# US 10,957,841 B2 · Capping layer for reducing ion mill damage

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,841 B2
- Document ID: US10957841B2
- Status: Granted
- Kind: B2
- Application number: 16/333,505
- Filed: 2016-09-15
- Published: 2019-08-22
- Granted: 2021-03-23
- Earliest claimed: 2016-09-15
- Assignees: Google Inc.
- Applicants: Google LLC
- Inventors: Anthony Edward Megrant
- Web page: https://patentgrep.com/patent/US10957841B2

## CPC

- H10N 60/805: {for Josephson-effect devices}
- G06N 10/40: Physical realisations or architectures of quantum processors or components for manipulating qubits, e.g. qubit coupling or qubit control
- H10N 60/01: Manufacture or treatment
- H10N 60/0912: {of Josephson-effect devices}
- H10N 60/80: Constructional details
- H10N 60/99: {Alleged superconductivity}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G06N: COMPUTING ARRANGEMENTS BASED ON SPECIFIC COMPUTATIONAL MODELS

## Abstract

A method of fabricating an electrical contact junction that allows current to flow includes: providing a substrate including a first layer of superconductor material; removing a native oxide of the superconductor material of the first layer from a first region of the first layer; forming a capping layer in contact with the first region of the first layer, in which the capping layer prevents reformation of the native oxide of the superconductor material in the first region; forming, after forming the capping layer, a second layer of superconductor material that electrically connects to the first region of the first layer of superconductor material to provide the electrical contact junction that allows current to flow.

## Claims

### Claim 1

A method of fabricating an electrical contact junction that allows a current to flow, the method comprising:
providing a substrate comprising a first layer of superconductor material;
removing a native oxide of the superconductor material of the first layer from a first region of the first layer, wherein removing the native oxide from the first region of the first layer of superconductor material comprises
applying a first photoresist layer to the first layer of superconductor material,
patterning the first photoresist layer to expose the first region of the first layer of superconductor material, and
ion milling the exposed first region of the first layer of superconductor material;
forming a capping layer in contact with the first region of the first layer, wherein the capping layer prevents reformation of the native oxide of the superconductor material in the first region, wherein forming the capping layer comprises
forming the capping layer on the patterned first photoresist layer such that part of the capping layer is in direct contact with the ion milled exposed first region of the first layer of superconductor material, and
removing a section of the capping layer that is not in direct contact with the ion milled exposed first region of the first layer of superconductor material;
forming, after forming the capping layer, a second layer of superconductor material that electrically connects to the first region of the first layer of superconductor material to provide the electrical contact junction that allows current to flow.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the second layer of superconductor material comprises:
applying a second photoresist layer;
patterning the second photoresist layer to expose the capping layer and a portion of a substrate surface; and
forming the second layer of superconductor material on the capping layer and an exposed portion of the substrate surface.

### Claim 3 (depends on 1)

The method of claim 1, wherein forming the second layer of superconductor material comprises:
applying a second photoresist layer;
patterning the second photoresist layer to expose the capping layer and a portion of a substrate surface;
removing the capping layer to expose the first region of the first layer without the native oxide; and
forming the second layer of superconductor material on the exposed first region of the first layer without the native oxide and on the exposed portion of the substrate surface.

### Claim 4 (depends on 1)

The method of claim 1, wherein the capping layer comprises a material that, when subject to ion milling at a predetermined set of ion beam parameters, has an etch rate that is higher than an etch rate of the native oxide subject to the same predetermined set of ion beam parameters.

### Claim 5 (depends on 4)

The method of claim 4, wherein the predetermined set of ion beam parameters comprises a beam voltage, a beam current, and a beam width.

### Claim 6 (depends on 4)

The method of claim 4, wherein the etch rate of the capping layer material is at least five times higher than the etch rate of the native oxide.

### Claim 7 (depends on 4)

The method of claim 4, wherein the etch rate of the capping layer material is at least fifteen times higher than the etch rate of the native oxide.

### Claim 8 (depends on 4)

The method of claim 4, wherein the capping layer material comprises silver or gold.

### Claim 9 (depends on 4)

The method of claim 4, wherein the capping layer material comprises a metal having a thickness such that the metal behaves as a superconductor material due to the superconductivity proximity effect when the electrical contact junction is cooled below a critical temperature of the superconductor material of the first layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein the thickness of the metal is between about 5 nm and about 10 nm.

### Claim 11 (depends on 4)

The method of claim 4, wherein the capping layer material comprises a superconductor material.

### Claim 12 (depends on 11)

The method of claim 11, wherein the superconductor material of the capping layer comprises titanium nitride, rhenium, or ruthenium.

### Claim 13 (depends on 1)

The method of claim 1, wherein the superconductor material of the first layer comprises aluminum.

### Claim 14 (depends on 1)

The method of claim 1, wherein the superconductor material of the second layer comprises aluminum.

### Claim 15

A device comprising:
a substrate;
a first layer of superconductor material on the substrate, the first layer of superconductor material having first and second opposing surfaces, wherein the second surface faces away from the substrate;
a capping layer in contact with the second surface of the first layer of superconductor material, wherein a region of the second surface of the first layer of superconductor material in contact with the capping layer is free of a native oxide of the superconductor material,
wherein the capping layer comprises a material that is associated with an ion milling etch rate that, at a set of predetermined ion beam parameters, is higher than an ion milling etch rate associated with the native oxide of the superconductor material of the first layer at the same set of predetermined ion beam parameters,
wherein a thickness of the capping layer is between about 5 nm and about 10 nm; and
a second layer of superconductor material in contact with the capping layer.

### Claim 16 (depends on 15)

The device of claim 15 wherein the first layer of superconductor material, the capping layer, and the second layer of superconductor material form an electrical contact junction that allows DC current to flow unimpeded.

### Claim 17 (depends on 16)

The device of claim 16, wherein the capping layer material comprises a metal having a thickness such that the metal behaves as a superconductor material due to the superconductivity proximity effect when the electrical contact junction is cooled below a critical temperature of the superconductor material of the first layer.

### Claim 18 (depends on 15)

The device of claim 15, wherein the etch rate associated with the capping layer material is at least five times higher than the etch rate of the native oxide of the superconductor material of the first layer.

### Claim 19 (depends on 15)

The device of claim 15, wherein the ion milling etch rate associated with the capping layer material is at least fifteen times higher than the ion milling etch rate of the native oxide of the superconductor material of the first layer.

### Claim 20 (depends on 15)

The device of claim 15, wherein the ion milling etch rate associated with the capping layer material is at least fifteen times higher than the ion milling etch rate of the native oxide of the superconductor material of the first layer.

### Claim 21 (depends on 15)

The device of claim 15, wherein the capping layer material comprises a metal having a thickness such that the metal behaves as a superconductor material due to the superconductivity proximity effect when the electrical contact junction is cooled below a critical temperature of the superconductor material of the first layer.

### Claim 22 (depends on 15)

The device of claim 15, wherein the capping layer material comprises a superconductor material.

### Claim 23 (depends on 22)

The device of claim 22, wherein the capping layer material comprises titanium nitride, rhenium, or ruthenium.

### Claim 24 (depends on 15)

The device of claim 15, wherein the superconductor material of the first layer is aluminum.

### Claim 25 (depends on 15)

The device of claim 15, wherein the superconductor material of the second layer is aluminum.

### Claim 26 (depends on 15)

The device of claim 15, wherein the device is a qubit.

### Claim 27 (depends on 15)

The device of claim 15, wherein the device is a capacitor.

### Claim 28 (depends on 15)

The device of claim 15, wherein the device is a cross-over bridge.

### Claim 29

A method of fabricating an electrical contact junction that allows a current to flow, the method comprising:
providing a substrate comprising a first layer of superconductor material;
removing a native oxide of the superconductor material of the first layer from a first region of the first layer;
forming a capping layer in contact with the first region of the first layer, wherein the capping layer prevents reformation of the native oxide of the superconductor material in the first region,
wherein the capping layer comprises a material that, when subject to ion milling at a predetermined set of ion beam parameters, has an etch rate that is higher than an etch rate of the native oxide subject to the same predetermined set of ion beam parameters;
forming, after forming the capping layer, a second layer of superconductor material that electrically connects to the first region of the first layer of superconductor material to provide the electrical contact junction that allows current to flow.

### Claim 30 (depends on 29)

The method of claim 29, wherein a thickness of the capping layer is between about 5 nm and about 10 nm.