# US 10,957,533 B2 · Methods for etching a structure for semiconductor applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,533 B2
- Document ID: US10957533B2
- Status: Granted
- Kind: B2
- Application number: 16/656,018
- Filed: 2019-10-17
- Published: 2020-04-30
- Granted: 2021-03-23
- Earliest claimed: 2018-10-30
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Hao Jiang; He Ren; Hao Chen; Mehul B. Naik
- Web page: https://patentgrep.com/patent/US10957533B2

## CPC

- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 72/0462: {characterised by the construction of the processing chambers, e.g. modular processing chambers}
- H10P 14/3241: {being conductive materials}
- H10P 50/266: {by vapour etching only}
- H10P 50/267: {using plasmas}
- H10P 50/269: {pre- or post-treatments, e.g. anti-corrosion processes}
- H10P 50/287: {by chemical means}
- H10P 70/273: {the processing being a delineation of conductive layers, e.g. by RIE}
- H10P 72/0402: {Apparatus for fluid treatment (H10P72/0441, H10P72/0448 take precedence)}
- H10P 72/0432: {mainly by conduction}
- H10P 72/0602: {Temperature monitoring}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10P 95/94: {Hydrogenation or deuterisation, e.g. using atomic hydrogen from a plasma}
- H01J 37/32449: {Gas control, e.g. control of the gas flow}
- H10P 72/0604: {Process monitoring, e.g. flow or thickness monitoring}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Embodiments of the present disclosure provide methods and apparatus for forming and patterning features in a film stack disposed on a substrate. In one embodiment, a method for patterning a conductive layer on a substrate includes supplying a gas mixture comprising a chlorine containing gas at a first flow rate to etch a first conductive layer disposed on the substrate, lowing the chlorine containing gas in the first gas mixture to a second flow rate lower than the first flow rate to continue etching the first conductive layer, and increasing the chlorine containing gas in the first gas mixture to a third flow rate greater than the second flow rate to remove the first conductive layer from the substrate.

## Claims

### Claim 1

A method for patterning a conductive layer on a substrate, comprising:
supplying a gas mixture comprising a chlorine containing gas at a first flow rate to etch a first conductive layer disposed on the substrate;
lowering the chlorine containing gas in the first gas mixture to a second flow rate lower than the first flow rate to continue etching the first conductive layer; and
increasing the chlorine containing gas in the first gas mixture to a third flow rate greater than the second flow rate to remove the first conductive layer from the substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first conductive layer is a Ti or Ta containing layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first gas mixture further comprises an inert gas.

### Claim 4 (depends on 1)

The method of claim 1, wherein the chlorine containing gas is Cl2 or HCl.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first flow rate is the same or similar to the third flow rate.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
performing a hydrogen treatment process prior to etch the first conductive layer.

### Claim 7 (depends on 6)

The method of claim 6, further comprising:
maintaining a substrate temperature at greater than 150 degrees Celsius while performing the hydrogen treatment process.

### Claim 8 (depends on 7)

The method of claim 7, wherein the substrate temperature between about 200 degrees Celsius and about 300 degrees Celsius.

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
performing a post annealing process to the substrate after the first conductive layer is removed from the substrate.

### Claim 10 (depends on 9)

The method of claim 9, wherein the post annealing process further comprises:
maintaining a process pressure between about 5 bar and 100 bar.

### Claim 11 (depends on 10)

The method of claim 10, further comprising:
supplying an annealing gas mixture including a hydrogen containing gas or a nitrogen containing gas while performing the post annealing process.

### Claim 12 (depends on 9)

The method of claim 9, wherein the post annealing process densifies a second conductive layer exposed on the substrate.

### Claim 13 (depends on 12)

The method of claim 12, wherein the second material containing layer is a Ru containing material.

### Claim 14 (depends on 1)

The method of claim 1, wherein the gas mixture supplied at the first flow rate removes an oxide material from the metal containing material.

### Claim 15 (depends on 1)

The method of claim 1, wherein the gas mixture supplied at the second flow rate removes between about 5% and about 95% of the first conductive layer.

### Claim 16

A method for patterning a conductive layer on a substrate, comprising:
performing a hydrogen treatment process on a substrate to remove residuals on the substrate wherein the treatment process is performed at temperatures exceeding 100 degrees Celsius to remove residual material from a first conductive layer;
performing an etching process by supplying an etching gas mixture comprising chlorine containing gas to etch a first conductive layer on the substrate until a second conductive layer is exposed on the substrate; and
performing a post annealing process at a process pressure between about 5 bar and 100 bar.

### Claim 17 (depends on 16)

The method of claim 16, wherein performing the etching process further comprising:
maintaining the chlorine containing gas in the etching gas mixture from a first flow rate to a second flow rate and further to a third flow rate while etching the first conductive layer.

### Claim 18 (depends on 17)

The method of claim 17, wherein the first flow rate is greater than the second flow rate.

### Claim 19 (depends on 16)

The method of claim 16, wherein the first conductive layer is a Ta or Ti containing layer and the second conductive layer is a Ru containing layer.

### Claim 20

A method for patterning a conductive layer on a substrate, comprising:
removing residuals from on a substrate by a hydrogen treatment process, wherein the residuals comprises organic material, wherein the substrate comprises having a first conductive layer disposed on a second conductive layer,
etching the first conductive layer by supplying an etching gas mixture comprising chlorine containing gas until a second conductive layer is exposed on the substrate, wherein the chlorine containing gas in the etching gas mixture is maintained from a first flow rate to a second flow rate and further to a third flow rate while etching the first conductive layer; and
performing a post annealing process at a process pressure between about 5 bar and 100 bar to thermally treat the second conductive layer on the substrate.