Rubber compositions containing carbon black and whey protein
AssigneeBridgestone Americas Tire Operations, LLC
InventorsBenjamin C. Galizio, Amy M. Randall, Melissa M. Clark
Life of this patent
Estimating the term…
Abstract
The present disclosure is directed to rubber compositions comprising at least one rubber, at least one reinforcing carbon black filler, and a whey protein component. The whey protein component is in an amount sufficient to provide about 0.1 to about 5 phr whey protein. The present disclosure is also directed to methods of preparing such rubber compositions and to tire components containing the rubber compositions disclosed herein.
Claims20
A method for modifying cross-linking of a reinforcing carbon black filler-containing tire rubber composition, the method comprising
- mixing ingredients comprising
- a whey protein powder in an amount sufficient to provide about 0.1 to about 5 phr of whey protein, at least one rubber, about 5 to about 50 phr of at least one reinforcing carbon black, reinforcing silica filler in an amount such that the total amount of reinforcing filler is about 50 to about 200 phr and the reinforcing silica filler is 50-99% by weight of the total amount of reinforcing filler, and a cure package,
- wherein the mixing includes at least one non-productive master-batch stage conducted at a temperature of about 130 to about 200° C. during which the at least one rubber and the whey protein powder are added.
A method for modifying cross-linking of a reinforcing carbon black filler-containing tire rubber composition, the method comprising
- mixing ingredients comprising
- a whey protein powder in an amount sufficient to provide about 0.1 to about 5 phr of whey protein;
- at least one rubber selected from the group consisting of styrene-butadiene rubber, polybutadiene rubber, polyisoprene, natural rubber, and combinations thereof;
- about 5 to about 50 phr of at least one reinforcing carbon black;
- reinforcing silica filler in an amount such that the total amount of reinforcing filler is about 50 to about 200 phr and the reinforcing silica filler is about 80 to about 99% by weight of the total amount of reinforcing filler;
- and a cure package,
- wherein the mixing includes at least one non-productive master-batch stage conducted at a temperature of about 130 to about 200° C. during which the at least one rubber and the whey protein powder are added.
Dependencies are inferred from the claim text.