# US 10,957,587 B2 · Structure and formation method of semiconductor device with conductive feature

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,587 B2
- Document ID: US10957587B2
- Status: Granted
- Kind: B2
- Application number: 16/450,665
- Filed: 2019-06-24
- Published: 2020-02-06
- Granted: 2021-03-23
- Earliest claimed: 2018-07-31
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Li-Chieh Wu; Kuo-Hsiu Wei; Kei-Wei Chen; Tang-Kuei Chang; Chia Hsuan Lee; Jian-Ci Lin
- Web page: https://patentgrep.com/patent/US10957587B2

## CPC

- H10W 20/0698: {Local interconnections}
- C09G 1/04: Aqueous dispersions (C09G1/02 takes precedence)
- H10P 52/403: {of conductive or resistive materials}
- H10W 20/033: {in openings in dielectrics}
- H10W 20/057: {by selectively depositing, e.g. by using selective CVD or plating}
- H10W 20/062: {by smoothing of conductive parts, e.g. by planarisation}
- H10W 20/065: {by making at least a portion of the conductive part non-conductive, e.g. by oxidation}
- H10W 20/076: {in via holes or trenches}
- H10W 20/083: {the openings being via holes penetrating underlying conductors}
- H10W 20/094: {by transforming insulators into conductors}
- H10W 20/20: Interconnections within wafers or substrates, e.g. through-silicon vias [TSV]
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A structure and a formation method of a semiconductor device are provided. The method includes forming a conductive feature over a semiconductor substrate and forming a dielectric layer over the conductive feature. The method also includes forming an opening in the dielectric layer to expose the conductive feature. The method further includes forming a conductive material to overfill the opening. In addition, the method includes thinning the conductive material using a chemical mechanical polishing process. A slurry used in the chemical mechanical polishing process includes an iron-containing oxidizer that oxidizes a portion of the conductive material.

## Claims

### Claim 1

A method for forming a semiconductor device structure, comprising:
forming a conductive feature over a semiconductor substrate;
forming a dielectric layer over the conductive feature;
forming an opening in the dielectric layer to expose the conductive feature;
forming a conductive material to overfill the opening; and
thinning the conductive material using a chemical mechanical polishing process, wherein a slurry used in the chemical mechanical polishing process comprises an iron-containing oxidizer that oxidizes a portion of the conductive material to form an oxidized portion located between the dielectric layer and a non-oxidized portion of the conductive material, wherein the oxidized portion has a height less than a height of the conductive material.

### Claim 2 (depends on 1)

The method for forming a semiconductor device structure as claimed in claim 1, wherein a weight percentage of the iron-containing oxidizer in the slurry is in a range from about 0.1% to about 2%.

### Claim 3 (depends on 1)

The method for forming a semiconductor device structure as claimed in claim 1, wherein the iron-containing oxidizer comprises ferric nitrate.

### Claim 4 (depends on 1)

The method for forming a semiconductor device structure as claimed in claim 1, wherein the slurry has a pH value in a range from about 2 to about 4.

### Claim 5 (depends on 1)

The method for forming a semiconductor device structure as claimed in claim 1, wherein the slurry comprises an inhibitor, and the inhibitor comprises a carbon chain having a carbon number in a range from 10 to 1000.

### Claim 6 (depends on 5)

The method for forming a semiconductor device structure as claimed in claim 5, wherein a weight percentage of the inhibitor in the slurry is in a range from about 0.01% to about 1%.

### Claim 7 (depends on 1)

The method for forming a semiconductor device structure as claimed in claim 1, wherein the slurry is kept at a temperature in a range from about 20 degrees C. to about 50 degrees C. during the chemical mechanical polishing process.

### Claim 8 (depends on 1)

The method for forming a semiconductor device structure as claimed in claim 1, wherein there is no barrier layer formed over sidewalls of the opening before the conductive material is formed.

### Claim 9 (depends on 1)

The method for forming a semiconductor device structure as claimed in claim 1, further comprising:
forming a second opening in the dielectric layer before the conductive material is formed;
forming a barrier layer over the conductive material, wherein the barrier layer extends over a bottom and sidewalls of the second opening;
forming a second conductive material over the barrier layer, wherein the second conductive material overfills the second opening; and
planarizing the second conductive material, the barrier layer, and the conductive material to expose the dielectric layer.

### Claim 10 (depends on 9)

The method for forming a semiconductor device structure as claimed in claim 9, wherein the conductive material is selectively formed on the conductive feature without being formed in the second opening.

### Claim 11

A method for forming a semiconductor device structure, comprising:
forming a conductive feature over a semiconductor substrate;
forming a dielectric layer over the conductive feature;
forming an opening in the dielectric layer to expose the conductive feature;
forming a tungsten-containing material directly on the conductive feature to overfill the opening;
partially removing the tungsten-containing material and the dielectric layer using a chemical mechanical polishing process, wherein an iron-containing oxidizer transforms a portion of the tungsten-containing material into an oxide material during the chemical mechanical polishing process;
forming a second opening in the dielectric layer before the tungsten-containing material is formed;
forming a barrier layer over the tungsten-containing material, wherein the barrier layer extends over a bottom and sidewalls of the second opening;
forming a second tungsten-containing material over the barrier layer, wherein the second tungsten-containing material overfills the second opening; and
planarizing the second tungsten-containing material, the barrier layer, and the tungsten-containing material to expose the dielectric layer.

### Claim 12 (depends on 11)

The method for forming a semiconductor device structure as claimed in claim 11, wherein the iron-containing oxidizer comprises ferric nitrate, and a weight percentage of the iron-containing oxidizer in the slurry is in a range from about 0.1% to about 2%.

### Claim 13 (depends on 11)

The method for forming a semiconductor device structure as claimed in claim 11, wherein the slurry comprises an inhibitor, the inhibitor comprises a carbon chain having a carbon number in a range from 10 to 1000, and a weight percentage of the inhibitor in the slurry is in a range from about 0.01% to about 1%.

### Claim 14 (depends on 11)

The method for forming a semiconductor device structure as claimed in claim 11, wherein the tungsten-containing material is selectively formed on the conductive feature without being formed in the second opening.

### Claim 15 (depends on 11)

The method as claimed in claim 11, wherein the oxide material is located between the dielectric layer and a non-oxidized portion of the tungsten-containing material, and wherein the oxide material has a height less than a height of the tungsten-containing material.

### Claim 16

A method of manufacturing a semiconductor device, the method comprising:
forming a first conductive feature over a semiconductor substrate;
forming a dielectric layer over the first conductive feature;
forming a second conductive feature surrounded by the dielectric layer and electrically connected to the first conductive feature, wherein the second conductive feature is made of a metal material; and
forming a protective element between a portion of the second conductive feature and a portion of the dielectric layer, wherein the protective element is an oxide material of the metal material, wherein the protective element has a height that is less than a height of the second conductive feature.

### Claim 17 (depends on 16)

The method as claimed in claim 16, wherein the metal material comprises tungsten, and the oxide material of the metal material comprises tungsten oxide.

### Claim 18 (depends on 16)

The method as claimed in claim 16, wherein the forming the protective element comprises forming a mixture of WO3 and WO2.

### Claim 19 (depends on 16)

The method as claimed in claim 16, wherein a hole is surrounded by the protective element, the second conductive feature, and the dielectric layer.

### Claim 20 (depends on 16)

The method as claimed in claim 16, wherein the first conductive feature and the second conductive feature are made of different materials.