889: Manganese, technetium or rhenium
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

The present invention relates to a catalyst for oxidative dehydrogenation and a method of preparing the same. More particularly, the present invention provides a catalyst for oxidative dehydrogenation having a porous structure which may easily control heat generation due to high-temperature and high-pressure reaction conditions and side reaction due to the porous structure and thus exhibits superior product selectivity, and a method of preparing the catalyst.

## Claims

### Claim 1

A method of preparing a catalyst for oxidative dehydrogenation, the method comprising:
a step of immersing a porous rubber in aluminum silicate to be coated with the aluminum silicate;
a step of firing the porous rubber coated with the aluminum silicate to obtain a porous aluminum silicate support, wherein a temperature of firing the porous rubber coated with aluminum silicate is 1,400 to 1,8000C;
a step of preparing a catalyst slurry comprising a metal oxide, or preparing a co-precipitated slurry comprising a precursor of the metal oxide;
a step of immersing the porous aluminum silicate support in the catalyst slurry or the co-precipitated slurry to be coated with the catalyst slurry or the co-precipitated slurry; and
a step of firing the porous aluminum silicate support coated with the catalyst slurry or the co-precipitated slurry,
wherein the metal oxide is represented by Formula 1:
AB2O4 [Formula 1]
wherein A is Zn and B is Fe (III), and
wherein the porous aluminum silicate support has a pore distribution of 10 ppi to 45 ppi (pores per inch).

### Claim 2 (depends on 1)

The method according to claim 1, wherein the step of immersing the porous rubber in aluminum silicate to be coated with the aluminum silicate comprises: a step of preparing an aluminum silicate slurry; a step of immersing the porous rubber in the aluminum silicate slurry to be coated with the aluminum silicate slurry; and a step of aerating and drying the aluminum silicate slurry-coated porous rubber.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the porous rubber is combusted at 300 to 800° C. during firing.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the porous rubber is polyurethane.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the catalyst slurry is prepared by diluting the metal oxide of Formula 1 with water.

### Claim 6 (depends on 5)

The method according to claim 5, wherein a weight ratio of the metal oxide:the water is 10:1 to 1:10.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the step of immersing the porous aluminum silicate support in the catalyst slurry or the co-precipitated slurry to be coated with the catalyst slurry or the co-precipitated slurry comprises: a step of immersing the porous aluminum silicate support in the catalyst slurry or the co-precipitated slurry; and a step of aerating and drying the porous aluminum silicate support coated with the catalyst slurry or the co-precipitated slurry.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the porous aluminum silicate support coated with the catalyst slurry or the co-precipitated slurry is dried at 80 to 160° C. for 0.5 to 24 hours.

### Claim 9 (depends on 1)

The method according to claim 1, wherein, to fire the porous aluminum silicate support coated with the catalyst slurry or the co-precipitated slurry, a temperature is elevated up to an elevated temperature of 400° C. to 800° C. at a heating rate of 0.5° C./min to 10° C./min and then the elevated temperature is maintained for 2 to 16 hours.

### Claim 10 (depends on 1)