# US 10,957,640 B2 · Method for manufacturing a semiconductor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,640 B2
- Document ID: US10957640B2
- Status: Granted
- Kind: B2
- Application number: 16/458,543
- Filed: 2019-07-01
- Published: 2020-01-02
- Granted: 2021-03-23
- Earliest claimed: 2015-11-17
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Limited
- Inventors: Yu-Hung Lin; Chun-Hsien Huang; I-Tseng Chen
- Web page: https://patentgrep.com/patent/US10957640B2

## CPC

- H10W 20/42: Vias, e.g. via plugs
- H10D 84/0149: {Manufacturing their interconnections or electrodes, e.g. source or drain electrodes}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/83: of only insulated-gate FETs [IGFET]
- H10P 50/73: {using masks for insulating materials}
- H10P 76/204: {of organic photoresist masks}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/082: {the openings being tapered via holes}
- H10W 20/43: Layouts of interconnections
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10W 20/40: Interconnections external to wafers or substrates, e.g. back-end-of-line [BEOL] metallisations or vias connecting to gate electrodes
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor structure includes a conductive structure, a dielectric layer, and a plurality of conductive features. The dielectric layer is present on the conductive structure. The dielectric layer has a plurality of through holes therein, and at least one of the through holes exposes the conductive structure. The conductive features are respectively present in the through holes. At least one of the conductive features has a bottom surface and at least one sidewall. The bottom surface and the sidewall of the conductive feature intersect to form an interior angle. The interior angles of adjacent two of the conductive features have a difference less than or substantially equal to about 3 degrees.

## Claims

### Claim 1

A method for manufacturing a semiconductor structure, comprising:
forming a conductive structure comprising a first portion and a second portion;
forming a dielectric layer over the conductive structure, wherein the first portion of the conductive structure is separated from the second portion of the conductive structure by the dielectric layer, wherein:
after forming the conductive structure and before forming the dielectric layer, a hole is defined between the first portion of the conductive structure and the second portion of the conductive structure, and
the hole overlies an electric element;
forming a metal hard mask over and in contact with the dielectric layer;
etching the metal hard mask to form a patterned metal hard mask; and
patterning the dielectric layer with the patterned metal hard mask to form a first through hole exposing the first portion of the conductive structure and a second through hole exposing the second portion of the conductive structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first portion of the conductive structure and the second portion of the conductive structure overlie the electric element.

### Claim 3 (depends on 1)

The method of claim 1, wherein:
the electric element is spaced apart from the first portion of the conductive structure by a layer, and
forming the dielectric layer comprises forming the dielectric layer to directly contact the layer.

### Claim 4 (depends on 1)

The method of claim 1, comprising, before etching the metal hard mask:
forming a bottom layer over the metal hard mask;
forming a middle layer over the bottom layer; and
forming a photoresist layer over the middle layer, wherein etching the metal hard mask comprises etching the metal hard mask using the photoresist layer, the middle layer, and the bottom layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein no degas process is performed between forming the dielectric layer and forming the metal hard mask.

### Claim 6 (depends on 1)

The method of claim 1, comprising, after forming the dielectric layer, transferring a wafer comprising the conductive structure and the dielectric layer directly from a load lock to a process chamber without entering a degas chamber.

### Claim 7 (depends on 1)

The method of claim 1, wherein forming the metal hard mask comprises beginning to form the metal hard mask when a temperature of the dielectric layer is no greater than 30° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein patterning the dielectric layer comprises:
patterning the dielectric layer to define a first angle between the first portion of the conductive structure and a first sidewall of the dielectric layer defining the first through hole; and
patterning the dielectric layer to define a second angle between the second portion of the conductive structure and a second sidewall of the dielectric layer defining the second through hole, wherein a difference between the first angle and the second angle is less than or equal to 3 degrees.

### Claim 9 (depends on 8)

The method of claim 8, wherein:
the first angle is between 92 degrees and 98 degrees, and
the second angle is between 92 degrees and 98 degrees.

### Claim 10 (depends on 1)

The method of claim 1, wherein patterning the dielectric layer comprises:
patterning the dielectric layer to define a first angle between the first portion of the conductive structure and a first sidewall of the dielectric layer defining the first through hole; and
patterning the dielectric layer to define a second angle between the second portion of the conductive structure and a second sidewall of the dielectric layer defining the second through hole, wherein:
the first angle is between 92 degrees and 98 degrees, and
the second angle is between 92 degrees and 98 degrees.

### Claim 11 (depends on 1)

The method of claim 1, wherein forming the metal hard mask comprises beginning to form the metal hard mask when a temperature of the dielectric layer is between 15° C. and 30° C.

### Claim 12

A method for manufacturing a semiconductor structure, comprising:
forming a conductive structure comprising a first portion and a second portion spaced apart from the first portion;
forming a first dielectric layer overlying the first portion of the conductive structure and the second portion of the conductive structure;
forming a second dielectric layer over the first dielectric layer;
forming a metal hard mask over the second dielectric layer;
etching the metal hard mask to form a patterned metal hard mask;
patterning the first dielectric layer with the patterned metal hard mask to form a first through hole exposing the first portion of the conductive structure and a second through hole exposing the second portion of the conductive structure; and
patterning the second dielectric layer with the patterned metal hard mask to form a third through hole exposing a third portion of the conductive structure between the first portion of the conductive structure and the second portion of the conductive structure, wherein:
patterning the first dielectric layer comprises:
patterning the first dielectric layer to define a first angle between the first portion of the conductive structure and a first sidewall of the first dielectric layer defining the first through hole; and
patterning the first dielectric layer to define a second angle between the second portion of the conductive structure and a second sidewall of the first dielectric layer defining the second through hole,
patterning the second dielectric layer comprises patterning the second dielectric layer to define a third angle between the third portion of the conductive structure and a first sidewall of the second dielectric layer defining the third through hole,
a difference between the first angle and the second angle is less than or equal to 3 degrees,
a difference between the first angle and the third angle is less than or equal to 3 degrees, and
a difference between the second angle and the third angle is less than or equal to 3 degrees.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first portion of the conductive structure comprises a first source/drain feature and the second portion of the conductive structure comprises a second source/drain feature.

### Claim 14 (depends on 12)

The method of claim 12, comprising:
patterning the second dielectric layer with the patterned metal hard mask to form the first through hole exposing the first portion of the conductive structure and the second through hole exposing the second portion of the conductive structure.

### Claim 15 (depends on 12)

The method of claim 12, wherein a depth of the third through hole is different than a depth of the first through hole and a depth of the second through hole.

### Claim 16

A method for manufacturing a semiconductor structure, comprising:
forming a conductive structure;
forming a first dielectric layer over the conductive structure;
forming a metal hard mask over the first dielectric layer, wherein forming the metal hard mask comprises beginning to form the metal hard mask when a temperature of the first dielectric layer is between 15° C. and 30° C.;
etching the metal hard mask to form a patterned metal hard mask; and
patterning the first dielectric layer with the patterned metal hard mask to form a first through hole exposing a first portion of the conductive structure and a second through hole exposing a second portion of the conductive structure.

### Claim 17 (depends on 16)

The method of claim 16, comprising:
forming a second dielectric layer over the first dielectric layer before forming the metal hard mask; and
patterning the second dielectric layer with the patterned metal hard mask to form a third through hole concurrently within forming the first through hole and the second through hole, wherein a depth of the third through hole is different than a depth of the first through hole and different than a depth of the second through hole.

### Claim 18 (depends on 17)

The method of claim 17, wherein:
a difference between a first angle defined by a surface defining a side of the first through hole and a surface defining a bottom of the first through hole and a second angle defined by a surface defining a side of the third through hole and a surface defining a bottom of the third through hole is less than 3 degrees.

### Claim 19 (depends on 1)

The method of claim 1, wherein the dielectric layer has a homogenous composition.

### Claim 20 (depends on 12)

The method of claim 12, wherein forming the metal hard mask comprises beginning to form the metal hard mask when a temperature of the second dielectric layer is between 15° C. and 30° C.