# US 10,957,851 B2 · Magnetic layer for magnetic random access memory (MRAM) by moment enhancement

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,851 B2
- Document ID: US10957851B2
- Status: Granted
- Kind: B2
- Application number: 16/728,455
- Filed: 2019-12-27
- Published: 2020-05-07
- Granted: 2021-03-23
- Earliest claimed: 2018-08-22
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Guenole Jan; Jodi Mari Iwata; Ru-Ying Tong; Huanlong Liu; Yuan-Jen Lee; Jian Zhu
- Web page: https://patentgrep.com/patent/US10957851B2

## CPC

- H10N 50/01: Manufacture or treatment
- G11C 11/161: {details concerning the memory cell structure, e.g. the layers of the ferromagnetic memory cell}
- H01F 10/3286: {Spin-exchange coupled multilayers having at least one layer with perpendicular magnetic anisotropy}
- H01F 41/302: {for applying spin-exchange-coupled multilayers, e.g. nanostructured superlattices (spin-exchange-coupled multilayers H01F10/32)}
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10B 61/10: {comprising components having two electrodes, e.g. diodes or MIM elements}
- H10N 50/10: Magnetoresistive devices
- H10N 50/80: Constructional details
- H10N 50/85: Materials of the active region
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A perpendicularly magnetized magnetic tunnel junction (p-MTJ) is disclosed wherein a boron containing free layer (FL) is subjected to a plasma treatment with inert gas, and a natural oxidation (NOX) process to form B2O3 before overlying layers are deposited. A metal layer such as Mg is deposited on the FL as a first step in forming a Hk enhancing layer that increases FL perpendicular magnetic anisotropy, or as a first step in forming a tunnel barrier layer on the FL. One or more anneal steps are essential in assisting B2O3 segregation from the free layer and thereby increasing the FL magnetic moment. A post-oxidation plasma treatment may also be used to partially remove B2O3 proximate to the FL top surface before the metal layer is deposited. Both plasma treatments use low power (<50 Watts) to remove a maximum of 2 Angstroms FL thickness.

## Claims

### Claim 1

A method comprising:
forming a free layer over a substrate, the free layer including boron (B);
performing a first plasma treatment process with a first inert gas on the free layer;
performing an oxidation process on the free layer to convert boron to boron oxide (B2O3) in the free layer;
forming a metal layer on the free layer; and
performing an annealing process to segregate a first portion of the boron oxide from the free layer.

### Claim 2 (depends on 1)

The method of claim 1, further comprising performing a second plasma treatment process with a second inert gas to remove a second portion of the boron oxide from the free layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the metal layer includes Mg.

### Claim 4 (depends on 1)

The method of claim 1, further comprising:
forming a seed layer over the substrate;
forming a reference layer over the seed layer;
forming a tunnel barrier layer over the reference layer, wherein forming the free layer over the substrate includes forming the free layer over the tunnel barrier layer; and
forming a cap layer over the metal layer.

### Claim 5 (depends on 4)

The method of claim 4, further comprising:
patterning the seed layer, the reference layer, the tunnel barrier layer, the free layer and the cap layer to form a magnetic tunnel junction (MTJ) structure;
encapsulating the MTJ structure with a dielectric material.

### Claim 6 (depends on 5)

The method of claim 5, wherein the performing of the annealing process to segregate the first portion of the boron oxide from the free layer occurs either during the encapsulating of the MTJ structure or after the forming of the metal layer on the free layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein performing the first plasma treatment process with the first inert gas on the free layer includes performing the first plasma treatment process with a radiofrequency power of less than about 50 Watts and with a flow of the first inert gas for less than one minute, and
wherein the first inert gas is selected from the group consisting of Ar, Kr, Xe, and Ne.

### Claim 8 (depends on 1)

The method of claim 1, wherein the performing of the oxidation process on the free layer includes applying a flow of oxygen in a range from about 0.1 to about 1 sccm for a period of time ranging from about one second to about six hundred seconds.

### Claim 9 (depends on 1)

The method of claim 1, wherein the annealing process occurs at a temperature ranging from about 360° to about 400°.

### Claim 10

A method comprising:
forming an Hk enhancing layer over a substrate;
forming a free layer over the Hk enhancing layer, the free layer including boron (B);
performing a first oxidation process on the free layer to convert boron to boron oxide (B2O3) in the free layer;
forming a metal layer on the free layer;
performing a second oxidation process on the metal layer to form a metal oxide layer;
performing an annealing process to segregate a first portion of the boron oxide from the free layer.

### Claim 11 (depends on 10)

The method of claim 10, further comprising performing a first plasma treatment process with a first inert gas on the free layer prior to the performing of the first oxidation process.

### Claim 12 (depends on 11)

The method of claim 11, further comprising performing a second plasma treatment process with a second inert gas to remove a second portion of the boron oxide from the free layer.

### Claim 13 (depends on 10)

The method of claim 10, further comprising:
forming a seed layer over the substrate;
forming a reference layer over the metal oxide layer, wherein the metal oxide layer is a tunnel barrier layer; and
forming a cap layer over the reference layer.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
patterning the seed layer, the Hk enhancing layer, the free layer, the tunnel barrier layer, the reference layer and the cap layer to form a magnetic tunnel junction (MTJ) structure; and
encapsulating the MTJ structure with a dielectric material.

### Claim 15 (depends on 10)

The method of claim 10, wherein the performing of the annealing process to segregate the first portion of the boron oxide from the free layer occurs after the performing of the second oxidation process on the metal layer to form the metal oxide layer.

### Claim 16

A method comprising:
forming a free layer over a substrate, the free layer having a first concentration of boron;
performing a treatment process on the free layer to form a treated free layer, the treated free layer having a second concentration of boron that is less than the first concentration, wherein the treatment process includes:
performing a first oxidation process on the free layer to convert boron to boron oxide (B2O3) in the free layer; and
performing a process to segregate a first portion of the boron oxide from the free layer; and
wherein at least a portion of the treated free layer is part of a magnetic tunnel junction (MTJ) structure.

### Claim 17 (depends on 16)

The method of claim 16, wherein performing the treatment process on the free layer to form the treated free layer further includes:
performing a plasma treatment process with a first inert gas on the free layer; and
wherein the performing of the process to segregate the first portion of the boron oxide from the free layer includes performing an annealing process to segregate a first portion of the boron oxide from the free layer to form the treated free layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein performing the treatment process on the free layer to form the treated free layer further includes:
forming a metal layer on the free layer;
performing a second oxidation process on the metal layer to form a metal oxide layer; and
wherein the performing of the process to segregate the first portion of the boron oxide from the free layer includes performing an annealing process to segregate a first portion of the boron oxide from the free layer.

### Claim 19 (depends on 16)

The method of claim 16, further comprising forming a tunnel barrier layer over the substrate, and
wherein forming the free layer over the substrate includes forming the free layer directly on the tunnel barrier layer.

### Claim 20 (depends on 16)

The method of claim 16, further comprising forming an Hk enhancing layer over the substrate, and
wherein forming the free layer over the substrate includes forming the free layer directly on the Hk enhancing layer.