# US 10,955,612 B2 · Stress-managed specialty fiber for sensory application

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,955,612 B2
- Document ID: US10955612B2
- Status: Granted
- Kind: B2
- Application number: 16/286,517
- Filed: 2019-02-26
- Published: 2020-07-02
- Granted: 2021-03-23
- Earliest claimed: 2018-12-31
- Assignees: Sterlite Technologies Limited
- Applicants: Sterlite Technologies Limited
- Inventors: Pramod Watekar; Annesha Maity; Manoj Mittal; Sandeep Gaikwad; Sham Nagarkar; Bhalchandra Pathak; Sathis Ram
- Web page: https://patentgrep.com/patent/US10955612B2

## CPC

- G02B 6/03694: {Multiple layers differing in properties other than the refractive index, e.g. attenuation, diffusion, stress properties}
- G01D 5/3537: {Optical fibre sensor using a particular arrangement of the optical fibre itself}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G01D: MEASURING NOT SPECIALLY ADAPTED FOR A SPECIFIC VARIABLE; ARRANGEMENTS FOR MEASURING TWO OR MORE VARIABLES NOT COVERED IN A SINGLE OTHER SUBCLASS; TARIFF METERING APPARATUS; MEASURING OR TESTING NOT OTHERWISE PROVIDED FOR

## Abstract

Embodiments describe an optical fiber that includes a core. The core has high compressive stress. The compressive stress of the core is in a range of about 20 to 60 MPa. The optical fiber further includes a cladding. The cladding is divided into a first cladding layer and a second cladding layer. The second cladding layer has a high residual stress. The high residual stress of the second cladding layer is in a range of about 20 to 60 MPa. The optical fiber enables reduction of particle related breaks. Further, the optical fiber has elevated LLT strength. The LLT strength is about 6 Kg. The optical fiber has high proof test yield. Furthermore, the optical fiber is highly sensitive to micro-bending of the optical fiber.

## Claims

### Claim 1

An optical fiber for sensory applications comprising:
a core, wherein the core has high compressive stress; and
a cladding, wherein the cladding is characterized by high residual stress.

### Claim 2 (depends on 1)

The optical fiber as claimed in claim 1, wherein the optical fiber is highly sensitive to micro-bending of the optical fiber.

### Claim 3 (depends on 1)

The optical fiber as claimed in claim 1, wherein the cladding comprises a first cladding layer and a second cladding layer, wherein the first cladding layer is an inner cladding layer and the second cladding layer is an outer cladding layer, wherein the first cladding layer and the second cladding layer is made of silica.

### Claim 4 (depends on 1)

The optical fiber as claimed in claim 1, wherein the cladding comprises a first cladding layer and a second cladding layer, wherein the first cladding layer of the cladding has low residual stress.

### Claim 5 (depends on 1)

The optical fiber as claimed in claim 1, wherein the cladding comprises a first cladding layer and a second cladding layer, wherein the second cladding layer has high residual stress, wherein residual stress of the second cladding layer facilitates high compressive stress of the core, wherein residual stress of the second cladding layer causes enhanced geometrical deformations at a boundary of the core and the first cladding layer and at a boundary of the first cladding layer and the second cladding layer.

### Claim 6 (depends on 1)

The optical fiber as claimed in claim 1, wherein the cladding comprises a first cladding layer and a second cladding layer, wherein the second cladding layer of the cladding is highly sensitive to residual stress causing attenuation of about 0.35 dB/km at a wavelength of about 1310 nm.

### Claim 7 (depends on 1)

The optical fiber as claimed in claim 1, wherein the cladding comprises a first cladding layer and a second cladding layer, wherein the second cladding layer of the cladding is sensitive to residual stress causing the attenuation at a value of about 0.33 decibels per kilometer at a wavelength of 1310 nanometers.

### Claim 8 (depends on 1)

The optical fiber as claimed in claim 1, wherein the optical fiber enables reduction of particle related breaks, wherein the optical fiber has elevated LLT strength, wherein the LLT strength is about 6 Kg, wherein the optical fiber has high proof test yield.

### Claim 9

An optical fiber for sensory applications comprising:
a core, wherein the core has high compressive stress; and
a cladding, wherein the cladding comprises a first cladding layer and a second cladding layer, wherein the second cladding layer has high residual stress,
wherein the optical fiber is highly sensitive to micro-bending of the optical fiber.

### Claim 10 (depends on 9)

The optical fiber as claimed in claim 9, wherein the first cladding layer has low residual stress.

### Claim 11 (depends on 9)

The optical fiber as claimed in claim 9, wherein residual stress of the second cladding layer facilitates high compressive stress of the core, wherein residual stress of the second cladding layer causes enhanced geometrical deformations at a boundary of the core and the first cladding layer and at a boundary of the first cladding layer and the second cladding layer.

### Claim 12 (depends on 9)

The optical fiber as claimed in claim 9, wherein the second cladding layer of the cladding is highly sensitive to residual stress causing attenuation of about 0.35 dB/km at a wavelength of about 1310 nm.

### Claim 13 (depends on 9)

The optical fiber as claimed in claim 9, wherein the second cladding layer of the cladding is sensitive to residual stress causing the attenuation at a value of about 0.33 decibels per kilometer at a wavelength of 1310 nanometers.

### Claim 14 (depends on 9)

The optical fiber as claimed in claim 9, wherein the optical fiber enables reduction of particle related breaks, wherein the optical fiber has elevated LLT strength, wherein the LLT strength is about 6 Kg, wherein the optical fiber has high proof test yield.

### Claim 15

An optical fiber for sensory applications comprising:
a core, wherein the core has high compressive stress, wherein compressive stress of the core is in a range of about 20-60 MPa; and
a cladding, wherein the cladding comprises a first cladding layer and a second cladding layer, wherein the second cladding layer has high residual stress, wherein residual stress of the second cladding layer is in a range of about 20 to 60 MPa,
wherein the optical fiber is highly sensitive to micro-bending of the optical fiber.

### Claim 16 (depends on 15)

The optical fiber as claimed in claim 15, wherein the second cladding layer of the optical fiber is sensitive to micro-bending loss at a value of about 0.35 decibels per kilometer.

### Claim 17 (depends on 15)

The optical fiber as claimed in claim 15, wherein the second cladding layer of the cladding is sensitive to attenuation at a value of about 0.33 decibels per kilometer at a wavelength of about 1310 nanometer.

### Claim 18 (depends on 15)

The optical fiber as claimed in claim 15, wherein the optical fiber enables reduction of particle related breaks, wherein the optical fiber has elevated LLT strength, the LLT strength is about 6 Kg wherein the optical fiber has high proof test yield.