# US 10,957,903 B2 · Layered lithium-rich manganese-based cathode material with olivine structured LIMPO4 surface modification and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,903 B2
- Document ID: US10957903B2
- Status: Granted
- Kind: B2
- Application number: 16/088,830
- Filed: 2016-12-08
- Published: 2020-10-15
- Granted: 2021-03-23
- Earliest claimed: 2016-03-27
- Assignees: South China University of Technology
- Applicants: South China University of Technology
- Inventors: Chenghao Yang; Fenghua Zheng; Xunhui Xiong; Meilin Liu
- Web page: https://patentgrep.com/patent/US10957903B2

## CPC

- H01M 4/366: {as layered products}
- C01B 25/45: containing plural metal, or metal and ammonium
- C01G 53/502: containing lithium and cobalt
- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/50: Solid solutions
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/03: obtained by SEM
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- C01P 2004/84: one phase coated with the other
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention provides a layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification and a preparation method thereof. The preparation method comprises: firstly, preparing a pure-phase layered lithium-rich manganese-based cathode material by using a coprecipitation method and a high temperature sintering method, and then uniformly coating and doping olivine-structured LiMPO4 to the surface of the layered lithium-manganese-rich composite cathode material by using a sol-gel method. According to the present invention, the surface of the layered lithium-rich manganese-based cathode material is modified by olivine structured LiMPO4, such that cycle stability thereof is effectively improved, and voltage drop generated by the material in the cycle course is inhibited. The preparation method according to the present invention is simple, low cost, environmentally friendly, and is suitable for large-scale industrial production.

## Claims

### Claim 1

A preparation method of a layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification, comprising steps of:
1) weighing a nickel salt, a cobalt salt and a manganese salt and dissolving the nickel salt, the cobalt salt and the manganese salt in deionized water respectively to formulate salt solutions of each having a concentration of 0.5-2 mol/L, wherein the nickel salt, the cobalt salt and the manganese salt are weighed based on a molar ratio of Ni, Co and Mn in a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, where 0.4≤x≤0.6, 0.1≤y≤0.2;
2) dissolving alkali and ammonia water in the deionized water to formulate a mixed alkali solution, wherein a concentration of the alkali is 2-10 mol/L, and a molar concentration of the ammonia water is 2-5 mol/L;
3) adding the mixed alkali solution obtained in step 2) into a reactor, wherein a volume of the mixed alkali solution accounts for 30% to 50% of a volume of the reactor, and controlling a pH value between 9 and 12, and controlling a temperature between 60° C. and 80° C.;
4) respectively adding the salt solutions of the nickel salt, the cobalt salt and the manganese salt formulated in step 1) into the reactor via a peristaltic pump at a constant speed, wherein in step 4), the pH value is between 9 and 12, and the temperature is between 60° C. and 80° C.;
5) after finished adding the salt solutions of the nickel salt, the cobalt salt and the manganese salt, standing still and aging for 12-20 hours, followed by filtering a precipitate, washing the precipitate and drying the precipitate;
6) uniformly mixing the precipitate with a lithium salt, presintering a mixture of the precipitate and the lithium salt at a presintering temperature of 450-550° C. for 3-5 hours, and then calcining the mixture of the precipitate and the lithium salt at a calcining temperature of 750-950° C. for 10-16 hours to obtain a pure-phase layered lithium-rich manganese-based cathode material; wherein a molar ratio of the precipitate to the lithium salt is 1:(1.05-1.1);
7) totally dissolving a lithium source, a transition metal source, a phosphorus source and an additive in the deionized water at a molar ratio of 1:1:1:(1-5), followed by adding the pure-phase layered lithium-rich manganese-based cathode material obtained in step 6), evaporating to dry at an evaporating temperature of 80-100° C. to form a gel; and
8) vacuum drying the gel obtained in step 7) at a vacuum drying temperature of 100-120° C., crushing the gel, and precalcining the gel at a precalcining temperature of 400 600° C. for 4-6 hours to obtain the layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein in step 1), the nickel salt is one or more of nickel sulfate, nickel nitrate and nickel acetate; the cobalt salt is one or more of cobalt sulfate, cobalt nitrate and cobalt acetate; the manganese salt is one or more of manganese sulfate, manganese nitrate and manganese acetate.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein in step 2), the alkali is one or more of a sodium hydroxide solution and a potassium hydroxide solution, and the concentration of the alkali is 2-5 mol/L; a molar ratio of sodium hydroxide to the ammonia water is 2:1.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein in step 6), the lithium salt is one or more of lithium hydroxide, lithium carbonate and lithium acetate.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein in step 6), the presintering temperature is raised to 450 550° C. at a heating rate of 1-5° C./min and is maintained for 3-5 hours; and then the calcining temperature is raised to 750-950° C. at the heating rate of 1-5° C./min and is maintained for 10-16 hours.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein in step 7), the lithium source is one or more of lithium hydroxide, lithium dihydrogen phosphate and lithium carbonate.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein in step 7), the transition metal source is one or more of ferrous sulfate, ferrous nitrate, ferrous oxalate and ferrous acetate.

### Claim 8 (depends on 1)

The preparation method according to claim 1, wherein in step 7), the phosphorus source is one or more of ammonium dihydrogen phosphate, ammonium hydrogen phosphate and phosphoric acid; and the additive is one or more of citric acid, tartaric acid, glucose and sucrose, and an amount of the additive is controlled to be 20-50% of a mass of the transition metal source.

### Claim 9 (depends on 1)

The preparation method according to claim 1, wherein in step 8), the precalcining temperature is raised to 400° C. to 600° C. at a heating rate of 1-5° C./min and is maintained for 4-6 hours.

### Claim 10 (depends on 1)

A layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification obtained by using a preparation method according to claim 1, wherein the layered lithium-rich manganese-based cathode material has a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, wherein x and y are moles, 0.4≤x≤0.6 and 0.1≤y≤0.2; an olivine structured LiMPO4 coating layer of the layered lithium-rich manganese-based cathode material is LiNiPO4, LiCoPO4, LiMnPO4, LiFePO4, LiCuPO4, LiAlPO4, LiMoPO4 or LiMgPO4, and a mass of the olivine structured LiMPO4 coating layer is controlled to be 1-10% of a mass of the layered lithium-rich manganese-based cathode material.

### Claim 11 (depends on 2)

A layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification obtained by using a preparation method according to claim 2, wherein the layered lithium-rich manganese-based cathode material has a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, wherein x and y are moles, 0.4≤x≤0.6 and 0.1≤y≤0.2; an olivine structured LiMPO4 coating layer of the layered lithium-rich manganese-based cathode material is LiNiPO4, LiCoPO4, LiMnPO4, LiFePO4, LiCuPO4, LiAlPO4, LiMoPO4 or LiMgPO4, and a mass of the olivine structured LiMPO4 coating layer is controlled to be 1-10% of a mass of the layered lithium-rich manganese-based cathode material.

### Claim 12 (depends on 3)

A layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification obtained by using a preparation method according to claim 3, wherein the layered lithium-rich manganese-based cathode material has a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, wherein x and y are moles, 0.4≤x≤0.6 and 0.1≤y≤0.2; an olivine structured LiMPO4 coating layer of the layered lithium-rich manganese-based cathode material is LiNiPO4, LiCoPO4, LiMnPO4, LiFePO4, LiCuPO4, LiAlPO4, LiMoPO4 or LiMgPO4, and a mass of the olivine structured LiMPO4 coating layer is controlled to be 1-10% of a mass of the layered lithium-rich manganese-based cathode material.

### Claim 13 (depends on 4)

A layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification obtained by using a preparation method according to claim 4, wherein the layered lithium-rich manganese-based cathode material has a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, wherein x and y are moles, 0.4≤x≤0.6 and 0.1≤y≤0.2; an olivine structured LiMPO4 coating layer of the layered lithium-rich manganese-based cathode material is LiNiPO4, LiCoPO4, LiMnPO4, LiFePO4, LiCuPO4, LiAlPO4, LiMoPO4 or LiMgPO4, and a mass of the olivine structured LiMPO4 coating layer is controlled to be 1-10% of a mass of the layered lithium-rich manganese-based cathode material.

### Claim 14 (depends on 5)

A layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification obtained by using a preparation method according to claim 5, wherein the layered lithium-rich manganese-based cathode material has a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, wherein x and y are moles, 0.4≤x≤0.6 and 0.1≤y≤0.2; an olivine structured LiMPO4 coating layer of the layered lithium-rich manganese-based cathode material is LiNiPO4, LiCoPO4, LiMnPO4, LiFePO4, LiCuPO4, LiAlPO4, LiMoPO4 or LiMgPO4, and a mass of the olivine structured LiMPO4 coating layer is controlled to be 1-10% of a mass of the layered lithium-rich manganese-based cathode material.

### Claim 15 (depends on 6)

A layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification obtained by using a preparation method according to claim 6, wherein the layered lithium-rich manganese-based cathode material has a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, wherein x and y are moles, 0.4≤x≤0.6 and 0.1≤y≤0.2; an olivine structured LiMPO4 coating layer of the layered lithium-rich manganese-based cathode material is LiNiPO4, LiCoPO4, LiMnPO4, LiFePO4, LiCuPO4, LiAlPO4, LiMoPO4 or LiMgPO4, and a mass of the olivine structured LiMPO4 coating layer is controlled to be 1-10% of a mass of the layered lithium-rich manganese-based cathode material.

### Claim 16 (depends on 7)

A layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification obtained by using a preparation method according to claim 7, wherein the layered lithium-rich manganese-based cathode material has a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, wherein x and y are moles, 0.4≤x≤0.6 and 0.1≤y≤0.2; an olivine structured LiMPO4 coating layer of the layered lithium-rich manganese-based cathode material is LiNiPO4, LiCoPO4, LiMnPO4, LiFePO4, LiCuPO4, LiAlPO4, LiMoPO4 or LiMgPO4, and a mass of the olivine structured LiMPO4 coating layer is controlled to be 1-10% of a mass of the layered lithium-rich manganese-based cathode material.

### Claim 17 (depends on 8)

A layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification obtained by using a preparation method according to claim 8, wherein the layered lithium-rich manganese-based cathode material has a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, wherein x and y are moles, 0.4≤x≤0.6 and 0.1≤y≤0.2; an olivine structured LiMPO4 coating layer of the layered lithium-rich manganese-based cathode material is LiNiPO4, LiCoPO4, LiMnPO4, LiFePO4, LiCuPO4, LiAlPO4, LiMoPO4 or LiMgPO4, and a mass of the olivine structured LiMPO4 coating layer is controlled to be 1-10% of a mass of the layered lithium-rich manganese-based cathode material.

### Claim 18 (depends on 9)

A layered lithium-rich manganese-based cathode material with olivine structured LiMPO4 surface modification obtained by using a preparation method according to claim 9, wherein the layered lithium-rich manganese-based cathode material has a chemical formula of Li1.2MnxNiyCo0.8-x-yO2, wherein x and y are moles, 0.4≤x≤0.6 and 0.1≤y≤0.2; an olivine structured LiMPO4 coating layer of the layered lithium-rich manganese-based cathode material is LiNiPO4, LiCoPO4, LiMnPO4, LiFePO4, LiCuPO4, LiAlPO4, LiMoPO4 or LiMgPO4, and a mass of the olivine structured LiMPO4 coating layer is controlled to be 1-10% of a mass of the layered lithium-rich manganese-based cathode material.