# US 10,957,918 B2 · Stable electrolyte matrix for molten carbonate fuel cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,918 B2
- Document ID: US10957918B2
- Status: Granted
- Kind: B2
- Application number: 16/938,281
- Filed: 2020-07-24
- Published: 2020-11-12
- Granted: 2021-03-23
- Earliest claimed: 2016-11-04
- Assignees: FuelCell Energy, Inc.
- Applicants: FuelCell Energy, Inc.
- Inventors: Abdelkader Hilmi; Arun Surendranath; Chao-Yi Yuh; Mohammad Farooque
- Web page: https://patentgrep.com/patent/US10957918B2

## CPC

- H01M 8/0295: Matrices for immobilising electrolyte melts
- H01M 8/145: {comprising carbonates}
- H01M 2008/147: {Fuel cells with molten carbonates}
- H01M 2300/0051: Carbonates
- H01M 2300/0091: in the form of mixtures
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of making an electrolyte matrix includes: preparing a slurry comprising a support material, a coarsening inhibitor, an electrolyte material, and a solvent; and drying the slurry to form an electrolyte matrix. The support material comprises lithium aluminate, the coarsening inhibitor comprises a material selected from the group consisting of MnO2, Mn2O3, TiO2, ZrO2, Fe2O3, LiFe2O3, and mixtures thereof, and the coarsening inhibitor has a particle size of about 0.005 μm to about 0.5 μm.

## Claims

### Claim 1

A method of making an electrolyte matrix comprising:
preparing a slurry comprising:
a support material comprising lithium aluminate,
a coarsening inhibitor comprising a material selected from the group consisting of MnO2, Mn2O3, TiO2, ZrO2, Fe2O3, LiFe2O3, and mixtures thereof, wherein the coarsening inhibitor has a particle size of about 0.005 μm to about 0.5 μm, and wherein the coarsening inhibitor has a BET surface area of about 10 m2/g to about 50 m2/g,
an electrolyte material,
a reinforcing material having an average particle size in a range of about 10 μm to about 120 μm, and
a solvent; and
drying the slurry to form an electrolyte matrix.

### Claim 2 (depends on 1)

The method of claim 1, wherein preparing the slurry comprises an attrition milling process that reduces the size of the materials in the slurry.

### Claim 3 (depends on 1)

The method of claim 1, further comprising tape casting the slurry before drying the slurry.

### Claim 4 (depends on 1)

The method of claim 1, further comprising adding a binder, a plasticizer, or a combination thereof to the slurry.

### Claim 5 (depends on 1)

The method of claim 1, wherein the coarsening inhibitor is present in an amount of about 0.1 vol. % to about 40 vol. % of dry components of the slurry.

### Claim 6

A method of making an electrolyte matrix comprising:
forming a mixture of an aluminum containing precursor, a lithium containing precursor, and a dopant precursor, wherein the dopant precursor is in oxide or salt form;
drying the mixture to form a powder;
heat treating the powder at a temperature of about 550° C. to about 800° C. for a period of about 6 hours to about 30 hours to form a lithium aluminate including a dopant, wherein the dopant comprises a material selected from the group consisting of MnO2, Mn2O3, TiO2, ZrO2, Fe2O3, LiFe2O3 and mixtures thereof;
preparing a slurry comprising the lithium aluminate including the dopant, an electrolyte material, and a solvent; and
drying the slurry to form an electrolyte matrix.

### Claim 7 (depends on 6)

The method of claim 6, wherein the dopant precursor comprises MnO2, TiO2, ZrO2, Fe2O3, or mixtures thereof.

### Claim 8 (depends on 6)

The method of claim 6, wherein the aluminum precursor comprises Al2O3.

### Claim 9 (depends on 6)

The method of claim 6, wherein the lithium precursor comprises lithium carbonate.

### Claim 10 (depends on 6)

The method of claim 6, further comprising tape casting the slurry before drying the slurry.

### Claim 11 (depends on 6)

The method of claim 6, further comprising adding a binder, a plasticizer, a reinforcing material, or a combination thereof to the slurry.

### Claim 12 (depends on 6)

The method of claim 6, wherein the lithium aluminate including a dopant comprises the dopant in an amount of about 0.1 mol. % to about 15 mol. %.

### Claim 13 (depends on 1)

The method of claim 1, wherein the coarsening inhibitor is provided as a dopant within the support material.