# US 10,957,899 B2 · Method of preparing lithium metal oxide and method of manufacturing lithium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,899 B2
- Document ID: US10957899B2
- Status: Granted
- Kind: B2
- Application number: 16/220,338
- Filed: 2018-12-14
- Published: 2019-06-20
- Granted: 2021-03-23
- Earliest claimed: 2017-12-15
- Assignees: SK Innovation Co., Ltd.
- Applicants: SK Innovation Co., Ltd.
- Inventors: Mi Jung Noh; Jik Soo Kim; Kook Hyun Han
- Web page: https://patentgrep.com/patent/US10957899B2

## CPC

- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/058: Construction or manufacture
- H01M 4/0404: {by coating on electrode collectors}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

In a method of preparing a lithium metal oxide, a preliminary lithium metal oxide is prepared. The preliminary lithium metal oxide is washed using an organic washing solution to remove lithium salt impurities. The organic washing solution includes an organic solvent and a multivalent carboxylic acid compound. A minimum distance between oxygen atoms included in different carboxylic acid groups neighboring each other in the multivalent carboxylic acid compound is 220 pm or more.

## Claims

### Claim 1

A method of preparing a lithium metal oxide, the method comprising:
preparing a preliminary lithium metal oxide; and
washing the preliminary lithium metal oxide using an organic washing solution to remove lithium salt impurities, wherein the organic washing solution includes an organic solvent and a multivalent carboxylic acid compound, and a minimum distance between oxygen atoms included in different carboxylic acid groups neighboring each other in the multivalent carboxylic acid compound is equal to or greater than 220 pm; and
filtering the washed preliminary lithium metal oxide to remove the multivalent carboxylic acid compound capturing the lithium salt impurities from the washed preliminary lithium metal oxide.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the minimum distance is in a range from 220 pm to about 500 pm.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the lithium salt impurities include LiOH and Li2CO3.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the multivalent carboxylic acid compound includes at least one selected from the group consisting of maleic acid, oxalic acid and poly acrylic acid (PAA).

### Claim 5 (depends on 1)

The method according to claim 1, wherein the organic solvent includes alcohol.

### Claim 6 (depends on 1)

The method according to claim 1, further comprising, before or after washing the preliminary lithium metal oxide using the organic washing solution, firing the preliminary lithium metal oxide.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the lithium metal oxide includes a compound represented by Chemical Formula 1 below:
Li1+αNi1−(x+y)CoxMyO2 Chemical Formula 1
wherein −0.05≤α≤0.15, 0.01≤x≤0.2, 0≤y≤0.2, and M is at least one element selected from the group consisting of Mg, Sr, Ba, B, Al, Si, Mn, Ti, Zr, and W.

### Claim 8 (depends on 1)

A method of manufacturing a lithium secondary battery, the method comprising:
preparing a cathode active material including the lithium metal oxide prepared according to claim 1;
coating the cathode active material on a cathode current collector to form a cathode; and
forming an anode facing the cathode with respect to a separation layer.