# US 10,955,350 B2 · SiC wafer defect measuring method, reference sample, and method of manufacturing SiC epitaxial wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,955,350 B2
- Document ID: US10955350B2
- Status: Granted
- Kind: B2
- Application number: 16/471,370
- Filed: 2017-12-07
- Published: 2019-10-31
- Granted: 2021-03-23
- Earliest claimed: 2016-12-28
- Assignees: Showa Denko K.K.
- Applicants: Showa Denko K.K.
- Inventors: Koji Kamei
- Web page: https://patentgrep.com/patent/US10955350B2

## CPC

- G01N 21/6489: {Photoluminescence of semiconductors}
- C30B 25/02: Epitaxial-layer growth
- C30B 25/04: Pattern deposit, e.g. by using masks
- C30B 29/06: Silicon
- C30B 29/36: Carbides
- G01B 11/02: for measuring length, width or thickness (G01B11/08 takes precedence)
- G01N 21/9501: {Semiconductor wafers (manufacturing processes per se of semiconductor devices implementing a measuring step H10P74/20)}
- G01N 21/95607: {using a comparative method}
- H10P 14/3408: {Silicon carbide}
- H10P 72/0616: {Monitoring of warpages, curvatures, damages, defects or the like}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- G01B: MEASURING LENGTH, THICKNESS OR SIMILAR LINEAR DIMENSIONS; MEASURING ANGLES; MEASURING AREAS; MEASURING IRREGULARITIES OF SURFACES OR CONTOURS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A SiC wafer defect measuring method which includes a device management step of managing a defect measuring device by irradiating a reference sample made of a material having a light-emitting intensity that does not change with repeated irradiation by excitation light and which has a pattern made of recesses and/or protrusions in the surface, the irradiation by the excitation light being performed before measuring defects in a SiC wafer and under the same irradiation conditions as the measurement of the defects in the SiC wafer, and then measuring the S/N ratio of the pattern from a reflection image of the pattern.

## Claims

### Claim 1

A SiC wafer defect measuring method of measuring defects in a SiC wafer using a photoluminescence device, the method comprising:
a device management step of managing a defect measuring device by irradiating a reference sample which is made of a material having a light-emitting intensity that does not change with repeated irradiation by excitation light and which has a pattern made of recesses and/or protrusions in a surface thereof, the irradiation by the excitation light being performed before measuring defects in a SiC wafer and under the same irradiation conditions as the measurement of the defects in the SiC wafer, and then measuring a S/N ratio of the pattern from a reflection image of the pattern.

### Claim 2 (depends on 1)

The SiC wafer defect measuring method according to claim 1, wherein a plurality of the patterns are formed in the reference sample.

### Claim 3 (depends on 2)

The SiC wafer defect measuring method according to claim 2, wherein a number density of patterns formed in the reference sample is from 0.1 to 1000 patterns/cm2.

### Claim 4 (depends on 2)

The SiC wafer defect measuring method according to claim 2, wherein a number of patterns is measured from a reflection image of the pattern by using a S/N ratio of the reflection image.

### Claim 5 (depends on 2)

The SiC wafer defect measuring method according to claim 2, wherein a number of patterns is measured automatically from a reflection image of the pattern.

### Claim 6 (depends on 1)

The SiC wafer defect measuring method according to claim 1, wherein the pattern includes a plurality of element patterns made of recesses and/or protrusions in a surface of the material.

### Claim 7 (depends on 6)

The SiC wafer defect measuring method according to claim 6, wherein an aspect ratio between a depth and a length of a long side of the element pattern is at least 0.04.

### Claim 8 (depends on 6)

The SiC wafer defect measuring method according to claim 6, wherein the element pattern has a rectangular shape.

### Claim 9 (depends on 6)

The SiC wafer defect measuring method according to claim 6, wherein a length of a long side of the element pattern is 100 μm or less.

### Claim 10 (depends on 1)

The SiC wafer defect measuring method according to claim 1, wherein a length of a short side of a pattern formed in the reference sample is from 5 to 50 μm in the reflection image, and a length of a long side is at least 10 μm.

### Claim 11

A reference sample used in a method of measuring defects in a SiC wafer using a photoluminescence device,
wherein the reference sample is made of a material having a light-emitting intensity that does not change with repeated irradiation by excitation light, and has a pattern made of recesses and/or protrusions in a surface thereof,
wherein the pattern includes a plurality of element patterns made of recesses and/or protrusions in a surface of the material, and
wherein an aspect ratio between a depth and a length of a long side of the element pattern is at least 0.04.

### Claim 12 (depends on 11)

The reference sample according to claim 11, wherein a plurality of the patterns are formed.

### Claim 13

A method of manufacturing a SiC epitaxial wafer, the method comprising:
a device management step of managing a defect measuring device by irradiating a reference sample which is made of a material having a light-emitting intensity that does not change with repeated irradiation by excitation light and which has a plurality of patterns made of recesses and/or protrusions in a surface thereof, the irradiation by the excitation light being performed before measuring defects in a SiC wafer and under the same irradiation conditions as the measurement of the defects in the SiC wafer, and then measuring a S/N ratio of the pattern from a reflection image of the pattern.