# US 11,001,039 B2 · Resin film for laminated glass, and laminated glass and preparation thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 11,001,039 B2
- Document ID: US11001039B2
- Status: Granted
- Kind: B2
- Application number: 16/696,806
- Filed: 2019-11-26
- Published: 2020-03-26
- Granted: 2021-05-11
- Earliest claimed: 2017-06-15
- Assignees: Skc Co., Ltd.
- Applicants: Skc Co., Ltd.
- Inventors: Kyu-Hun Kim; Jewon Yeon; Sung Jin Chung; Heung Sik Kim; Hyejin Kim; Hak Soo Lee
- Web page: https://patentgrep.com/patent/US11001039B2

## CPC

- B32B 17/10761: {containing vinyl acetal}
- B32B 17/10036: {comprising two outer glass sheets}
- B32B 17/10577: {Surface roughness}
- B32B 17/10678: {comprising UV absorbers or stabilizers, e.g. antioxidants}
- B32B 17/10688: {Adjustment of the adherence to the glass layers}
- B32B 17/10954: {by using an aligning laminating device}
- B32B 37/182: {one or more of the layers being plastic}
- B32B 17/10596: {created by melt fracture}
- B32B 17/10935: {as a preformed layer, e.g. formed by extrusion}
- B32B 2250/03: 3 layers
- B32B 2307/102: Insulating
- C09J 159/00: Adhesives based on polyacetals; Adhesives based on derivatives of polyacetals
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

A resin film for laminated glass, laminated glass including the resin film, and a process for manufacturing the laminated glass are disclosed. The resin film for laminated glass comprises a resin layer comprising a polyvinyl acetal resin and a contact surface in direct contact with glass, wherein the contact surface has an Rz roughness of 25 to 90 μm and a maximum static friction coefficient at 20° C. of 0.85 to 1.60, and the compressive elastic deformation index measured in the perpendicular direction from the contact surface at 35° C. is 40 to 310 μm/N.

## Claims

### Claim 1

A resin film for laminated glass, which comprises:
a resin layer comprising a polyvinyl acetal resin and a contact surface in direct contact with glass,
wherein the contact surface has an Rz roughness of 25 to 90 μm, a maximum static friction coefficient at 20° C. of 0.85 to 1.60, a maximum static friction coefficient at 40° C. of 1.05 to 1.80, and a maximum static friction coefficient at 45° C. of 1.20 to 2.10,
wherein a content of OH group in the polyvinyl acetal resin is 36 to 54% by mole, and
wherein a compressive elastic deformation index defined by the following Equation 1 and measured in the perpendicular direction from the contact surface at 35° C. is 40 to 310 μm/N:
Compressive elastic deformation index=d/F Equation 1
wherein F is a force of 0.05 to 0.6 N applied in the direction perpendicular to the contact surface by a tip having a flat end and a diameter of 4 mm, and d is a depth that is compressively deformed in the perpendicular direction by the tip.

### Claim 2 (depends on 1)

The resin film for laminated glass of claim 1, which has a compressive elastic deformation index of 80 to 310 μm/N when F is 0.05 to 0.2 N and a compressive elastic deformation index of 60 to 140 μm/N when F is 0.2 to 0.4 N.

### Claim 3 (depends on 1)

The resin film for laminated glass of claim 1, wherein the resin layer further comprises a plasticizer.

### Claim 4 (depends on 3)

The resin film for laminated glass of claim 3, wherein the resin layer comprises 20 to 50 parts by weight of the plasticizer based on 100 parts by weight of the first polyvinyl acetal resin, and the plasticizer is at least one selected from the group consisting of an ester-based plasticizer and a phosphoric acid-based plasticizer.

### Claim 5 (depends on 3)

The resin film for laminated glass of claim 3, wherein the polyvinyl acetal resin is prepared from a mixture of polyvinyl alcohols that comprise 5 to 15% by weight of a polyvinyl alcohol having a degree of polymerization of 1,000 to 1,300, 70 to 85% by weight of a polyvinyl alcohol having a degree of polymerization of 1,500 to 1,900, and 8 to 25% by weight of a polyvinyl alcohol having a degree of polymerization of 2,000 to 2,500.

### Claim 6 (depends on 1)

The resin film for laminated glass of claim 1, wherein the thickness of the resin layer is 580 to 940 μm, and the upper and lower sides of the resin layer are in contact with glass, respectively.

### Claim 7 (depends on 1)

A laminated glass, which comprises a first glass panel; the resin film for laminated glass of claim 1; and a second glass panel sequentially laminated.

### Claim 8 (depends on 1)

A process for manufacturing a laminated glass, which comprises:
(1) disposing the resin film for laminated glass of claim 1 on a first glass panel;
(2) disposing a second glass panel on the resin film for laminated glass; and
(3) aligning the second glass panel with respect to the first glass panel.

### Claim 9

A resin film for laminated glass, which comprises a structure in which a first skin layer, an intermediate resin layer, and a second skin layer are sequentially laminated,
wherein the first skin layer and the second skin layer each comprise a first contact surface or a second contact surface in direct contact with glass,
the first skin layer and the second skin layer each comprise a first polyvinyl acetal resin,
the first contact surface and the second contact surface each have an Rz roughness of 25 to 90 μm, a maximum static friction coefficient at 20° C. of 0.85 to 1.60, a maximum static friction coefficient at 40° C. of 1.05 to 1.80, and a maximum static friction coefficient at 45° C. of 1.20 to 2.10,
wherein a content of OH group in the first polyvinyl acetal resin is 36 to 54% by mole, and
wherein a compressive elastic deformation index defined by the following Equation 1 and measured in the perpendicular direction from each of the first contact surface and the second contact surface at 35° C. is 40 to 310 μm/N:
Compressive elastic deformation index=d/F Equation 1
wherein F is a force of 0.05 to 0.6 N applied in the direction perpendicular to the contact surface by a tip having a flat end and a diameter of 4 mm, and d is a depth that is compressively deformed in the perpendicular direction by the tip.

### Claim 10 (depends on 9)

The resin film for laminated glass of claim 9, wherein the thicknesses of the first skin layer and the thicknesses of the second skin layer are 250 to 400 μm, respectively, and the thickness of the intermediate resin layer is 80 to 140 μm.

### Claim 11 (depends on 9)

The resin film for laminated glass of claim 9, wherein the intermediate resin layer comprises a second polyvinyl acetal resin and a plasticizer,
the intermediate resin layer comprises 30 to 40 parts by weight of the plasticizer based on 100 parts by weight of the second polyvinyl acetal resin, and
a content of OH group in the second polyvinyl acetal resin is 5 to 30% by mole.

### Claim 12 (depends on 9)

A laminated glass, which comprises a first glass panel; the resin film for laminated glass of claim 9; and a second glass panel sequentially laminated.

### Claim 13 (depends on 9)

A process for manufacturing a laminated glass, which comprises:
(1) disposing the resin film for laminated glass of claim 9 on a first glass panel;
(2) disposing a second glass panel on the resin film for laminated glass; and
(3) aligning the second glass panel with respect to the first glass panel.