# US 11,117,098 B2 · Multifunctional filters for diesel emission control

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,117,098 B2
- Document ID: US11117098B2
- Status: Granted
- Kind: B2
- Application number: 15/562,645
- Filed: 2016-03-30
- Published: 2018-04-26
- Granted: 2021-09-14
- Earliest claimed: 2015-03-30
- Assignees: BASF SE
- Applicants: BASF Corporation
- Inventors: Yuejin Li; Stanley A. Roth
- Web page: https://patentgrep.com/patent/US11117098B2

## CPC

- B01D 53/9472: {in different zones}
- B01D 46/2429: {of the honeycomb walls or cells}
- B01D 46/24491: {Porosity}
- B01D 46/24492: {Pore diameter}
- B01D 46/2474: {of the walls along the length of the honeycomb}
- B01D 46/2482: {Thickness, height, width, length or diameter}
- B01D 53/9418: {for removing nitrogen oxides by selective catalytic reduction [SCR] using a reducing agent in a lean exhaust gas}
- B01D 53/9436: {Ammonia}
- B01D 53/944: {Simultaneously removing carbon monoxide, hydrocarbons or carbon making use of oxidation catalysts (three-way-catalysts [TWC] B01D53/9445)}
- B01D 53/945: {characterised by a specific catalyst}
- B01D 53/9468: {in different layers}
- B01J 23/42: Platinum
- B01J 29/763: {CHA-type, e.g. Chabazite, LZ-218}
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 35/56: Foraminous structures having flow-through passages or channels, e.g. grids or three-dimensional [3D] monoliths
- B01J 35/657: {larger than 1000 nm}
- B01J 37/024: {Multiple impregnation or coating}
- B01D 53/9477: {with catalysts positioned on separate bricks, e.g. exhaust systems}
- B01D 2255/1021: Platinum
- B01D 2255/20761: Copper
- B01D 2255/2092: Aluminium
- B01D 2255/30: Silica
- B01D 2255/50: Zeolites
- B01D 2255/902: Multilayered catalyst
- B01D 2255/9022: Two layers
- B01D 2255/9025: Three layers
- B01D 2255/903: Multi-zoned catalysts
- B01D 2255/9032: Two zones
- B01D 2255/9035: Three zones
- B01D 2255/9037: More than three zones
- B01D 2255/9155: Wall flow filters
- B01D 2258/012: Diesel engines and lean burn gasoline engines
- F01N 3/035: with catalytic reactors
- F01N 3/2066: {Selective catalytic reduction [SCR]}
- F01N 2370/04: Zeolitic material
- Y02T 10/12: Improving ICE efficiencies
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- F01N: GAS-FLOW SILENCERS OR EXHAUST APPARATUS FOR MACHINES OR ENGINES IN GENERAL; GAS-FLOW SILENCERS OR EXHAUST APPARATUS FOR INTERNAL-COMBUSTION ENGINES (arrangements in connection with gas exhaust of propulsion units in vehicles B60K13/00; combustion-air intake silencers specially adapted for, or arranged on, internal-combustion engines F02M35/00; protecting against, or damping, noise in general G10K11/16)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

Provided are multi-zone catalyst articles, methods of manufacturing multi-zone catalyst articles, and methods for controlling emissions in diesel engine exhaust streams with multi-zone catalyst articles, where the emission treatment system of various embodiments effectively treats diesel engine exhaust with a single multi-zone catalyst article.

## Claims

### Claim 1

A catalyzed particulate filter comprising:
a plurality of porous walls extending longitudinally to form a plurality of parallel passages extending from an inlet end to an outlet end, wherein a quantity of the passages are inlet passages that are open at the inlet end and closed at the outlet end, and a quantity of passages are outlet passages that are closed at the inlet end and open at the outlet end;
a first coating permeating through at least a portion of the porous walls of the particulate filter, wherein the length of porous wall permeated with the first coating is in the range of about 1% to about 80% of the wall length extending from the outlet end of the passages, and wherein the first coating is an oxidation catalyst comprising a platinum group metal;
a second coating permeating through at least a portion of the porous walls of the particulate filter, wherein the length of porous wall permeated with the second coating is in the range of about 50% to about 100% of the wall length extending from the inlet end of the passages, and wherein the second coating comprises a first selective catalytic reduction catalyst; and
a third coating that permeates through a portion of the porous walls of the particulate filter in the range of about 20% to about 80% of the wall length from the outlet end; wherein the third coating comprises a second selective reduction catalyst;
wherein the length of the porous walls permeated only with the second coating forms a first catalytic zone of a first SCR catalyst, the length of the porous walls permeated with the second coating and the first coating forms a second catalytic zone of the first SCR catalyst and an AMOx catalyst, and the length of the porous walls permeated with both the first coating and third coating forms a third catalytic zone of a second SCR catalyst and an AMOx catalyst.

### Claim 2 (depends on 1)

The catalyzed particulate filter of claim 1, wherein the first selective catalytic reduction catalyst is a zeolitic framework material promoted with a metal selected from Cu, Fe, Co, Ni, La, Ce, Mn, V, Ag, and combinations thereof.

### Claim 3 (depends on 1)

The catalyzed particulate filter of claim 1, wherein the second coating permeates the porous walls of the particulate filter over 90-100% the entire length of the porous walls of the particulate filter, and the first coating is intermingled with the second coating over about 1% to about 80% of the wall length extending from the outlet end of the passages.

### Claim 4 (depends on 3)

The catalyzed particulate filter of claim 3, wherein the first selective catalytic reduction catalyst comprises a molecular sieve promoted with a base metal, and wherein the length of the porous walls permeated only with the second coating forms a first catalytic zone, and the length of the porous walls permeated with both the first coating and second coating forms a second catalytic zone, wherein the oxidation catalyst intermingles with the first selective catalytic reduction catalyst in the second catalytic zone.

### Claim 5 (depends on 4)

The catalyzed particulate filter of claim 4, wherein the platinum group metal loading in the second catalytic zone is in the range of about 0.1 g/ft3 to about 50 g/ft3.

### Claim 6 (depends on 1)

The catalyzed particulate filter of claim 1, wherein the length of porous wall permeated with the second coating is in the range of about 50% to about 80% of the wall length extending from the inlet end of the passages;
wherein the length of porous wall that is permeated with the first coating but not permeated with the second coating is in the range of about 20% to about 50% of the wall length extending from the outlet end of the passages; and
wherein the length of porous wall permeated with the second coating and having an overlapping first coating is in the range of about 5% to about 60% of the wall length, where the first coating is coated onto the surface of an overlapping portion wherein the porous wall is permeated with the second coating.

### Claim 7 (depends on 1)

The catalyzed particulate filter of claim 1, wherein the length of porous wall permeated with the second coating is in the range of about 95% to about 100% of the wall length extending from the inlet end of the passages;
wherein the length of porous wall that is permeated with the first coating but not permeated with the second coating is in the range of about 0% to about 5% of the wall length extending from the outlet end of the passages; and
wherein the length of porous wall permeated with the second coating and having an overlapping first coating is in the range of about 5% to about 75% of the wall length, where the first coating is coated onto the surface of an overlapping portion wherein the porous wall is permeated with the second coating.

### Claim 8 (depends on 7)

The catalyzed particulate filter of claim 7, wherein the length of the porous wall coated on the surface with the first coating and the third coating is about the same.

### Claim 9 (depends on 7)

The catalyzed particulate filter of claim 7, which further comprises a plug coating on the outlet side of the closed outlet end of the inlet passages, wherein the plug coating comprises a platinum group metal.

### Claim 10 (depends on 1)

The catalyzed particulate filter of claim 1,
wherein the porosity of the porous walls is in the range of about 40% to about 75%, and the mean pore size of the porous walls is in the range of about 10 μm to about 30 μm;
and the first selective catalytic reduction catalyst comprises a copper or iron promoted CHA structure type molecular sieve.

### Claim 11 (depends on 1)

The catalyzed particulate filter of claim 1, wherein the third coating comprises a copper or iron promoted CHA structure type molecular sieve.

### Claim 12 (depends on 1)

The catalyzed particulate filter of claim 1, wherein the length of porous wall permeated with the second coating is in the range of about 95% to about 100% of the wall length extending from the inlet end of the passages, the length of porous wall coated on the surface with the first coating is in the range of about 5% to about 50% of the wall length, and the third coating permeated through the portion of the porous walls of the particulate filter not permeated with the second coating and coated onto the surface of the porous wall in the range of about 1% to about 70% of the wall length, wherein at least a portion of the first coating on the surface of the porous wall is sandwiched between the second coating and a portion of the third coating.

### Claim 13

A method of manufacturing a coated particulate filter, comprising:
introducing an oxidation catalyst comprising a plurality of particles into an outlet end of a plurality of parallel passages formed by a plurality of porous walls closed by a plug on an inlet end opposite the outlet end, wherein the particles of the oxidation catalyst permeates through at least a portion of the porous walls and wherein the length of porous wall permeated with the oxidation catalyst is in the range of about 1% to about 80% of the wall length extending from the outlet end of the passages; and
introducing a first selective catalytic reduction catalyst comprising a plurality of particles into an inlet end of a plurality of parallel passages formed by a plurality of porous walls closed by a plug on an outlet side opposite the inlet side, wherein the particles of the first selective catalytic reduction catalyst permeates through the porous walls, and wherein the length of porous wall permeated with the particles of the first selective catalytic reduction catalyst is in the range of about 50% to about 100% of the wall extending from the inlet end of the passages,
wherein the first selective catalytic reduction catalyst is introduced into the inlet end of the plurality of parallel passages before the oxidation catalyst is introduced into the outlet end of the plurality of parallel passages, and the length of porous wall permeated with the first selective catalytic reduction catalyst is in the range of about 50% to about 80% of the wall length extending from the inlet end of the passages, the length of porous wall that is not permeated with the first selective catalytic reduction catalyst, but permeated with the oxidative catalyst, is in the range of about 20% to about 50% of the wall length extending from the outlet end of the passages, and the length of porous wall permeated with the first selective catalytic reduction catalyst and having an overlapping oxidation catalyst is in the range of about 5% to about 50% of the wall length, wherein the oxidation catalyst remains essentially on the surface of the overlapping portion of the porous wall without interspersing with the first selective catalytic reduction catalyst throughout the porous wall,
which further comprises introducing a second selective catalytic reduction catalyst comprising a plurality of particles comprising a copper or iron promoted CHA structure type molecular sieve into the outlet end of the plurality of parallel passages, wherein the second selective catalytic reduction catalyst permeates through the portion of the porous walls of the particulate filter not previously permeated with the first selective catalytic reduction catalyst, and wherein the first selective catalytic reduction catalysts comprises a copper or iron promoted CHA structure type molecular sieve.

### Claim 14 (depends on 13)

The method of claim 13, wherein the porosity of the porous walls is in the range of about 40% to about 70%, and the mean pore size of the porous walls is in the range of about 10 μm to about 30 μm;
wherein the oxidation catalyst further comprises at least one platinum group metal on the plurality of particles, and the plurality of particles of the oxidation catalyst have a composition of alumina, titania, zirconia, silica, silica/alumina, or a combination thereof; and
wherein the first selective catalytic reduction catalyst is a molecular sieve promoted with a metal selected from Cu, Fe, Co, Ni, La, V, Mo, W, Mn, Ce, Ag and combinations thereof.

### Claim 15 (depends on 13)

The method of claim 13, wherein the length of porous wall permeated with the particles of the first selective catalytic reduction catalyst is in the range of about 95% to about 100% of the wall length extending from the inlet end of the passages, the length of porous wall coated on the surface with the particles of the oxidation catalyst is in the range of about 1% to about 80% of the wall length extending from the outlet end of the passages, and the second selective catalytic reduction catalyst is coated onto the porous walls in the range of about 1% to about 80% of the wall length extending from the outlet end of the passages, wherein the second selective catalytic reduction catalyst is coated onto the surfaces of the porous walls where the second selective catalytic reduction catalyst overlaps with the first selective catalytic reduction catalyst.

### Claim 16 (depends on 13)

The method of claim 13, which further comprises coating a platinum group metal onto the filter such that it only covers the plug at the end of the outlet passages.

### Claim 17 (depends on 14)

The method of claim 14, which further comprises:
impregnating the platinum group metal into the plurality of the alumina, titania, zirconia, silica, silica/alumina, or a combination thereof particles by an incipient wetness technique followed by thermally treating the impregnated particles at a temperature of about 400° C. to about 600° C.,
wherein the loading of platinum group metal onto the length of porous wall permeated with the oxidation catalyst is in the range of about 0.1 g/ft3 to about 50 g/ft3.

### Claim 18 (depends on 17)

The method of claim 17, wherein a copper or iron promoted CHA structure type molecular sieve is mixed with the plurality of platinum group metal impregnated particles to form a slurry, and the length of porous wall permeated with the slurry is in the range of about 10% to about 50% of the wall length extending from the outlet end of the passages.