# US 10,957,548 B2 · Method of etching copper indium gallium selenide (CIGS) material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,548 B2
- Document ID: US10957548B2
- Status: Granted
- Kind: B2
- Application number: 16/683,828
- Filed: 2019-11-14
- Published: 2020-05-14
- Granted: 2021-03-23
- Earliest claimed: 2018-11-14
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Mang-Mang Ling; Jong Mun Kim; Chentsau Ying
- Web page: https://patentgrep.com/patent/US10957548B2

## CPC

- H10P 50/242: {of Group IV materials}
- C01B 19/002: {Compounds containing, besides selenium or tellurium, more than one other element, with -O- and -OH not being considered as anions}
- C09K 13/10: containing a boron compound
- H10F 77/126: {comprising only Group I-III-VI chalcopyrite materials, e.g. CuInSe2, CuGaSe2 or CuInGaSe2 [CIGS]}
- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H10P 72/0461: {characterised by the presence of two or more transfer chambers}
- C01P 2006/40: Electric properties
- H10P 72/0421: {for drying etching}
- H10P 72/0454: {surrounding a central transfer chamber}
- Y02E 10/541: CuInSe2 material PV cells
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Methods for dry plasma etching thin layers of material including Cu(In, Ga)Se, e.g., CIGS material on semiconductor substrates are provided. A method of etching a CIGS material layer such as copper indium gallium selenide film, includes: flowing an etching gas including a mixture of gases into a process chamber having a substrate disposed therein, the substrate including a copper indium gallium selenide layer having a patterned film stack disposed thereon, the patterned film stack covering a first portion of the copper indium gallium selenide layer and exposing a second portion of the copper indium gallium selenide layer; and contacting the copper indium gallium selenide layer with the etching gas to remove the second portion and form one or more copper indium gallium selenide edges of the first portion.

## Claims

### Claim 1

A method of etching a copper indium gallium selenide film, comprising:
flowing an etching gas comprising a mixture of gases into a process chamber having a substrate disposed therein, the substrate comprising a copper indium gallium selenide layer having a patterned film stack disposed thereon, the patterned film stack covering a first portion of the copper indium gallium selenide layer and exposing a second portion of the copper indium gallium selenide layer, wherein the patterned film stack comprises a plurality of layers, one of the plurality of layers having a first thickness and another one of the plurality of layers having a second thickness different from the first thickness; and
contacting the copper indium gallium selenide layer with the etching gas to remove the second portion and form one or more copper indium gallium selenide edges of the first portion.

### Claim 2 (depends on 1)

The method of claim 1, wherein the one or more copper indium gallium selenide edges have a profile of greater than 80 degrees.

### Claim 3 (depends on 1)

The method of claim 1, wherein the one or more copper indium gallium selenide edges have a profile of about 90 degrees.

### Claim 4 (depends on 1)

The method of claim 1, wherein the mixture of gases comprises boron trichloride (BCl3), hydrogen bromide (HBr), argon (Ar), chlorine (Cl2), and nitrogen trifluoride (NF3), or combinations thereof for etching copper indium gallium (di)selenide film.

### Claim 5 (depends on 1)

The method of claim 1, wherein a pressure of the process chamber is between about 1 mTorr and 10 mTorr.

### Claim 6 (depends on 1)

The method of claim 1, wherein the process chamber is under conditions where a source power is about 400 W to 800 W and a bias power is between about 400 W to about 500 W.

### Claim 7 (depends on 1)

The method of claim 1, wherein the process chamber comprises a temperature of about 80 to about 110 degrees Celsius.

### Claim 8

A method of etching a copper indium gallium selenide material, comprising:
contacting a copper indium gallium selenide material disposed on a substrate in a process chamber with an etching gas sufficient to etch the copper indium gallium selenide material, wherein the etching gas comprises boron trichloride (BCl3), hydrogen bromide (HBr), argon (Ar), chlorine (Cl2), and nitrogen trifluoride (NF3) for the etching the copper indium gallium selenide material.

### Claim 9 (depends on 8)

The method of claim 8, wherein a pressure of the process chamber is between about 1 mTorr and 10 mTorr.

### Claim 10 (depends on 8)

The method of claim 8, wherein the process chamber is under conditions where a source power is about 400 W to 800 W and a bias power is between about 400 W to about 500 W.

### Claim 11 (depends on 8)

The method of claim 8, wherein the process chamber is at a temperature of about 80 to 110 degrees Celsius.

### Claim 12 (depends on 8)

The method of claim 8, wherein the etching gas comprises boron trichloride (BCL3) flowed into the process chamber at a flow rate of about 50 standard cubic centimeters per minute.

### Claim 13 (depends on 8)

The method of claim 8, wherein the etching gas comprises hydrogen bromide (HBr) flowed into the process chamber at a flow rate of about 50 standard cubic centimeters per minute.

### Claim 14 (depends on 8)

The method of claim 8, wherein the etching gas comprises argon flowed into the process chamber at a flow rate of about 400 standard cubic centimeters per minute.

### Claim 15 (depends on 8)

The method of claim 8, wherein the etching gas comprises chlorine flowed into the process chamber at a flow rate of about 20 standard cubic centimeters per minute.

### Claim 16 (depends on 8)

The method of claim 8, wherein the etching gas comprises nitrogen trifluoride (NF3) flowed into the process chamber at a flow rate of about 20 standard cubic centimeters per minute.

### Claim 17

A method of etching a copper indium gallium selenide film, comprising:
flowing an etching gas comprising a mixture of gases into a process chamber having a substrate disposed therein, the substrate comprising a copper indium gallium selenide layer having a patterned film stack disposed thereon, the patterned film stack covering a first portion of the copper indium gallium selenide layer and exposing a second portion of the copper indium gallium selenide layer, wherein the patterned film stack comprises a plurality of layers, one of the plurality of layers having a first thickness and another one of the plurality of layers having a second thickness different from the first thickness; and
contacting the copper indium gallium selenide layer with the etching gas to remove the second portion and form one or more copper indium gallium selenide edges of the first portion, wherein the one or more copper indium gallium selenide edges have a side profile contacting the substrate on an angle in an amount of 70 degrees to 90 degrees to a substrate plane.

### Claim 18 (depends on 17)

The method of claim 17, wherein the angle is in an amount of 80 degrees to 90 degrees to a substrate plane.

### Claim 19 (depends on 17)

The method of claim 17, wherein the mixture of gases comprises boron trichloride (BCl3), hydrogen bromide (HBr), argon (Ar), chlorine (Cl2), and nitrogen trifluoride (NF3), or combinations thereof for etching copper indium gallium selenide film.

### Claim 20 (depends on 17)

The method of claim 17, wherein the process chamber is at a temperature of about 80 to 110 degrees Celsius.