Adsorbent and method for producing the same
AssigneesJnc Corporation, SofSera Corporation
InventorsYoshihiro Matsumoto, Akihiro Uchida, Yasuto Umeda
Life of this patent
Estimating the term…
Abstract
An adsorbent, which can be produced by a method in which a particle size, a pore size, a specific surface area or the like can be easily controlled, and is suitable for isolation of biomolecules. The adsorbent contains aggregates of calcium phosphate-based particles, and has an average pore size of 15 to 36 nanometers and a specific surface area of 40 to 90 m2/mL when measurement is carried out by mercury porosimetry.
Claims16
An adsorbent, comprising aggregates of calcium phosphate-based particles and having an average pore size of 15 to 24 nanometers and a specific surface area of 50 to 90 m2/mL when measurement is carried out by mercury porosimetry.
A method for producing an adsorbent, comprising:
- (a) spray-drying slurry containing calcium phosphate-based particles having an average major-axis size of 20 to 50 nanometers to obtain aggregates of calcium phosphate-based particles, and
- (b) calcining the aggregates of calcium phosphate-based particles at a temperature of 100 to 600° C.,
- wherein the produced adsorbent comprises aggregates of calcium phosphate-based particles and has an average pore size of 15 to 24 nanometers and a specific surface area of 50 to 90 m2/mL when measurement is carried out by mercury porosimetry.