# US 10,954,728 B2 · Hardbanding method and apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,728 B2
- Document ID: US10954728B2
- Status: Granted
- Kind: B2
- Application number: 16/238,078
- Filed: 2019-01-02
- Published: 2019-05-09
- Granted: 2021-03-23
- Earliest claimed: 2014-03-10
- Assignees: Postle Industries, Inc.
- Applicants: Postle Industries, Inc.
- Inventors: Robert F. Miller
- Web page: https://patentgrep.com/patent/US10954728B2

## CPC

- E21B 17/1085: {Wear protectors; Blast joints; Hard facing}
- B23K 9/0026: {specially adapted for particular articles or work}
- B23K 9/048: {on cylindrical surfaces}
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

Various methods of hardbanding an apparatus are described. In one aspect of the invention an improved method of re-applying a hardbanding alloy to worn tool joints of a previously hardbanded drill pipe results in preservation of the metallurgical properties of the drill pipe and preservation of the internal polymer coating that lines the drill pipe. A method for applying hardbanding includes arc welding a consumable metal welding wire to a tool joint having a surface temperature that ranges from about 50° F. to about 170° F. and the arc welding power supply utilizes DC current. The method herein produces a hardbanded tool joint comprising a heat affected zone (HAZ) of a based metal having a Rockwell hardness of 40 Rc or less.

## Claims

### Claim 1

A method of hardbanding a tool joint of a drill pipe in a region of said drill pipe that has been previously hardbanded, the method comprising:
providing said drill pipe that includes a tube portion and a tool joint, said tool joint positioned at one end region of said drill pipe, an outer surface of said tool joint having a prior hardbanding alloy and a base metal heat-affected zone that was formed during application of said prior hardbanding alloy, said base metal heat-affected zone extending about the sides and bottom of said prior hardbanding alloy, said base metal heat-affected zone extending a greater depth into said tool joint than said prior hardbanding alloy; and,
applying a secondary hardfacing alloy on at least a portion of a top surface of said prior hardbanding alloy by welding a consumable metal welding wire onto at least a portion of said top surface of said prior hardbanding alloy, a top surface of said secondary hardfacing alloy extending above said top surface of said prior hardfacing alloy and also above a top surface of said tool joint, said step of applying said secondary hardfacing alloy forms a secondary heat-affected zone at least partially in said prior hardbanding alloy, a depth of said secondary heat-affected zone in said tool joint is less than a depth of said base metal heat-affected zone in said tool joint.

### Claim 2 (depends on 1)

The method as defined in claim 1, wherein said secondary heat-affected zone that is positioned in said prior hardbanding alloy does not fully extend through said prior hardbanding alloy.

### Claim 3 (depends on 1)

The method as defined in claim 1, wherein said prior hardbanding alloy is formed from one or more prior weld beads each having a width, said secondary hardfacing alloy applied as one or more secondary weld beads, a width of each of said secondary weld bead is 20-60% said width of each of said prior weld heads.

### Claim 4 (depends on 1)

The method as defined in claim 1, wherein said base metal heat-affected zone has a hardness of no greater than 40 Rc prior to said step of applying said secondary hardfacing alloy, and said base metal heat-affected zone that is not affected by said step of applying said secondary hardfacing alloy is no more than 40 Rc.

### Claim 5 (depends on 1)

The method as defined in claim 1, wherein a temperature of said tool joint does not exceed 150° F. prior to said step of applying said secondary hardfacing alloy.

### Claim 6 (depends on 1)

The method as defined in claim 1, wherein said metal welding wire is applied to said tool joint while rotating said tool joint at a speed of 0.25-3 revolutions per minute, said tool joint is cooled at a rate of 100-300° F. per hour after applying said secondary hardfacing alloy to said tool joint.

### Claim 7 (depends on 1)

The method as defined in claim 1, wherein said drill pipe includes a polymer coating on an inner surface of a cavity of said drill pipe, said polymer coating not damaged by heat during said step of applying said secondary hardfacing alloy, no fluid cooling liquid medium flows through said cavity of said drill pipe during said step of applying said secondary hardfacing alloy.

### Claim 8 (depends on 1)

The method as defined in claim 1, wherein said step of applying said secondary hardfacing alloy forms at least three zones of hardness, said secondary hardfacing alloy having a hardness that is greater than a hardness of said secondary heat-affected zone, said secondary heat-affected zone having a hardness that is greater than a hardness of said base metal heat-affected zone.

### Claim 9

A method of hardbanding a tool joint of a drill pipe in a region of said drill pipe that has been previously hardbanded, the method comprising:
providing said drill pipe that includes a tube portion and a tool joint that is positioned at one end region of said drill pipe, said tool joint having a larger outer diameter than an outer diameter of said tube portion, an outer surface of said tool joint having a prior hardbanding alloy and a base metal heat-affected zone that was formed during application of said prior hardbanding alloy, said base metal heat-affected zone extending about the sides and bottom of said prior hardbanding alloy, said base metal heat-affected zone extending a greater depth into said tool joint than said prior hardbanding alloy; and,
arc welding a consumable metal welding wire onto a top surface of said prior hardbanding alloy to form a secondary hardfacing alloy, a top surface of said secondary hardfacing alloy extending above said top surface of said prior hardfacing alloy and also extending above a top surface of said tool joint;
and wherein said step of arc welding forms a secondary heat-affected zone at least partially in said prior hardbanding alloy, a depth of said secondary heat-affected zone in said tool joint is less than a depth of said base metal heat-affected zone in said tool joint.

### Claim 10 (depends on 9)

The method as defined in claim 9, wherein said hardness of said base metal heat-affected zone after said step of arc welding that is not affected by said arc welding of said secondary hardfacing alloy is less than about 4Rc.

### Claim 11 (depends on 9)

The method as defined in claim 9, wherein said base metal heat-affected zone includes iron alloy, said base metal heat-affected zone prior to said step of arc welding having a Rockwell hardness of less than about 40 Rc.

### Claim 12 (depends on 9)

The method as defined in claim 9, wherein said secondary heat-affected zone positioned in said prior hardbanding alloy does not fully extend through said prior hardbanding alloy.

### Claim 13 (depends on 9)

The method as defined in claim 9, wherein said prior hardbanding alloy is formed from one or more prior weld beads each having a width, said secondary hardfacing alloy applied as one or more secondary weld beads, a width of each of said secondary weld bead is 20-60% said width of each of said prior weld beads.

### Claim 14 (depends on 9)

The method as defined in claim 9, wherein a temperature of said pipe does not exceed 150° F. prior to said step of applying said secondary hardfacing alloy.

### Claim 15 (depends on 9)

The method as defined in claim 9, wherein said metal welding wire is applied to said pipe while rotating said pipe at a speed of 0.25-3 revolutions per minute, said pipe is cooled at a rate of 100-300° F. per hour after applying said secondary hardfacing alloy to said pipe.

### Claim 16 (depends on 9)

The method as defined in claim 9, wherein said pipe includes a polymer coating on an inner surface of a cavity of said pipe, said polymer coating not damaged by heat during said step of applying said secondary hardfacing alloy, no fluid cooling liquid medium flows through said cavity of said pipe during said step of applying said secondary hardfacing alloy.

### Claim 17 (depends on 9)

The method as defined in claim 9, wherein said step of applying said secondary hardfacing alloy forms at least three zones of hardness, said secondary hardfacing alloy having a hardness greater than a hardness of said secondary heat-affected zone, said secondary heat-affected zone having a hardness greater than a hardness of said base metal heat-affected zone.