# US 11,078,147 B2 · Method for preparing acrolein

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,078,147 B2
- Document ID: US11078147B2
- Status: Granted
- Kind: B2
- Application number: 16/980,934
- Filed: 2019-02-21
- Published: 2020-12-31
- Granted: 2021-08-03
- Earliest claimed: 2018-03-21
- Assignees: Rohm and Haas Company
- Applicants: Rohm and Haas Company
- Inventors: Donald A. Ebert; Timothy Allen Hale; Brian Robert Keyes; Justin Rose; Jinsuo Xu
- Web page: https://patentgrep.com/patent/US11078147B2

## CPC

- C07C 45/35: in propene or isobutene
- C07C 47/22: Acryaldehyde; Methacryaldehyde
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

Provided is a process for preparing acrolein by catalytic gas phase oxidation comprising (a) providing a reaction gas comprising (i) 5 to 10 mol % propylene, (ii) 0.02 to 0.75 mol % propane, and (iii) 0.25 to 1.9 mol % of a fuel mixture comprising at least one of methane and ethane, wherein the molar ratio of the total amount of propane, methane, and ethane to the total amount of propylene is from 0.01:1 to 0.25:1, and (b) contacting the reaction gas with a mixed metal oxide catalyst comprising one or more of molybdenum, bismuth, cobalt, and iron.

## Claims

### Claim 1

A process for preparing acrolein by catalytic gas phase oxidation comprising:
(a) providing a reaction gas comprising
(i) 5 to 10 mol % propylene,
(ii) 0.02 to 0.75 mol % propane, and
(iii) 0.25 to 1.9 mol % of a fuel mixture comprising at least one of methane and ethane,
wherein the molar ratio of the total amount of propane, methane, and ethane to the total amount of propylene is from 0.01:1 to 0.25:1; and
(b) contacting the reaction gas with a mixed metal oxide catalyst to form a mixture comprising acrolein, wherein the mixed metal oxide catalyst comprises one or more of molybdenum, bismuth, cobalt, and iron.

### Claim 2 (depends on 1)

The process of claim 1, wherein the fuel mixture comprises methane.

### Claim 3 (depends on 1)

The process of claim 1, wherein the reaction gas comprises propylene in an amount of from 7.5 to 8.2 mol %.

### Claim 4 (depends on 1)

The process of claim 1, wherein the reaction gas comprises propane in an amount of from 0.03 to 0.62 mol %.

### Claim 5 (depends on 1)

The process of claim 1, wherein the reaction gas comprises the fuel mixture in an amount of from 0.5 to 1.4 mol %.

### Claim 6 (depends on 2)

The process of claim 2, wherein the reaction gas comprises methane in an amount of from 1.1 to 1.4 mol %.

### Claim 7 (depends on 1)

The process of claim 1, wherein the molar ratio of the total amount of propane, methane, and ethane to the total amount of propylene is from 0.1:1 to 0.18:1.

### Claim 8 (depends on 1)

The process of claim 1, wherein the mixed metal oxide catalyst comprises (1) a primary component selected from the group consisting of molybdenum, bismuth, and combinations thereof, and (2) a secondary component selected from the group consisting of cobalt, iron, nickel, zinc, tungsten, phosphorous, manganese, potassium, magnesium, silicon, aluminum, and combinations thereof, wherein the primary component and secondary component are in an atomic ratio of from 9:28 to 28:9.

### Claim 9 (depends on 1)

The process of claim 1, wherein the fuel mixture comprises sulfur in an amount of less than 30 parts per million by volume of the fuel mixture.

### Claim 10

A process for preparing acrolein by catalytic gas phase oxidation comprising:
(a) providing a reaction gas comprising
(i) 7.5 to 8.2 mol % propylene,
(ii) 0.03 to 0.62 mol % propane, and
(iii) 0.5 to 1.4 mol % of a fuel mixture comprising at least one of methane and ethane, wherein the fuel mixture comprises sulfur in an amount of less than 30 parts per million by volume of the fuel mixture,
wherein the molar ratio of the total amount of propane, methane, and ethane to the total amount of propylene is from 0.1:1 to 0.18:1; and
(b) contacting the reaction gas with a mixed metal oxide catalyst to form a mixture comprising acrolein, wherein the mixed metal oxide catalyst comprises (1) a primary component selected from the group consisting of molybdenum, bismuth, and combinations thereof, and (2) a secondary component selected from the group consisting of cobalt, iron, nickel, zinc, tungsten, phosphorous, manganese, potassium, magnesium, silicon, aluminum, and combinations thereof, wherein the primary component and secondary component are in an atomic ratio of from 9:28 to 28:9.