# US 10,957,481 B2 · Process for manufacturing a thin strip made of soft magnetic alloy and strip obtained

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,481 B2
- Document ID: US10957481B2
- Status: Granted
- Kind: B2
- Application number: 14/365,035
- Filed: 2012-12-17
- Published: 2014-10-09
- Granted: 2021-03-23
- Earliest claimed: 2011-12-16
- Assignees: Aperam
- Applicants: Aperam
- Inventors: Thierry Waeckerle; Remy Batonnet
- Web page: https://patentgrep.com/patent/US10957481B2

## CPC

- H01F 41/02: for manufacturing cores, coils, or magnets (H01F41/14 takes precedence; for dynamo-electric machines H02K15/00)
- A63B 21/4017: {to the upper limbs}
- A63B 23/14: for wrist joints
- C21D 6/007: {containing Co}
- C21D 8/12: during manufacturing of articles with special electromagnetic properties
- C21D 8/1233: {Cold rolling}
- C21D 8/1261: {following hot rolling}
- C22C 19/07: based on cobalt
- C22C 30/00: Alloys containing less than 50% by weight of each constituent
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/10: containing cobalt
- C22C 38/105: {containing Co and Ni}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/16: containing copper
- C22C 38/42: with copper
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/52: with cobalt
- C22F 1/10: of nickel or cobalt or alloys based thereon
- C22F 1/16: of other metals or alloys based thereon
- H01F 1/147: Alloys characterised by their composition {(treatment thereof for enhancing their electromagnetic properties C21D8/12)}
- H01F 1/16: in the form of sheets (H01F1/147 takes precedence)
- A63B 2208/12: specially adapted for children
- Y10T 29/49009: Dynamoelectric machine
- Y10T 29/49826: Assembling or joining
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for manufacturing a strip in a soft magnetic alloy capable of being cut out mechanically, the chemical composition of which comprises by weight: 18%≤Co≤55% 0%≤V+W≤3% 0%≤Cr≤3% 0%≤Si≤3% 0%≤Nb≤0.5% 0%≤B≤0.05% 0%≤C≤0.1% 0%≤Zr+Ta≤0.5% 0%≤Ni≤5% 0%≤Mn≤2% The remainder being iron and impurities resulting from the elaboration, according to which a strip obtained by hot rolling is cold-rolled in order to obtain a cold-rolled strip with a thickness of less than 0.6 mm. After cold rolling, a continuous annealing treatment is carried out by passing into a continuous oven, at a temperature comprised between the order/disorder transition temperature of the alloy and the onset temperature of ferritic/austenitic transformation of the alloy, followed by rapid cooling down to a temperature below 200° C. Strip obtained.

## Claims

### Claim 1

A method for manufacturing a strip in a soft magnetic alloy capable of being mechanically cut out, the chemical composition of which comprises by weight:
18%≤Co≤55%
0%≤V+W≤3%
0%≤Cr≤3%
0%≤Si≤3%
0%≤Nb≤0.5%
0%≤B≤0.05%
0%≤C≤0.1%
0%≤Zr+Ta≤0.5%
0%≤Ni≤5%
0%≤Mn≤2%
the remainder consisting of iron and impurities resulting from elaboration,
wherein the method comprises:
cold-rolling a strip obtained by hot rolling of a semi-finished product consisting of the alloy is cold-rolled in order to obtain a cold rolled strip with a thickness of less than 0.6 mm, and
after the cold rolling, carrying out a continuous annealing treatment on the strip by having it pass into a continuous oven, at a temperature comprised between the order/disorder transition temperature of the alloy and the ferritic/austenitic transformation point of the alloy, followed by rapid cooling down to a temperature below 200° C., with a cooling rate between the order/disorder temperature and 200° C. greater than 1,000° C. per hour, so as to achieve a recrystallized structure with an average grain size of more than 110 μm2.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the annealing temperature is between 700° C. and 930° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the annealing temperature is between 720° C. and 900° C.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the passing speed of the strip is adapted so that the dwelling time in the continuous oven of the strip at the annealing temperature is less than 10 mins.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the passing speed of the strip in the continuous oven and the annealing temperature are adapted for adjusting the mechanical strength of the strip.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the chemical composition of the alloy is such that:
47%≤Co≤49.5%
0.5%≤V≤2.5%
0%≤Ta≤0.5%
0%≤Nb≤0.5%
0%≤Cr<0.1%
0%≤Si<0.1%
0%≤Ni<0.1%
0%≤Mn<0.1%.