# US 10,954,630 B2 · Process for producing cellulose with low impurities from sugarcane bagasse

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,630 B2
- Document ID: US10954630B2
- Status: Granted
- Kind: B2
- Application number: 15/753,943
- Filed: 2016-08-19
- Published: 2019-01-10
- Granted: 2021-03-23
- Earliest claimed: 2015-08-19
- Assignees: Godavari Biorefineries Limited
- Applicants: Godavari Biorefineries Ltd.
- Inventors: Sangeeta Srivastava; Ramesh Shettar; Rakesh Kumar Jain; Ashwani Kumar Dixit; Diwakar Pandey
- Web page: https://patentgrep.com/patent/US10954630B2

## CPC

- D21C 5/005: {Treatment of cellulose-containing material with microorganisms or enzymes}
- C12N 9/248: {Xylanases}
- D21C 3/02: with inorganic bases or alkaline reacting compounds, e.g. sulfate processes
- D21C 3/022: {in presence of S-containing compounds}
- D21C 5/00: Other processes for obtaining cellulose, e.g. cooking cotton linters (obtaining fibres for spinning D01C); {Processes characterised by the choice of cellulose-containing starting materials}
- D21C 9/10: Bleaching {; Apparatus therefor}
- D21C: PRODUCTION OF CELLULOSE BY REMOVING NON-CELLULOSE SUBSTANCES FROM CELLULOSE-CONTAINING MATERIALS; REGENERATION OF PULPING LIQUORS; APPARATUS THEREFOR
- C12N: MICROORGANISMS OR ENZYMES; COMPOSITIONS THEREOF; PROPAGATING, PRESERVING, OR MAINTAINING MICROORGANISMS; MUTATION OR GENETIC ENGINEERING; CULTURE MEDIA (microbiological testing media C12Q1/00)

## Abstract

The present invention relates to a process for producing cellulose with low inorganic impurities from sugarcane bagasse, the process comprising treating prehydrolysed sugarcane bagasse with a mixture of sulfite and at least one alkali to obtain residue having undissolved cellulose along with lignin rich liquor. The residue having undissolved cellulose is further subjected to delignification and addition of at least one enzyme to obtain a cellulose rich pulp. The cellulose rich pulp obtained is then treated with bleaching agents followed by separating pure cellulose rich pulp having high a-cellulose content and low inorganic impurities.

## Claims

### Claim 1

A process for producing cellulose from sugarcane bagasse, the process comprising:
treating prehydrolyzed sugarcane bagasse in the absence of anthraquinone with mixture of sulfite and at least one alkali to obtain a residue having undissolved cellulose along with lignin rich liquor, the prehydrolyzed sugarcane bagasse is obtained by treating sugarcane bagasse residue with water at a temperature in a range of 120° C.-170° C.;
subjecting the residue having undissolved cellulose to delignification at a temperature in a range of 60° C.-140° C., at a pH of 10-11 in the presence of 2-4% of sodium hydroxide and oxygen pressure at 3-5 kgs; and
after the delignification, adding at least one enzyme to obtain a cellulose rich pulp having less than 0.05% of inorganic impurities including silica;
wherein the cellulose rich pulp is suitable for making microcrystalline cellulose or cellulose esters.

### Claim 2 (depends on 1)

The process as claimed in claim 1, wherein the sulfite is sodium sulfite and the alkali is selected from sodium carbonate, sodium hydroxide or mixture thereof.

### Claim 3 (depends on 2)

The process as claimed in claim 2, comprising 5%-10% sodium sulfite, 1%-4% sodium carbonate and 7%-18% sodium hydroxide and wherein the process is carried out at a temperature in the range of 140° C. -180° C.

### Claim 4 (depends on 1)

The process as claimed in claim 1, comprising:
treating the cellulose rich pulp with a bleaching agent to obtain a pure cellulose rich pulp; and
separating the pure cellulose rich pulp having a high α-cellulose content.

### Claim 5 (depends on 1)

The process as claimed in claim 1, wherein the enzyme is selected from a class of hemicelluloses including xylanase, and wherein the enzyme is added at a temperature of 30° C.-60° C. and pH of 5-8.

### Claim 6 (depends on 4)

The process as claimed in claim 4, comprising adding an elemental chlorine free bleaching agent followed by adding 2%-5% sodium hydroxide and 2-4% hydrogen peroxide, further followed by treatment with elemental free chlorine bleaching agent to the cellulose rich pulp to obtain the pure cellulose rich pulp.

### Claim 7 (depends on 4)

The process as claimed in claim 4, wherein the bleaching agent is selected from chlorine dioxide, and the bleaching agent is added at a temperature in a range of 40° C.-90° C. at a pH of 2-4.