# US 10,955,332 B2 · Flow cell package and method for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,955,332 B2
- Document ID: US10955332B2
- Status: Granted
- Kind: B2
- Application number: 15/848,450
- Filed: 2017-12-20
- Published: 2018-07-12
- Granted: 2021-03-23
- Earliest claimed: 2016-12-22
- Assignees: Illumina, Inc.; Illumina Cambridge Limited
- Applicants: Illumina, Inc.; Illumina Cambridge Limited
- Inventors: James Tsay; Anmiv Prabhu; David Heiner; Edwin Li; Alexandre Richez; John M. Beierle; Kevan Samiee; Kristina Munoz; Leonid Malevanchik; Ludovic Vincent; Naiqian Zhan; Peyton Shieh; Robert Yang; Samantha Schmitt; Sang Park; Scott Bailey; Sean M. Ramirez; Sunmin Ahn; Valerie Uzzell; Wei Wei; Yuxiang Huang; Tyler Jamison Dill
- Web page: https://patentgrep.com/patent/US10955332B2

## CPC

- G01N 15/1436: {the optical arrangement forming an integrated apparatus with the sample container, e.g. a flow cell}
- B01J 19/0046: {Sequential or parallel reactions, e.g. for the synthesis of polypeptides or polynucleotides; Apparatus and devices for combinatorial chemistry or for making molecular arrays (synthesis methods per se C40B50/00)}
- B01L 3/502: {with fluid transport, e.g. in multi-compartment structures}
- B01L 3/502707: {characterised by the manufacture of the container or its components}
- C09D 133/24: Homopolymers or copolymers of amides or imides
- C09D 133/26: Homopolymers or copolymers of acrylamide or methacrylamide
- C12Q 1/6874: involving nucleic acid arrays, e.g. sequencing by hybridisation
- G01N 15/1484: {microstructural devices}
- B01J 2219/00286: Reactor vessels with top and bottom openings
- B01J 2219/00317: Microwell devices, i.e. having large numbers of wells
- B01J 2219/00319: the blocks being mounted in stacked arrangements
- B01J 2219/00418: using pressure
- B01J 2219/00585: Parallel processes
- B01J 2219/00596: Solid-phase processes
- B01J 2219/00612: the surface being inorganic
- B01J 2219/00637: by coating it with another layer
- B01J 2219/00662: Two-dimensional arrays within two-dimensional arrays
- B01J 2219/00722: Nucleotides
- B01L 2200/12: Specific details about manufacturing devices
- B01L 2300/0829: Multi-well plates; Microtitration plates
- B01L 2300/0848: Specific forms of parts of containers
- B01L 2300/087: Multiple sequential chambers
- B01L 2300/0887: Laminated structure
- B01L 2300/16: Surface properties and coatings
- G01N 2015/1006: {for cytology}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B01L: CHEMICAL OR PHYSICAL LABORATORY APPARATUS FOR GENERAL USE
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C12Q: MEASURING OR TESTING PROCESSES INVOLVING ENZYMES, NUCLEIC ACIDS OR MICROORGANISMS (immunoassay G01N33/53); COMPOSITIONS OR TEST PAPERS THEREFOR; PROCESSES OF PREPARING SUCH COMPOSITIONS; CONDITION-RESPONSIVE CONTROL IN MICROBIOLOGICAL OR ENZYMOLOGICAL PROCESSES

## Abstract

A flow cell package includes first and second surface-modified patterned wafers and a spacer layer. The first surface-modified patterned wafer includes first depressions separated by first interstitial regions, a first functionalized molecule bound to a first silane or silane derivative in at least some of the first depressions, and a first primer grafted to the first functionalized molecule in the at least some of the first depressions. The second surface-modified patterned wafer includes second depressions separated by second interstitial regions, a second functionalized molecule bound to a second silane or silane derivative in at least some of the second depressions, and a second primer grafted to the second functionalized molecule in the at least some of the second depressions. The spacer layer bonds at least some first interstitial regions to at least some second interstitial regions, and at least partially defines respective fluidic chambers of the flow cell package.

## Claims

### Claim 1

A method, comprising:
forming a surface-modified patterned wafer by:
attaching a silane or a silane derivative to a surface of a patterned wafer including depressions separated by interstitial regions, thereby forming silanized depressions and silanized interstitial regions;
forming a coating layer of a functionalized molecule in the silanized depressions and on the silanized interstitial regions, wherein the functionalized molecule is a hydrogel;
polishing the coating layer from the silanized interstitial regions while leaving the coating layer in the silanized depressions and leaving the surface of the patterned wafer at least substantially intact, wherein the polishing is performed using i) a basic, aqueous slurry having a pH ranging from about 7.5 to about 11 and including an abrasive particle having a hardness that is less than a hardness of the patterned wafer and a polyacrylate dispersant, the abrasive particle being selected from the group consisting of calcium carbonate, agarose, graphite, poly(methyl methacrylate), and polystyrene, or ii) a polishing pad and a solution free of the abrasive particle; and
grafting a primer to the coating layer in the silanized depressions to form functionalized depressions; and
bonding two of the surface-modified patterned wafers together with a spacer layer therebetween.

### Claim 2 (depends on 1)

The method as defined in claim 1 wherein attaching the silane or the silane derivative to the surface of the patterned wafer involves at least one of vapor deposition, spin coating, chemical vapor deposition, or Yield Engineering Systems (YES) method.

### Claim 3 (depends on 1)

The method as defined in claim 1 wherein forming the coating layer of the functionalized molecule involves reacting a functional group of the functionalized molecule with an unsaturated moiety of the silane or silane derivative, and optionally wherein the unsaturated moiety is selected from the group consisting of cycloalkenes, cycloalkynes, heterocycloalkenes, heterocycloalkynes, substituted variants thereof, and combinations thereof.

### Claim 4 (depends on 1)

The method as defined in claim 1 wherein forming the coating layer of the functionalized molecule includes:
depositing a solution including the functionalized molecule onto the silanized depressions and the silanized interstitial regions; and
curing the functionalized molecule.

### Claim 5 (depends on 1)

The method as defined in claim 1 wherein the basic, aqueous slurry further includes a chelating agent, a surfactant, or a combination thereof.

### Claim 6 (depends on 1)

The method as defined in claim 1 wherein grafting of the primer to the coating layer involves dunk coating, spray coating, puddle dispensing, or a combination thereof.

### Claim 7 (depends on 1)

The method as defined in claim 1, further comprising plasma ashing the patterned wafer prior to attaching the silane or the silane derivative.

### Claim 8 (depends on 1)

The method as defined in claim 1 wherein the coating layer of the functionalized molecule has a thickness of about 200 nm or less.

### Claim 9 (depends on 1)

The method as defined in claim 1, further comprising dicing the bonded surface-modified patterned wafers into respective flow cells.

### Claim 10 (depends on 1)

The method as defined in claim 1 wherein the spacer layer is a radiation-absorbing material.

### Claim 11 (depends on 10)

The method as defined in claim 10, wherein the bonding involves:
positioning the radiation-absorbing material at an interface between the two surface-modified patterned wafers such that the radiation-absorbing material contacts at least some of the interstitial regions of each of the two surface-modified patterned wafers; and
applying compression at the interface and irradiating the radiation-absorbing material.

### Claim 12 (depends on 1)

The method as defined in claim 1 wherein the spacer layer includes a radiation-absorbing material in contact therewith.

### Claim 13 (depends on 12)

The method as defined in claim 12, wherein the bonding involves:
positioning the radiation-absorbing material at a respective interface between the spacer layer and each of the two surface-modified patterned wafers such that the radiation-absorbing material contacts at least some of the interstitial regions of each of the two surface-modified patterned wafers; and
applying compression at the respective interfaces and irradiating the radiation-absorbing material.

### Claim 14 (depends on 10)

The method as defined in claim 10 wherein:
the two surface-modified patterned wafers are positioned so that at least some of the functionalized depressions of one of the two surface-modified patterned wafers are aligned with a respective functionalized depression of another of the two surface-modified patterned wafers to form a fluidic chamber; and
the spacer layer defines longitudinal walls between adjacent fluidic chambers.

### Claim 15 (depends on 14)

The method as defined in claim 14 wherein each of the functionalized depressions is:
in a flow channel defined by the two bonded surface-modified patterned wafers; or
one of a plurality of wells within the flow channel.

### Claim 16

A method, comprising:
forming a surface-modified patterned wafer by:
plasma ashing a surface of a patterned wafer including depressions separated by interstitial regions;
forming a coating layer of a functionalized molecule in the depressions and on the interstitial regions, wherein the functionalized molecule is a hydrogel;
polishing the coating layer from the interstitial regions while leaving the coating layer in the depressions and leaving the surface of the patterned wafer at least substantially intact, wherein the polishing is performed, using i) a basic, aqueous slurry having a pH ranging from about 7.5 to about 11 and including an abrasive particle having a hardness that is less than a hardness of patterned wafer and a polyacrylate dispersant, the abrasive particle being selected from the group consisting of calcium carbonate, agarose, graphite, poly(methyl methacrylate), and polystyrene, or ii) a polishing pad and a solution free of the abrasive particle; and
grafting a primer to the coating layer in the depressions to form functionalized depressions; and
bonding two of the surface-modified patterned wafers together with a spacer layer therebetween.

### Claim 17 (depends on 1)

The method as defined in claim 1 wherein the polyacrylate dispersant is poly(acrylic acid sodium salt).

### Claim 18 (depends on 1)

The method as defined in claim 1 wherein the hydrogel is poly(N-(5-azidoacetamidylpentyl) acrylamide-co-acrylamide).

### Claim 19 (depends on 1)

The method as defined in claim 1 wherein the abrasive particles have an average particle size ranging from about 700 nm to about 5 μm.

### Claim 20 (depends on 1)

The method as defined in claim 1, wherein the basic, aqueous slurry consists of the abrasive particle, the polyacrylate dispersant, a buffer, a chelating agent, a surfactant, and water.

### Claim 21 (depends on 1)

The method as defined in claim 1, wherein the polishing uses the solution free of the abrasive particle.