Abstract
A method for producing a foamed blow-molded article, which includes extruding a physical blowing agent-containing foamable molten resin downwardly through a annular die to form a tubular foamed parison, clamping the foamed parison between split molds, and then blow molding it. At the latest before completion of the clamping of the foamed parison between the split molds, a gas is blown toward an inner peripheral surface of an upper portion of the foamed parison, the bottom portion of which has been closed, from a gas ejection outlet located within the foamed parison at a position immediately below the annular die to widen the foamed parison.
Claims15
A method for producing a foamed blow-molded article, comprising the steps of:
- (a) extruding a physical blowing agent-containing foamable molten resin vertically downwardly through an annular die to form a tubular foamed parison,
- (b) closing a bottom portion of the foamed parison,
- (c) blowing a gas toward a whole inner peripheral surface of an upper portion of the foamed parison, the bottom portion of which has been closed, from a gas ejection outlet located within the foamed parison at a position below the annular die to form a gas stream that directly impinges upon the whole inner peripheral surface and to widen the foamed parison,
- (d) closing split molds to clamp the foamed parison therebetween, and
- (e) blow molding the foamed parison within the split molds,
- wherein step (c) is carried out at the latest before completion of step (d),
- wherein the gas ejection outlet is positioned only between just below a resin discharge outlet of the annular die and above the split molds, and
- wherein the upper portion of the foamed parison is a portion of the foamed parison from the resin discharge outlet of the annular die to ⅓ the length of the foamed parison, said length being a vertical length between the resin discharge outlet of the annular die and the closed bottom portion of the foamed parison,
- wherein a ratio (D2/D1) of a perimeter length (D2) of the foamed parison that has been widened in step (c) to a perimeter length (D1) of the resin discharge outlet of the annular die is 3.0 to 5, and
- wherein the foamed blow-molded article obtained in step (e) has an apparent density of 0.1 to 0.25 g/cm3 and an average wall thickness of 1 to 4 mm.
A method for producing a foamed blow-molded article, comprising the steps of:
- (a) extruding a physical blowing agent-containing foamable molten resin vertically downwardly through an annular die to form a tubular foamed parison,
- (b) closing a bottom portion of the foamed parison,
- (c) blowing a gas toward a whole inner peripheral surface of an upper portion of the foamed parison, the bottom portion of which has been closed, from a gas ejection outlet located within the foamed parison at a position below the annular die to form a gas stream that directly impinges upon the whole inner peripheral surface and to widen the foamed parison,
- (d) closing split molds to clamp the foamed parison therebetween, and
- (e) blow molding the foamed parison within the split molds,
- wherein step (c) is carried out at the latest before completion of step (d),
- wherein the gas ejection outlet is positioned only between just below a resin discharge outlet of the annular die and above the split molds,
- wherein, in step (c), the gas is ejected from the gas ejection outlet at an angle of 70-110 degrees relative to the vertical direction, and
- wherein the gas ejection outlet is an annular slit and the gas is ejected from the gas ejection slit in all 360 degrees directions around a centerline of the annular die only towards the upper portion of the foamed parison,
- wherein a ratio (D2/D1) of a perimeter length (D2) of the foamed parison that has been widened in step (c) to a perimeter length (D1) of the resin discharge outlet of the annular die is 3.0 to 5, and
- wherein the foamed blow-molded article obtained in step (e) has an apparent density of 0.1 to 0.25 g/cm3 and an average wall thickness of 1 to 4 mm.
A method for producing a foamed blow-molded article, comprising the steps of:
- (a) extruding a physical blowing agent-containing foamable molten resin vertically downwardly through an annular die to form a tubular foamed parison,
- (b) closing a bottom portion of the foamed parison,
- (c) blowing a gas in a nearly horizontal direction toward a whole inner peripheral surface of an upper portion of the foamed parison, the bottom portion of which has been closed, from a gas ejection outlet located within the foamed parison at a position below the annular die to form a gas stream that directly impinges upon the whole inner peripheral surface and to widen the foamed parison,
- (d) closing split molds to clamp the foamed parison therebetween, and
- (e) blow molding the foamed parison within the split molds,
- wherein step (c) is carried out at the latest before completion of step (d), and
- wherein the gas ejection outlet is positioned only between just below a resin discharge outlet of the annular die and above the split molds and only ejects the gas toward the upper portion of the foamed parison,
- wherein a ratio (D2/D1) of a perimeter length (D2) of the foamed parison that has been widened in step (c) to a perimeter length (D1) of the resin discharge outlet of the annular die is 3.0 to 5, and
- wherein the foamed blow-molded article obtained in step (e) has an apparent density of 0.1 to 0.25 g/cm3 and an average wall thickness of 1 to 4 mm.