# US 11,117,115 B2 · Carbon nanofiber grafted polyurethane composite for separation of nonpolar components from water

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,117,115 B2
- Document ID: US11117115B2
- Status: Granted
- Kind: B2
- Application number: 16/351,720
- Filed: 2019-03-13
- Published: 2020-09-17
- Granted: 2021-09-14
- Earliest claimed: 2019-03-13
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Tawfik Abdo Saleh Awadh; Nadeem Baig
- Web page: https://patentgrep.com/patent/US11117115B2

## CPC

- B01J 20/205: {Carbon nanostructures, e.g. nanotubes, nanohorns, nanocones, nanoballs (carbon nanotubes per se C01B32/15)}
- B01J 20/262: {obtained otherwise than by reactions only involving carbon to carbon unsaturated bonds, e.g. obtained by polycondensation (macromolecular compounds obtained otherwise than by reactions only involving unsaturated carbon-to-carbon bonds per se C08G)}
- B01J 20/28004: {Sorbent size or size distribution, e.g. particle size}
- B01J 20/28011: {Other properties, e.g. density, crush strength}
- B01J 20/28023: {Fibres or filaments (fibres or filaments in the form of membranes B01J20/28038; B01J20/28007 takes precedence)}
- B01J 20/28045: {Honeycomb or cellular structures; Solid foams or sponges}
- B01J 20/28059: {being less than 100 m2/g}
- B01J 20/28061: {being in the range 100-500 m2/g}
- B01J 20/28083: {being in the range 2-50 nm, i.e. mesopores}
- B01J 20/28085: {being more than 50 nm, i.e. macropores}
- B01J 20/3212: {consisting of a polymer obtained by reactions otherwise than involving only carbon to carbon unsaturated bonds}
- B01J 20/3217: {Resulting in a chemical bond between the coating or impregnating layer and the carrier, support or substrate, e.g. a covalent bond}
- B01J 20/324: {containing free carbon, e.g. activated carbon}
- B01J 20/3295: {Coatings made of particles, nanoparticles, fibers, nanofibers}
- B01J 20/3416: {of sorbents or filter aids comprising free carbon, e.g. activated carbon}
- C02F 1/288: {using composite sorbents, e.g. coated, impregnated, multi-layered}
- C09K 3/32: for absorbing liquids to remove pollution, e.g. oil, gasoline, fat
- C02F 1/283: {using coal, charred products, or inorganic mixtures containing them}
- C02F 1/285: {using synthetic organic sorbents}
- C02F 2101/32: Hydrocarbons, e.g. oil
- C02F 2103/08: Seawater, e.g. for desalination
- C02F 2303/16: Regeneration of sorbents, filters
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A composite of polyurethane foam grafted with carbon nanofibers is described. This composite foam may be made by contacting and drying a polyurethane foam with a suspension of carbon nanofibers and then drying. Additional carbon nanofiber layers may be added with repeated contacting. The composite film has a high surface area of 276 m2/g and a hydrophobic character that may be exploited for separating an oil phase from water.

## Claims

### Claim 1

A carbon nanofiber (CNF) grafted polyurethane composite, comprising:
a polyurethane foam coated with a layer of carbon nanofibers,
wherein a BET surface area is in a range of 220-320 m2/g, and
wherein an apparent contact angle with water is 140°-170°.

### Claim 2 (depends on 1)

The CNF grafted polyurethane composite of claim 1, wherein the layer of carbon nanofibers is porous with an average pore size of 2-5 nm.

### Claim 3 (depends on 1)

The CNF grafted polyurethane composite of claim 1, wherein the polyurethane foam has an average pore diameter in a range of 200-850 μm.

### Claim 4 (depends on 1)

The CNF grafted polyurethane composite of claim 1, wherein the carbon nanofibers have an average length in a range of 5-20 μm and an average thickness in a range of 5-15 nm.

### Claim 5 (depends on 1)

The CNF grafted polyurethane composite of claim 1, wherein the layer of carbon nanofibers further comprises carbon nanoparticles having an average diameter in a range of 1-2 μm.

### Claim 6 (depends on 1)

The CNF grafted polyurethane composite of claim 1, wherein at least 70% of the surface of the polyurethane foam is coated with the layer of carbon nanofibers.

### Claim 7 (depends on 1)

A method of making the CNF grafted polyurethane composite of claim 1, comprising:
contacting a polyurethane foam with a suspension of carbon nanofibers in an alcohol to produce a wet scaffold, and
drying the wet scaffold to produce the CNF grafted polyurethane composite.

### Claim 8 (depends on 7)

The method of claim 7, wherein the polyurethane foam has a surface area in a range of 5-20 m2/g.

### Claim 9 (depends on 7)

The method of claim 7, wherein the carbon nanofibers are present in the suspension at a concentration of 0.1-5 mg/mL.

### Claim 10 (depends on 7)

The method of claim 7, wherein the alcohol is methanol, ethanol, butanol, or isopropanol.

### Claim 11 (depends on 7)

The method of claim 7, wherein the contacting is done for a period of 3-60 min.

### Claim 12 (depends on 7)

The method of claim 7, wherein the drying is at a temperature of 50-80° C. for a period of 12-24 h.

### Claim 13 (depends on 7)

The method of claim 7, wherein the contacting and drying are each repeated two more times on the CNF grafted polyurethane composite.

### Claim 14 (depends on 1)

A method of separating a nonpolar compound from an aqueous solution in a mixture, the method comprising:
contacting the mixture with the CNF grafted polyurethane composite of claim 1,
wherein the CNF grafted polyurethane composite adsorbs 20-50 times its weight of the nonpolar compound.

### Claim 15 (depends on 14)

The method of claim 14, wherein the nonpolar compound is at least one selected from the group consisting of hexane, heptane, toluene, xylene, and a petroleum-derived liquid.

### Claim 16 (depends on 14)

The method of claim 14, wherein the nonpolar compound is petrol.

### Claim 17 (depends on 14)

The method of claim 14, wherein the CNF grafted polyurethane composite adsorbs less than 20% of its weight of the aqueous solution.

### Claim 18 (depends on 14)

The method of claim 14, wherein the contacting involves filtering the mixture through the CNF grafted polyurethane composite.

### Claim 19 (depends on 14)

The method of claim 14, further comprising:
compressing the CNF grafted polyurethane composite after the contacting to produce a discharged polyurethane composite, and
reusing the discharged polyurethane composite.

### Claim 20 (depends on 19)

The method of claim 19, wherein the discharged polyurethane composite comprises at least 95 wt % carbon nanofibers relative to a weight of carbon nanofibers in the CNF grafted polyurethane composite.