# US 10,957,530 B2 · Freezing a sacrificial material in forming a semiconductor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,530 B2
- Document ID: US10957530B2
- Status: Granted
- Kind: B2
- Application number: 15/847,705
- Filed: 2017-12-19
- Published: 2019-06-20
- Granted: 2021-03-23
- Earliest claimed: 2017-12-19
- Assignees: Micron Technology, Inc.
- Applicants: Micron Technology, Inc.
- Inventors: Matthew S. Thorum
- Web page: https://patentgrep.com/patent/US10957530B2

## CPC

- H10P 72/0406: {for cleaning followed by drying, rinsing, stripping, blasting or the like}
- B08B 9/00: Cleaning hollow articles by methods or apparatus specially adapted thereto
- B81C 1/00793: {Avoid contamination, e.g. absorption of impurities or oxidation}
- B81C 1/00825: {Protect against mechanical threats, e.g. against shocks, or residues (B81C1/00261 take precedence)}
- H10P 14/6528: {In-situ cleaning after layer formation, e.g. removing process residues}
- H10P 70/20: {Cleaning during device manufacture}
- H10P 70/23: {during, before or after processing of insulating materials}
- H10P 70/234: {the processing being the formation of vias or contact holes}
- H10P 72/0408: {for drying}
- H10P 72/0602: {Temperature monitoring}
- B08B 1/00: Cleaning by methods involving the use of tools (cleaning hollow articles by methods or apparatus specially adapted thereto B08B9/00)
- B08B 3/08: the liquid having chemical or dissolving effect
- B81C 1/00849: {during manufacture}
- B81C 2201/0109: Sacrificial layers not provided for in B81C2201/0107 - B81C2201/0108
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B08B: CLEANING IN GENERAL; PREVENTION OF FOULING IN GENERAL
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)

## Abstract

The present disclosure includes apparatuses and methods related to freezing a sacrificial material in forming a semiconductor. In an example, a method may include solidifying, via freezing, a sacrificial material in an opening of a structure, wherein the sacrificial material has a freezing point below a boiling point of a solvent used in a wet clean operation and removing the sacrificial material via sublimation by exposing the sacrificial material to a particular temperature range.

## Claims

### Claim 1

A method for forming a semiconductor device, comprising:
displacing a solvent used in a wet clean operation in an opening of a structure with a sacrificial material at a wet cleaning tool, wherein the sacrificial material is applied above room temperature, and wherein the sacrificial material has a freezing point below a boiling point of the solvent;
solidifying, via freezing, the sacrificial material in the opening of the structure at the wet cleaning tool, wherein the sacrificial material includes naphthalene and the freezing point of the sacrificial material is between 30 and 60 degrees Celsius;
exposing the structure with the sacrificial material to oxygen after solidifying the sacrificial material and prior to removing the sacrificial material via sublimation in response to moving the structure from the wet cleaning tool to a deposition tool; and
removing the sacrificial material via sublimation by exposing the sacrificial material to a particular temperature range at the deposition tool.

### Claim 2 (depends on 1)

The method of claim 1, wherein solidifying the sacrificial material obstructs the opening of the structure.

### Claim 3 (depends on 1)

The method of claim 1, wherein solidifying the sacrificial material includes cooling the sacrificial material below its freezing point.

### Claim 4 (depends on 1)

The method of claim 1, wherein the sacrificial material is a camphor and naphthalene mixture.

### Claim 5 (depends on 1)

The method of claim 1, wherein solidifying the sacrificial material prevents pattern collapse while the structure dries.

### Claim 6

A method for forming a semiconductor device, comprising:
forming a plurality of features in a structure at a dry etch tool;
performing a wet clean operation on the structure using a solvent at a wet cleaning tool;
displacing the solvent with a sacrificial material at the wet cleaning tool, wherein the sacrificial material is applied above room temperature, and wherein the sacrificial material has a freezing point below a boiling point of the solvent;
solidifying, via freezing, the sacrificial material in openings of the plurality of features at the wet cleaning tool, wherein the sacrificial material includes camphor and the freezing point of the sacrificial material is between 30 and 60 degrees Celsius;
exposing the structure with the sacrificial material to oxygen after solidifying the sacrificial material and prior to removing the sacrificial material via sublimation in response to moving the structure from the wet cleaning tool to a deposition tool; and
removing the sacrificial material via sublimation by exposing the sacrificial material to a particular temperature range at the deposition tool.

### Claim 7 (depends on 6)

The method of claim 6, wherein the sacrificial material is a eutectic mixture.

### Claim 8

A method for forming a semiconductor device, comprising:
forming a plurality of features in a structure at a dry etch tool;
performing a wet clean operation on the structure using a solvent at a wet cleaning tool;
displacing the solvent with a sacrificial material at the wet cleaning tool, wherein the sacrificial material is applied above room temperature, and wherein the sacrificial material has a freezing point below a boiling point of the solvent;
solidifying, via freezing, the sacrificial material in an opening of the plurality of features at the wet cleaning tool, wherein the sacrificial material is a camphor and naphthalene mixture and the freezing point of the sacrificial material is between 30 and 60 degrees Celsius;
exposing the structure with the sacrificial material to oxygen after solidifying the sacrificial material and prior to removing the sacrificial material via sublimation in response to moving the structure from the wet cleaning tool to a deposition tool; and
removing the sacrificial material via sublimation by exposing the sacrificial material to a particular temperature range at the deposition tool.

### Claim 9 (depends on 8)

The method of claim 8, wherein the freezing point of the sacrificial material is above a temperature at which sublimation occurs.

### Claim 10 (depends on 8)

The method of claim 8, wherein the freezing point of the sacrificial material is below the boiling point of the solvent to prevent the solvent from boiling.

### Claim 11 (depends on 8)

The method of claim 8, wherein vapor bubbles form when the solvent boils.

### Claim 12 (depends on 11)

The method of claim 11, wherein the vapor bubbles cause pattern collapse.

### Claim 13 (depends on 8)

The method of claim 8, wherein the solvent is isopropyl alcohol (IPA).