# US 10,955,567 B2 · Scintillating nanocomposites

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,955,567 B2
- Document ID: US10955567B2
- Status: Granted
- Kind: B2
- Application number: 15/771,163
- Filed: 2016-11-07
- Published: 2018-10-25
- Granted: 2021-03-23
- Earliest claimed: 2015-11-19
- Assignees: Koninklijke Philips N.V.
- Applicants: Koninklijke Philips N.V.
- Inventors: Aneta Wiatrowska; Herfried Karl Wieczorek; Cornelis Reinder Ronda; Wilhelmus Cornelis Keur; Malgorzata Nachman
- Web page: https://patentgrep.com/patent/US10955567B2

## CPC

- G01T 1/2033: {Selection of materials}
- C09K 11/02: Use of particular materials as binders, particle coatings or suspension media therefor
- C09K 11/025: {non-luminescent particle coatings or suspension media}
- C09K 11/7774: {Aluminates}
- G01T 1/1606: {with other specified detectors not provided for in the other subgroups of G01T1/16}
- G01T 1/203: the detector being made of plastics
- G21K 4/00: Conversion screens for the conversion of the spatial distribution of X-rays or particle radiation into visible images, e.g. fluoroscopic screens (photographic processes using X-ray intensifiers G03C5/17; discharge tubes comprising luminescent screens H01J1/62; cathode ray tubes for X-ray conversion with optical output H01J31/50)
- B82Y 15/00: Nanotechnology for interacting, sensing or actuating, e.g. quantum dots as markers in protein assays or molecular motors
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- B82Y 40/00: Manufacture or treatment of nanostructures
- G01T: MEASUREMENT OF NUCLEAR OR X-RADIATION (radiation analysis of materials, mass spectrometry G01N23/00; tubes for determining the presence, intensity, density or energy of radiation or particles H01J47/00)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- G21K: HANDLING OF PARTICLES OR IONISING RADIATION NOT OTHERWISE PROVIDED FOR; IRRADIATION DEVICES; GAMMA RAY OR X-RAY MICROSCOPES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

An improved scintillator nanocomposite comprising nanoparticles with scintillating properties and a diameter between 10 and 50 nanometer and a first matrix material comprises is obtained by introducing the nanoparticles into a dispersing medium to form a stable suspension. The dispersing medium is a precursor to the first matrix material, which is cured to form the first matrix material.

## Claims

### Claim 1

A method for producing a scintillator nanocomposite, the method comprising:
introducing nanoparticles into a first dispersing medium to form a stable suspension, wherein the first dispersing medium is a precursor for a first matrix material; and
curing the first dispersing medium to form the first matrix material,
wherein the scintillator nanocomposite comprises the nanoparticles with scintillating properties and a diameter between 10 and 50 nanometer and the first matrix material.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the nanoparticles are garnet nanoparticles.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the first matrix material is a polymeric material.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the dispersing medium is a glycol.

### Claim 5 (depends on 1)

The method according to claim 1, wherein a second dispersing medium is mixed with the first dispersing medium prior to introducing the nanoparticles or to the stable suspension, wherein the second dispersing medium is a precursor for a second matrix material.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the second matrix material is a polymeric material, preferably a polymeric material selected from the group of polyurethane, polyester, such as polybutylene terephthalate, unsaturated polyester resin, aromatic polyamide, aromatic polyimide, polystyrene or polysulfone.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the curing results in a co-polymer of the first matrix material and the second matrix material.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the curing is performed at elevated temperature, and/or at elevated pressure greater than 20 bar, and/or for at least 24 hours.

### Claim 9

A scintillator nanocomposite comprising:
nanoparticles with scintillating properties and a diameter between 10 and 50 nanometer; and
a first matrix material; and
wherein the nanoparticles are introduced into a first dispersing medium to form a stable suspension; and
wherein the first matrix material is formed by curing the first dispersing medium.

### Claim 10 (depends on 9)

The scintillator nanocomposite according to claim 9, wherein the first matrix material is polyurethane.

### Claim 11 (depends on 9)

A product comprising the scintillator nanocomposite according to claim 9.

### Claim 12

A method to produce a transparent scintillator comprising:
melting a nanocomposite obtained with a method comprising introducing the nanoparticles into a first dispersing medium to form a stable suspension, wherein the first dispersing medium is a precursor for the first matrix material;
curing the first dispersing medium to form the first matrix material; and
injection molding the molten nanocomposite; and
wherein the scintillator nanocomposite comprises the nanoparticles with scintillating properties and a diameter between 10 and 50 nanometer and the first matrix material.

### Claim 13 (depends on 12)

A transparent scintillator obtainable by the method according to claim 12.

### Claim 14 (depends on 13)

A radiation detector comprising the transparent scintillator according to claim 13.

### Claim 15 (depends on 14)

An imaging system comprising the radiation detector according to claim 14.

### Claim 16 (depends on 2)

The method according to claim 2, wherein the nanoparticles are Cerium-doped nanoparticles.

### Claim 17 (depends on 2)

The method according to claim 2, wherein the nanoparticles are chosen from the group of Y3Al5O12:Ce nanoparticles, (Lu,Gd)3Al5O12:Ce nanoparticles or (LGGAG:Ce) nanoparticles.

### Claim 18 (depends on 3)

The method according to claim 3, wherein the polymeric material comprises a polymeric material selected from the group of polyurethane, polyester, polybutylene terephthalate, unsaturated polyester resin, aromatic polyamide, aromatic polyimide, polystyrene or polysulfone.

### Claim 19 (depends on 4)

The method according to claim 4, wherein the glycol comprises a 1, 4 butanediol.

### Claim 20 (depends on 8)

The method according to claim 8,
wherein the elevated temperature is between 220 degrees Celsius and 250 degrees Celsius; and/or
wherein the elevated pressure is about 40 bar.