# US 10,957,532 B2 · Method and apparatus for deposition of low-k films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,532 B2
- Document ID: US10957532B2
- Status: Granted
- Kind: B2
- Application number: 16/567,044
- Filed: 2019-09-11
- Published: 2020-01-02
- Granted: 2021-03-23
- Earliest claimed: 2017-04-13
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Ning Li; Zhelin Sun; Mihaela Balseanu; Li-Qun Xia; Bhaskar Jyoti Bhuyan; Mark Saly
- Web page: https://patentgrep.com/patent/US10957532B2

## CPC

- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/36: Carbonitrides
- C23C 16/45551: {for relative movement of the substrate and the gas injectors or half-reaction reactor compartments}
- C23C 16/56: After-treatment
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/6687: {the compound comprising silicon and nitrogen}
- H10P 14/6905: {being a silicon carbide or silicon carbonitride and not containing oxygen, e.g. SiC or SiC:H}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Methods and apparatus for forming a conformal SiOC film on a surface are described. A SiCN film is formed on a substrate surface and exposed to a steam annealing process to decrease the nitrogen content, increase the oxygen content and leave the carbon content about the same. The annealed film has one or more of the wet etch rate or dielectric constant of the film.

## Claims

### Claim 1

A processing platform comprising: a central transfer station comprising a plurality of sides and a robot positioned therein; a batch processing chamber connected to a side of the central transfer station; a steam annealing chamber connected to a side of the central transfer station; and a controller coupled to the central transfer station, the batch processing chamber and the steam annealing chamber, the controller having configurations including: a first configuration to move a substrate to the batch processing chamber, a second configuration to provide a plurality of process gases to the batch processing chamber to form a conformal film on the substrate in the batch processing chamber, a third configuration to move a substrate from the batch processing chamber to the steam annealing chamber, a fourth configuration to heat the steam annealing chamber to an annealing temperature, a fifth configuration to provide a flow of water vapor to the steam annealing chamber, and a sixth configuration to remove the substrate from the steam annealing chamber, wherein the conformal film comprises SiCN, having an initial carbon content, an initial nitrogen content and an initial oxygen content.

### Claim 2 (depends on 1)

The processing platform of claim 1, wherein heating the steam annealing chamber to an annealing temperature reduces the initial nitrogen content to an annealed nitrogen content and increases the initial oxygen content to an annealed oxygen content.

### Claim 3 (depends on 2)

The processing platform of claim 2, wherein the annealed nitrogen content is less than or equal to about 1% on an atomic basis.

### Claim 4 (depends on 2)

The processing platform of claim 2, wherein an annealed carbon content after a steam anneal in the steam annealing chamber is within ±10% of the initial carbon content.

### Claim 5 (depends on 4)

The processing platform of claim 4, wherein the annealed carbon content is about 10% on an atomic basis.

### Claim 6 (depends on 1)

The processing platform of claim 1, wherein the conformal film has a thickness in the range of about 10 Å to about 500 Å.

### Claim 7 (depends on 6)

The processing platform of claim 6, wherein the conformal film is annealed and has a substantially uniform composition of carbon, nitrogen and oxygen.

### Claim 8 (depends on 7)

The processing platform of claim 7, wherein the annealed conformal film has a thickness in the range of about 100 Å to about 140 Å.

### Claim 9 (depends on 8)

The processing platform of claim 8, wherein the annealed conformal film has a wet etch rate in dilute HF less than about 20 Å/min for the first minute.

### Claim 10 (depends on 8)

The processing platform of claim 8, wherein the annealed conformal film has a leakage current less than or equal to about 1.5×10−7 Å/cm2.

### Claim 11 (depends on 8)

The processing platform of claim 8, wherein the annealed conformal film has a dielectric constant less than 5.

### Claim 12 (depends on 1)

The processing platform of claim 1, wherein forming the conformal film comprises sequentially exposing the substrate to a silicon precursor and a reactant.

### Claim 13 (depends on 12)

The processing platform of claim 12, wherein the silicon precursor comprises bis(trichlorosilyl)methane and the reactant comprises ammonia.

### Claim 14 (depends on 1)

The processing platform of claim 1, wherein forming the conformal film and steam annealing occur in the same processing chamber.

### Claim 15 (depends on 1)

The processing platform of claim 1, wherein forming the conformal film occurs in an atomic layer deposition chamber and steam annealing occurs in a furnace.

### Claim 16 (depends on 1)

The processing platform of claim 1, wherein the conformal film is annealed in the steam annealing chamber at a temperature in the range of about 300° C. to about 600° C.

### Claim 17 (depends on 16)

The processing platform of claim 16, wherein the conformal film is annealed with a partial pressure of water greater than or equal to about 500 Torr.