# US 10,957,663 B2 · Spoked solder pad to improve solderability and self-alignment of integrated circuit packages

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,663 B2
- Document ID: US10957663B2
- Status: Granted
- Kind: B2
- Application number: 16/197,221
- Filed: 2018-11-20
- Published: 2019-03-21
- Granted: 2021-03-23
- Earliest claimed: 2014-12-19
- Applicants: Myron Walker
- Inventors: Myron Walker
- Web page: https://patentgrep.com/patent/US10957663B2

## CPC

- H05K 1/111: {Pads for surface mounting, e.g. lay-out}
- H05K 1/181: associated with surface mounted components
- H05K 3/3436: {having an array of bottom contacts, e.g. pad grid array or ball grid array components}
- H05K 2201/09381: Shape of non-curved single flat metallic pad, land or exposed part thereof; Shape of electrode of leadless component
- H05K 2203/048: Self-alignment during soldering; Terminals, pads or shape of solder adapted therefor
- H10W 72/931: {Shapes of bond pads}
- H10W 72/932: {Plan-view shape, i.e. in top view}
- H10W 72/934: {Cross-sectional shape, i.e. in side view}
- H10W 72/942: {relative to underlying supporting features, e.g. bond pads, RDLs or vias}
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A center pad or paddle that is shaped with three or more curved spires which are symmetrical in form about axis that radiate from the center of the integrated circuit package, which takes advantage of the surface tension of solder to produce increased rotational align forces and increased centering forces during package soldering when aligned to a matching shaped pad on the surface of a circuit board.

## Claims

### Claim 1

A component alignment system that acts as a center pivot to align a component on a substrate or to reveal if the component is misaligned on the substrate, the component alignment system comprising:
a first spoked solder pad on a mating surface of the component, the first spoked solder pad comprising:
a component pad central area that defines a rotational center for the component alignment system, and
at least three component pad spokes extending from the component pad central area;
a second spoked solder pad on a mating surface of the substrate for receiving the component, the second spoked solder pad comprising:
a substrate pad central area that corresponds to the component pad central area, and
at least three substrate pad spokes extending from the substrate pad central area that correspond to component pad spokes;
wherein the component alignment system has a shape and an area relative to the mating surface of the component configured so that, when solder is flowed between the first spoked solder pad and the second spoked solder pad:
the solder applies a centering alignment force sufficient to move the component to align the component pad central area and the substrate pad central area;
the rotational center for the component alignment system acts as a center of rotation for the component on the substrate, and
the solder applies a rotational alignment force on the component pad spokes and the substrate pad spokes sufficient to rotate the component; and
wherein the component alignment system is configured to rotate the component to a position on the substrate that is either properly aligned or clearly misaligned, wherein the component alignment system is configured to rotate the component to a final alignment position on the substrate that is properly aligned if the component is placed on the substrate in a correct orientation, and is configured to rotate the component to a final alignment position on the substrate that is clearly misaligned if the component is placed on the substrate in an incorrect orientation.

### Claim 2 (depends on 1)

The component alignment system of claim 1, wherein the first spoked solder pad on the mating surface of the component is centrally positioned on a bottom surface of the component, and the second spoked solder pad on the mating surface of the substrate is centrally positioned in an installation location for the component on the substrate.

### Claim 3 (depends on 1)

The component alignment system of claim 1, wherein the mating surface of the component within a smallest circle encompassing the first spoked solder pad and the mating surface of the substrate within a smallest circle encompassing the second spoked solder pad are free of solder pads besides the spoked solder pads of the component alignment system.

### Claim 4 (depends on 1)

The component alignment system of claim 1, wherein a diameter of the first spoked solder pad is at least approximately 40% of a narrowest width of the mating surface of the component.

### Claim 5 (depends on 1)

The component alignment system of claim 1, wherein an area of the first spoked solder pad is at least approximately 10% of an area of the mating surface of the component.

### Claim 6 (depends on 1)

The component alignment system of claim 1, wherein an area of a smallest circle encompassing the first spoked solder pad is at least approximately 25% of an area of the mating surface of the component.

### Claim 7 (depends on 1)

The component alignment system of claim 1, wherein the component pad spokes and the substrate pad spokes do not extend to or past an edge of the mating surface of the component.

### Claim 8 (depends on 1)

The component alignment system of claim 1, wherein a diameter of the first spoked solder pad is no greater than approximately 90% of a narrowest width of the mating surface of the component, such that the component pad spokes do not extend to within 5% of the narrowest width from the edge of the component.

### Claim 9 (depends on 1)

The component alignment system of claim 1, wherein the component pad spokes and the substrate pad spokes are radially symmetrical or are aligned on radial axes.

### Claim 10 (depends on 1)

The component alignment system of claim 1, wherein the component pad spokes and the substrate pad spokes are equidistantly spaced.

### Claim 11 (depends on 1)

The component alignment system of claim 1, wherein the first spoked solder pad and the second spoked solder pad are shaped to direct molten solder surface tension and intermolecular forces to move the component in a direction substantially perpendicular to a radial axis extending from the rotational center for the component alignment system.

### Claim 12 (depends on 1)

The component alignment system of claim 1, wherein the number of component pad spokes or the number of substrate pad spokes is odd.

### Claim 13 (depends on 1)

The component alignment system of claim 1, wherein the component is an integrated circuit package and the substrate is a circuit board.

### Claim 14 (depends on 13)

The component alignment system of claim 13, wherein the integrated circuit package is substantially rectangular, having four side edges, and the number of component pad spokes or the number of substrate pad spokes is three, five, seven, or nine.

### Claim 15 (depends on 1)

The component alignment system of claim 1, wherein the number of component pad spokes and the number of substrate pad spokes are not equal, and the higher number is a multiple of the lower number.

### Claim 16 (depends on 1)

The component alignment system of claim 1, wherein the substrate pad central area or the component pad central area comprises a solder prefill region, and the component alignment system is configured for solder to flow between the substrate pad spokes and the component pad spokes.

### Claim 17 (depends on 16)

The component alignment system of Claim 16, further comprising a solder prefill on the solder prefill region.

### Claim 18

A method of mounting a component on a substrate using spoked solder pads that act as a center pivot to align the component on the substrate or to reveal if the component is misaligned on the substrate, the method comprising:
causing a first spoked solder pad to be placed on a mating surface of the component, the first spoked solder pad comprising:
a component pad central area that defines a rotational center for the component alignment system, and
at least three component pad spokes extending from the component pad central area;
causing a second spoked solder pad to be placed on a mating surface of the substrate for receiving the component, the second spoked solder pad comprising:
a substrate pad central area that corresponds to the component pad central area, and
at least three substrate pad spokes extending from the substrate pad central area that correspond to component pad spokes;
wherein the spoked solder pads have a shape and an area relative to the mating surface of the component configured so that, when solder is flowed between the first spoked solder pad and the second spoked solder pad:
the solder applies a centering alignment force sufficient to move the component to align the component pad central area and the substrate pad central area;
the rotational center for the component alignment system acts as a center of rotation for the component on the substrate, and
the solder applies a rotational alignment force on the component pad spokes and the substrate pad spokes sufficient to rotate the component; and
wherein the component alignment system is configured to rotate the component to a position on the substrate that is either properly aligned or clearly misaligned, wherein the component alignment system is configured to rotate the component to a final alignment position on the substrate that is properly aligned if the component is placed on the substrate in a correct orientation, and is configured to rotate the component to a final alignment position on the substrate that is clearly misaligned if the component is placed on the substrate in an incorrect orientation.

### Claim 19 (depends on 18)

The method of claim 18, further comprising mating the component and the substrate and causing solder to be flowed between the first spoked solder pad and the second spoked solder pad.

### Claim 20 (depends on 19)

The method of claim 19, wherein causing solder to be flowed comprises causing solder between the substrate pad central area and the component pad central area to flow between the substrate pad spokes and the component pad spokes.