# US 10,957,550 B2 · Semiconductor structure and formation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,550 B2
- Document ID: US10957550B2
- Status: Granted
- Kind: B2
- Application number: 16/537,072
- Filed: 2019-08-09
- Published: 2020-09-03
- Granted: 2021-03-23
- Earliest claimed: 2019-02-28
- Assignees: Semiconductor Manufacturing (Beijing) International Corporation; Semconductor Manufacturing (Shanghai) International Corporation
- Applicants: Semiconductor Manufacturing International (Beijing) Corporation; Semiconductor Manufacturing International (Shanghai) Corporation
- Inventors: Haiyang Zhang; Erhu Zheng
- Web page: https://patentgrep.com/patent/US10957550B2

## CPC

- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- H10D 62/117: {Shapes of semiconductor bodies}
- H10P 14/6304: {Formation by oxidation, e.g. oxidation of the substrate}
- H10P 50/242: {of Group IV materials}
- H10P 50/283: {by chemical means}
- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H10P 50/696: {Process specially adapted to improve the resolution of the mask}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/6319: {Formation by plasma treatments, e.g. plasma oxidation of the substrate}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/683: {carbon-based polymeric organic materials, e.g. polyimides, poly cyclobutene or PVC}
- H10P 14/687: {the materials being fluorocarbon compounds, e.g. (CHxFy) n or polytetrafluoroethylene}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 76/20: of masks comprising organic materials
- H10P 76/40: of masks comprising inorganic materials
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor structure and a formation method thereof are provided. The formation method includes: providing a base, the base including a pattern dense region and a pattern isolated region; forming a plurality of separate hard mask layers on the base, where adjacent hard mask layers and the base define an opening, and an opening of the pattern isolated region is wider than an opening of the pattern dense region; forming a trimming layer at least on a side wall of the opening of the pattern isolated region, the trimming layer and the hard mask layer constituting a mask structure layer; and etching, using the mask structure layer as a mask, a portion of the thickness of the base exposed by the opening to form a plurality of target pattern layers protruding from the remaining base. Embodiments and implementations of the present disclosure are advantageous for improving a critical dimension uniformity of a target pattern layer in each region.

## Claims

### Claim 1

A method for forming a semiconductor structure, comprising:
providing a base, the base comprising a pattern dense region and a pattern isolated region;
forming a plurality of separate hard mask layers on the base, wherein adjacent hard mask layers and the base define openings, and wherein an opening of the pattern isolated region is wider than an opening of the pattern dense region;
forming a trimming layer on side walls of the openings of the pattern isolated region and the pattern dense region, the trimming layer and the hard mask layers constituting a mask structure layer, a thickness of the trimming layer on a side wall of the opening of the pattern isolated region is greater than that of the trimming layer on a side wall of the opening of the pattern dense region in a direction perpendicular to the side walls of the openings; and
etching, using the mask structure layer as a mask, a portion of a thickness of the base exposed by the openings to form a plurality of target pattern layers protruding from the remaining base.

### Claim 2 (depends on 1)

The method for forming the semiconductor structure according to claim 1, wherein the method further comprises:
before forming the trimming layer, performing at least one pre-etch pretreatment, and
the step of pre-etch pretreatment comprises:
performing plasma pretreatment,
forming a trimming material layer on a bottom and the side walls of the openings and a top of the hard mask layers, and
removing the trimming material layer on the bottom of the openings and the top of the hard mask layers,
wherein a thickness of a remaining trimming material layer on the side wall of the opening of the pattern isolated region is greater than that of a remaining trimming material layer on the side wall of the opening of the pattern dense region in a direction perpendicular to the side walls of the openings.

### Claim 3 (depends on 1)

The method for forming the semiconductor structure according to claim 1, wherein the step of forming the trimming layer comprises:
oxidizing the hard mask layers exposed by the side walls of the openings of the pattern isolated region and the pattern dense region, and
forming the trimming layer on the side walls of the remaining hard mask layers, where the thickness of the trimming layer of the pattern isolated region is greater than that of the trimming layer of the pattern dense region in a direction perpendicular to the side walls of the openings.

### Claim 4 (depends on 2)

The method for forming the semiconductor structure according to claim 2, wherein the method further comprises:
before etching, using the mask structure layer as a mask, a portion of the thickness of the base exposed by the openings, removing the trimming layer of the pattern dense region.

### Claim 5 (depends on 2)

The method for forming the semiconductor structure according to claim 2, wherein parameters of the plasma pretreatment comprise:
reaction gas comprises SiCl4, CH4, CH3F or CH2F2 gas,
where SiCl4 has a gas flow rate of 5 sccm to 500 sccm, or CH4 has a gas flow rate of 5 sccm to 500 sccm, or CH3F has a gas flow rate of 5 sccm to 500 sccm, or CH2F2 has a gas flow rate of 5 sccm to 500 sccm, and a source power is in a range of 100 W to 1,000 W, and a process pressure is in a range of 5 mtorr to 200 mtorr.

### Claim 6 (depends on 2)

The method for forming the semiconductor structure according to claim 2, wherein the trimming material layer on the bottom of the openings and the top of the hard mask layers are removed by a plasma etching process.

### Claim 7 (depends on 6)

The method for forming the semiconductor structure according to claim 6, wherein parameters of the plasma etching process comprise:
etching gas comprises CH4, CH3F and NF3,
where CH4 has a gas flow rate of 5 sccm to 500 sccm, CH3F has a gas flow rate of 5 sccm to 500 sccm, NF3 has a gas flow rate of 5 sccm to 500 sccm, a source power is in a range of 100 W to 1,000 W, a bias power is in a range of 50 W to 500 W, and a process pressure is in a range of 5 mtorr to 200 mtorr.

### Claim 8 (depends on 3)

The method for forming the semiconductor structure according to claim 3, wherein the oxidation treatment is performed by plasma oxidation treatment of the hard mask layers exposed by the side walls of the openings.

### Claim 9 (depends on 8)

The method for forming the semiconductor structure according to claim 8, wherein parameters of the plasma oxidation treatment comprise:
oxidizing gas comprises one or more of O2, SO2, CO, CO2, and COS,
carrier gas comprises one or both of argon gas and helium gas,
where the oxidizing gas has a gas flow rate of 10 sccm to 500 sccm, the carrier gas has a gas flow rate of 100 sccm to 500 sccm, a source power is in a range of 100 W to 1,000 W, a process time is in a range of 10 S to 600 S, and a process pressure is in a range of 5 mtorr to 5,000 mtorr.

### Claim 10 (depends on 2)

The method for forming the semiconductor structure according to claim 2, wherein in the step of forming the trimming layer, a thickness difference between the trimming layer of the pattern isolated region and the trimming layer of the pattern dense region is in a range of 0.5 nm to 3 nm.

### Claim 11 (depends on 2)

The method for forming the semiconductor structure according to claim 2, wherein the material of the trimming layer is a silicon-containing oxide layer or a carbon-containing polymer.

### Claim 12 (depends on 3)

The method for forming the semiconductor structure according to claim 3, wherein the material of the trimming layer is silicon oxynitride, boron oxynitride, titanium oxynitride or tantalum oxynitride.

### Claim 13 (depends on 1)

The method for forming the semiconductor structure according to claim 1, wherein the portion of the thickness of the base exposed by the openings is etched by an etching process having a square wave pulse type bias voltage.

### Claim 14 (depends on 1)

The method for forming the semiconductor structure according to claim 1, wherein after etching the portion of the thickness of the base exposed by the opening, the remaining base is used as a substrate, and the target pattern layers are fins.