# US 10,957,553 B2 · Etching solution, etching method, and method for manufacturing an electronic component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,553 B2
- Document ID: US10957553B2
- Status: Granted
- Kind: B2
- Application number: 16/294,508
- Filed: 2019-03-06
- Published: 2019-06-27
- Granted: 2021-03-23
- Earliest claimed: 2017-03-15
- Assignees: Kabushiki Kaisha Toshiba
- Applicants: Kabushiki Kaisha Toshiba
- Inventors: Yukako Murakami; Masaaki Hirakawa; Ikuo Uematsu
- Web page: https://patentgrep.com/patent/US10957553B2

## CPC

- H10P 50/283: {by chemical means}
- C09K 13/08: containing a fluorine compound
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 50/642: {Chemical etching}
- H10P 72/0422: {for wet etching}
- H10P 72/0426: {with the semiconductor substrates being dipped in baths or vessels}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

According to one embodiment, an etching solution used for etching of silicon nitride is provided. The etching solution includes phosphoric acid, an acid, silicic acid compound, and water. The phosphoric acid has a first acid dissociation exponent pKa1. The acid has an acid dissociation exponent smaller than the first acid dissociation exponent pKa1. A mass ratio M1/M2 of mass M1 of the phosphoric acid to mass M2 of the acid having the acid dissociation exponent smaller than the first acid dissociation exponent pKa1 is within a range of 0.82 or more and 725 or less.

## Claims

### Claim 1

An etching solution suitable for etching silicon nitride, the solution comprising:
phosphoric acid having a first acid dissociation exponent pKa1;
a second acid having an acid dissociation exponent smaller than the first acid dissociation exponent pKa1;
a silicic acid compound;
and water,
wherein the silicic acid compound comprises a monomer or multimer of formula (I)
n being an integer in a range of from 1 to 5,
wherein a mass ratio M1/M2 of mass M1 of the phosphoric acid to mass M2 of the second acid is in a range of from 0.82 to 725, and
wherein the second acid is at least one selected from the group consisting of sulfuric acid, hydrochloric acid, and trifluorosulfonic acid.

### Claim 2 (depends on 1)

The solution of claim 1, having a silicon concentration in a range of from 5 to 98 ppm.

### Claim 3 (depends on 1)

The solution of claim 1, wherein the silicon concentration of the etching solution is Y1 ppm or more when a concentration of the second acid is in a range of from 0.11 to 2.9 mass %,
wherein the silicon concentration of the etching solution is Y2 ppm or more when the concentration of the second acid is in a range of from more than 2.9 to 28.33 mass %, and
wherein the silicon concentration of the etching solution is 5 ppm or more when the concentration of the second acid is within a range of from more than 28.33 to 48.3 mass %, and
wherein Y1 is of formula (1), Y2 is of formula (2), and x is a reciprocal of a value of the concentration of the second acid:
Y1=21.876×e0.712x (1), and
Y2=6.6356×loge(X)+29.083 (2).

### Claim 4 (depends on 1)

The solution of claim 1, wherein the silicon concentration is within a range of 5 ppm or more and Y3 ppm or less when the concentration of the second acid is in a range of from 0.11 to 0.58 mass %, and
wherein the silicon concentration is in a range of from 5 ppm to Y4 ppm when the concentration of the second acid is in a range of from more than 0.58 to 28.33 mass %, and
wherein Y3 is of formula (3), Y4 is of formula (4), and X is a reciprocal of a value of the concentration of the second acid:
Y3=18.958×loge(X)+53.583 (3), and
Y4=18.111×loge(X)+65.953 (4).

### Claim 5 (depends on 4)

The solution of claim 4, wherein the silicon concentration is within a range of from the Y1 ppm to the Y3 ppm when the concentration of the second acid is in a range of from 0.11 to 0.58 mass %,
wherein the silicon concentration is within a range of from the Y1 to the Y4 ppm when the concentration of the second acid is in a range of from more than 0.58 to 2.9 mass %, and
wherein the silicon concentration is within a range of from the Y2 ppm to the Y4 ppm when the concentration of the second acid is in a range of from more than 2.9 to 28.33 mass %,
wherein Y1 of formula (1), the Y2 is of formula (2), and x is a reciprocal of a value of the concentration of the second acid:
Y1=21.876×e0.1712x (1), and
Y2=6.6356×loge(X)+29.083 (2).

### Claim 6 (depends on 1)

The solution of claim 1, wherein a water concentration of the etching solution is 12 mass % or less.

### Claim 7 (depends on 1)

The solution of claim 1, wherein a concentration of the phosphoric acid is in a range of from 60 to 85 mass %,
wherein a concentration of the second acid is in a range of from 0.1 to 28.33 mass %, and
wherein a concentration of the water is in a range of from 4 to 17 mass %.

### Claim 8 (depends on 1)

The solution of claim 1, wherein the second acid comprises the sulfuric acid.

### Claim 9 (depends on 1)

The solution of claim 1, wherein the second acid comprises the hydrochloric acid.

### Claim 10 (depends on 1)

An etching method, comprising:
etching of silicon nitride using the solution of claim 1.

### Claim 11 (depends on 1)

A method for manufacturing an electronic component, the method comprising:
etching of silicon nitride using the solution of claim 1.

### Claim 12 (depends on 11)

A method for manufacturing an electronic component, the method comprising:
etching a silicon nitride layer from a substrate by the method of claim 11, the substrate comprising the silicon nitride layer and a silicon oxide layer; and
depositing a conductive material on at least a portion of an area from which the silicon nitride layer has been removed.

### Claim 13

An etching solution suitable for etching silicon nitride, the solution comprising:
phosphoric acid having a first acid dissociation exponent pKa1;
a second acid having an acid dissociation exponent smaller than the first acid dissociation exponent pKa1;
a silicic acid compound;
a salt comprising a monovalent cation having a hydration number of 3.5 or less; and
water,
wherein a mass ratio M1/M2 of mass M1 of the phosphoric acid to mass M2 of the second acid is in a range of from 0.82 to 725,
wherein the second acid is at least one selected from the group consisting of sulfuric acid, hydrochloric acid, and trifluorosulfonic acid, and
wherein a concentration of the salt is in a range of from 0.05 to 2 mol/L.

### Claim 14

An etching solution suitable for etching silicon nitride, the etching solution comprising:
phosphoric acid having a first acid dissociation exponent pKa1;
a second acid having an acid dissociation exponent smaller than the first acid dissociation exponent pKa;
a silicic acid compound;
and water,
wherein a concentration of the phosphoric acid is in a range of from 88 to 95 mass %,
wherein a concentration of the second acid is in a range of from 1 to 5 mass %,
wherein a concentration of the water is in a range of from 4 to 11 mass %,
wherein the second acid is at least one selected from the group consisting of sulfuric acid, hydrochloric acid, and trifluorosulfonic acid, and
wherein the silicic acid compound comprises a monomer or multimer of formula (I)
n being an integer in a range of from 1 to 5.

### Claim 15 (depends on 14)

The solution of claim 14, having a silicon concentration in a range of from 40 to 160 ppm.

### Claim 16 (depends on 14)

The solution of claim 14, having a silicon concentration in a range of from 40 to 100 ppm.

### Claim 17 (depends on 14)

The solution of claim 14, wherein the concentration of the second acid is in a range of from 1.0 to 4.0 mass %.

### Claim 18 (depends on 14)

The solution of claim 14, wherein the concentration of the water is in a range of from 6.0 to 9.0 mass %.

### Claim 19 (depends on 14)

An etching method, comprising:
etching of silicon nitride using the solution of claim 14.

### Claim 20 (depends on 14)

A method for manufacturing an electronic component, the method comprising:
etching of silicon nitride using the solution of claim 14.

### Claim 21 (depends on 19)

A method for manufacturing an electronic component, the method comprising:
etching a silicon nitride layer from a substrate by the method of claim 19, the substrate comprising the silicon nitride layer and a silicon oxide layer; and
depositing a conductive material on at least a portion of an area from which the silicon nitride layer has been removed.

### Claim 22

An etching solution suitable for etching silicon nitride, the etching solution comprising:
phosphoric acid having a first acid dissociation exponent pKa1;
a second acid having an acid dissociation exponent smaller than the first acid dissociation exponent pKa1;
hexafluorosilicic acid;
hydrogen fluoride; and
water,
wherein the second acid is at least one selected from the group consisting of sulfuric acid, hydrochloric acid, and trifluorosulfonic acid.

### Claim 23 (depends on 22)

The solution of claim 22, wherein a concentration of the second acid is in a range of from 5 to 30 mass %.

### Claim 24 (depends on 22)

The solution of claim 22, wherein a concentration of the hexafluorosilicic acid is in a range of from 0.1 to 0.2 mass %.

### Claim 25 (depends on 22)

The solution of claim 22, wherein a concentration of the phosphoric acid is in a range of from 63 to 89 mass %.

### Claim 26 (depends on 22)

The solution of claim 22, wherein a concentration of the phosphoric acid is in a range of from 63 to 89 mass %,
wherein a concentration of the second acid is in a range of from 0.7 to 30 mass %,
wherein a concentration of the water is in a range of from 6 to 8 mass %, and
wherein a concentration of the hexafluorosilicic acid is in a range of from 0.1 to 0.71 mass %.

### Claim 27 (depends on 22)

An etching method, comprising:
etching of silicon nitride using the solution of claim 22.

### Claim 28 (depends on 22)

A method for manufacturing an electronic component, the method comprising:
etching of silicon nitride using the solution of claim 22.

### Claim 29 (depends on 27)

A method for manufacturing an electronic component, the method comprising:
etching a silicon nitride layer from a substrate by the method of claim 27, the substrate comprising the silicon nitride layer and a silicon oxide layer; and
depositing a conductive material on at least a portion of an area from which the silicon nitride film has been removed.

### Claim 30

An etching solution suitable for etching silicon nitride, the etching solution comprising:
phosphoric acid having a first acid dissociation exponent pKa1;
a second acid having an acid dissociation exponent smaller than the first acid dissociation exponent pKa2;
a silicic acid compound;
a salt comprising a monovalent cation having a hydration number of 3.5 or less; and
water,
wherein a concentration of the phosphoric acid is in a range of from 88 to 95 mass %,
wherein a concentration of the second acid is in a range of from 1 to 5 mass %,
wherein a concentration of the water is in a range of from 4 to 11 mass %,
wherein a concentration of the salt is in a range of from 0.05 to 2 mol/L, and
wherein the second acid is at least one selected from the group consisting of sulfuric acid, hydrochloric acid, and trifluorosulfonic acid.