Bead milled spray dried nano-explosive
AssigneeThe United States of America as represented by the Secretary of the Army
InventorsRajen Patel, Victor Stepanov, Ashok Surapaneni, Anthony DiStasio, Hongwei Qiu
Life of this patent
Estimating the term…
Loading patent…
AssigneeThe United States of America as represented by the Secretary of the Army
InventorsRajen Patel, Victor Stepanov, Ashok Surapaneni, Anthony DiStasio, Hongwei Qiu
Estimating the term…
A method for manufacturing nano-sized insensitive high explosive molding powder usable as a booster HE is provided herein. The method preferably involving the steps of dissolving a binder in a liquid and suspending crystalline high explosive to said liquid, grinding that suspension in a bead mill until the crystalline high explosive is nano-sized, and precipitating the binder and crystalline high explosive using a spray dryer to produce granules containing nano-sized crystalline high explosive. The liquid may be water or an organic solvent so long as the binder is highly soluble in the liquid and the crystalline high explosive is generally insoluble in the liquid. A fatty alcohol, water defoaming/dispersant/surfactant agent can be added to the dissolved binder/suspended crystalline high explosive, to aid in the manufacturability.
A method of manufacture of an insensitive high explosive molding powder comprising: