# US 10,957,372 B2 · Switching skyrmions with VCMA/electric field for memory, computing and information processing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,957,372 B2
- Document ID: US10957372B2
- Status: Granted
- Kind: B2
- Application number: 16/782,209
- Filed: 2020-02-05
- Published: 2020-07-02
- Granted: 2021-03-23
- Earliest claimed: 2016-03-01
- Assignees: Virginia Commonwealth University
- Applicants: Virginia Commonwealth University
- Inventors: Jayasimha Atulasimha; Dhritiman Bhattcaharya; Md Mamun Al-Rashid
- Web page: https://patentgrep.com/patent/US10957372B2

## CPC

- G11C 11/1675: {Writing or programming circuits or methods}
- G11C 11/161: {details concerning the memory cell structure, e.g. the layers of the ferromagnetic memory cell}
- G11C 11/1659: {Cell access}
- G11C 11/1673: {Reading or sensing circuits or methods}
- G11C 11/5607: {using magnetic storage elements}
- G11C: STATIC STORES (semiconductor memory devices H10B)

## Abstract

A fixed magnetic skyrmion in a memory or Boolean logic or non-Boolean computing element is reversibly switched or switchable (1) with only an electric field and without a magnetic field or spin current; and (2) using voltage control of magnetic anisotropy (VCMA) to reduce the spin current needed to switch the skyrmion. Some embodiments switch between four states: two skyrmion states and two ferromagnetic states. Other embodiments switch between two states which are both skyrmionic, in which case the switching process may use ferromagnetic intermediate states, or both ferromagnetic, in which case the switching process may use skyrmionic intermediate states, or between a Skyrmion and ferromagnetic state. Boolean and non-Boolean logic devices are also provided which are based on these switching methods.

## Claims

### Claim 1

A method of switching between states of a non-volatile magnetic element that has four stable states, comprising one or more of:
switching the element from a first skyrmion state to a first ferromagnetic state by applying a first voltage waveform of a first polarity that increases the perpendicular magnetic anisotropy (PMA) present at an interface of a free layer and oxide layer of the element;
switching the element from the first ferromagnetic state to a second skyrmion state by applying a second voltage waveform of a second polarity that decreases the PMA present at the interface, wherein the second polarity is of opposite polarity to the first polarity;
switching the element from the second skyrmion state to a second ferromagnetic state by applying a third voltage waveform of the first polarity that increases the PMA present at the interface; and
switching the element from the second ferromagnetic state to the first skyrmion state by applying a fourth voltage waveform of the second polarity that decreases the PMA present at the interface,
wherein the first skyrmion state, the second skyrmion state, the first ferromagnetic state, and the second ferromagnetic state are all stable states in an absence of an applied voltage or external magnetic field bias.

### Claim 2 (depends on 1)

The method of claim 1, wherein the stable states are one or more of thermally stable and stable in the presence of magnetic fields.

### Claim 3 (depends on 1)

The method of claim 1, wherein each switching step is performed in an absence of a spin current or external magnetic field bias.

### Claim 4 (depends on 1)

The method of claim 1, wherein the element the state of which is switched by the method is configured to be a memory, Boolean, or non-Boolean element.

### Claim 5

A method of switching between states of a non-volatile magnetic element, comprising
applying a first voltage waveform of a first polarity that eliminates a first skyrmion state by increasing the perpendicular magnetic anisotropy (PMA) present at an interface of a free layer and oxide layer of the element; and
applying a second voltage waveform of a second polarity that creates a second skyrmion state by decreasing the PMA at the interface, wherein the second polarity is of opposite polarity to the first polarity.

### Claim 6 (depends on 5)

The method of claim 5, wherein switching is accomplished only with voltage control of magnetic anisotropy.

### Claim 7 (depends on 5)

The method of claim 5, wherein switching is accomplished without spin current or an external magnetic field.

### Claim 8 (depends on 5)

The method of claim 5, wherein the first and second voltage waveforms are each unipolar waveforms or separate parts of a bipolar waveform.

### Claim 9 (depends on 5)

The method of claim 5, wherein the element the state of which is switched by the method is configured to be or configured to be a part of a memory element, a Boolean element, or a non-Boolean element.

### Claim 10

A method of switching a non-volatile magnetic element comprising a magneto tunneling junction (MTJ) structure that includes an interface of a free layer with an oxide layer, the method comprising
applying a unipolar voltage waveform across the MTJ structure, the unipolar voltage waveform reducing a perpendicular magnetic anisotropy (PMA) of the interface such that an initial ferromagnetic state of a free layer of the MTJ structure changes to an intermediate skyrmionic state; and
removing the applied unipolar voltage waveform to restore the PMA to an original value, the removal annihilating the intermediate skyrmionic state and stabilizing a final ferromagnetic state that has opposite polarity of the original ferromagnetic state.

### Claim 11 (depends on 10)

The method of claim 10, wherein the applying and removing steps are performed in an absence of a spin current or external magnetic field bias.

### Claim 12 (depends on 10)

The method of claim 10, further comprising a step of providing a ferromagnetic fixed layer in the MTJ structure.

### Claim 13 (depends on 10)

The method of claim 10, wherein the element the state of which is switched by the method is configured to be or configured to be a part of a memory element, a Boolean element, or a non-Boolean element.

### Claim 14

A method of switching a non-volatile magnetic element comprising a magneto tunneling junction (MTJ) structure that includes an interface of a free layer with an oxide layer, the method comprising
applying a unipolar voltage waveform across the MTJ structure, the unipolar voltage waveform increasing a perpendicular magnetic anisotropy (PMA) of the interface such that an initial skyrmionic state of a free layer of the MTJ structure is annihilated and the free layer takes an intermediate ferromagnetic state; and
removing the applied unipolar voltage waveform to restore an original PMA and stabilize a final skyrmionic state that has opposite polarity of the original skyrmionic state.

### Claim 15 (depends on 14)

The method of claim 14, wherein the applying and removing steps are performed in an absence of a spin current or external magnetic field bias.

### Claim 16 (depends on 14)

The method of claim 14, further comprising a step of providing a skyrmionic fixed layer in the MTJ structure.

### Claim 17 (depends on 14)

The method of claim 14, wherein the element the state of which is switched by the method is configured to be or configured to be a part of a memory element, a Boolean element, or a non-Boolean element.

### Claim 18

A method of switching a non-volatile magnetic element comprising a magneto tunneling junction (MTJ) structure that includes an interface of a free layer with an oxide layer, the method comprising
controlling a perpendicular magnetic anisotropy (PMA) of the interface with a voltage waveform applied across the MTJ structure, said voltage waveform temporarily reducing the PMA and reducing a switching current from an initial value to a reduced value; and
switching a free layer of the MTJ structure between two skyrmionic states using a current that is equal to or greater than the reduced value and less than the initial value.

### Claim 19 (depends on 18)

The method of claim 18, wherein the PMA is reduced irrespective of the polarity of the voltage waveform.

### Claim 20 (depends on 18)

The method of claim 18, wherein the controlling and switching steps are performed in an absence of a magnetic field bias.

### Claim 21 (depends on 18)

The method of claim 18, wherein the element the state of which is switched by the method is configured to be or configured to be a part of a memory element, a Boolean element, or a non-Boolean element.

### Claim 22

A method of switching between states of a non-volatile magnetic element, comprising
applying a first voltage waveform of a first polarity that eliminates a first ferromagnetic state by decreasing the perpendicular magnetic anisotropy (PMA) present at an interface of a free layer and oxide layer of the element; and
applying a second voltage waveform of a second polarity that creates a second ferromagnetic state by increasing the PMA at the interface, wherein the second polarity is of opposite polarity to the first polarity.

### Claim 23 (depends on 22)

The method of claim 22, wherein switching is accomplished only with voltage control of magnetic anisotropy.

### Claim 24 (depends on 22)

The method of claim 22, wherein switching is accomplished without spin current or an external magnetic field.

### Claim 25 (depends on 22)

The method of claim 22, wherein the first and second voltage waveforms are each unipolar waveforms or separate parts of a bipolar waveform.

### Claim 26 (depends on 22)

The method of claim 22, wherein the element the state of which is switched by the method is configured to be or configured to be a part of a memory element, a Boolean element, or a non-Boolean element.