# US 10,954,615 B2 · Migration resistant batting with stretch and methods of making and articles comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,615 B2
- Document ID: US10954615B2
- Status: Granted
- Kind: B2
- Application number: 15/542,678
- Filed: 2016-01-20
- Published: 2017-12-28
- Granted: 2021-03-23
- Earliest claimed: 2015-01-21
- Assignees: Primaloft, Inc.
- Applicants: Primaloft, Inc.
- Inventors: Vanessa Mason
- Web page: https://patentgrep.com/patent/US10954615B2

## CPC

- D04H 1/43835: {Mixed fibres, e.g. at least two chemically different fibres or fibre blends}
- D02G 1/00: Producing crimped or curled fibres, filaments, yarns, or threads, giving them latent characteristics (yarns per se D02G3/00; during formation of artificial filaments, threads, or the like D01D5/22; general aspects of chemical treatment D06M)
- D02J 13/00: Heating or cooling the yarn, thread, cord, rope, or the like, not specific to any one of the processes provided for in this subclass (heating, cooling or drying during spinning or twisting D01H; drying of yarns or the like, in general F26B)
- D04H 1/02: Cotton wool; Wadding
- D04H 1/435: Polyesters
- D04H 1/43828: {sheath-core}
- D04H 1/43838: {Ultrafine fibres, e.g. microfibres}
- D04H 1/43918: {nonlinear fibres, e.g. crimped or coiled fibres}
- D04H 1/5412: {sheath-core}
- D04H 1/5418: {Mixed fibres, e.g. at least two chemically different fibres or fibre blends}
- D04H 1/64: the bonding agent being applied in wet state, e.g. chemical agents in dispersions or solutions
- A41D 31/00: Materials specially adapted for outerwear
- A47C 17/86: Parts or details specially adapted for beds, sofas or couches not fully covered by any single one of groups A47C17/02 - A47C17/84
- D04H 1/43832: {side-by-side}
- D04H 1/5414: {side-by-side}
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- D02G: CRIMPING OR CURLING FIBRES, FILAMENTS, THREADS, OR YARNS; YARNS OR THREADS
- D02J: FINISHING OR DRESSING OF FILAMENTS, YARNS, THREADS, CORDS, ROPES OR THE LIKE (curling or crimping D02G; by treatment with liquids, gases or vapours D06B; finishing other than by liquid treatment, of yarns in warp or sheet form D06C; for chemical matters, see D06L, D06M, D06P, D06Q; treatment during rope-making, apparatus for treating ropes auxiliary to rope-making D07B)
- A41D: OUTERWEAR; PROTECTIVE GARMENTS; ACCESSORIES
- A47C: CHAIRS; SOFAS; BEDS

## Abstract

The invention provides migration resistant batting that includes a nonwoven web comprising a first surface parallel to a second surface, and a fiber mixture that includes: 35 to 65 wt % synthetic polymeric fibers having a denier of less than or equal to 1.0, wherein 50 to 100 wt % of said synthetic polymeric fibers are siliconized fibers; 10 to 30 wt % spiral-crimped synthetic polymeric fibers having a length of greater than or equal to 60 mm, wherein 50 to 100 wt % of said spiral-crimped synthetic polymeric fibers are siliconized fibers; 20 to 50 wt % elastomeric fibers having a denier between 2.0 and 7.0; and 5 to 25 wt % synthetic binder fibers having a denier of 1.5 to 4.0, said binder fibers have a bonding temperature lower than the softening temperature of the synthetic polymeric fibers, wherein said first and second surfaces comprise a cross-linked resin. Also provided are articles comprising the batting and methods of making the batting.

## Claims

### Claim 1

Batting comprising a bonded nonwoven web having a first surface parallel to a second surface, wherein said bonded nonwoven web comprises a fiber mixture having:
35 to 65 wt % of a first population of synthetic polymeric fibers having a denier between 0.7 and 1.0, wherein 50 to 100 wt % of said synthetic polymeric fibers are siliconized fibers, and wherein the first population of synthetic polymeric fibers have a length of 18 mm to 59 mm;
10 to 30 wt % of a second population of spiral-crimped synthetic polymeric fibers having a length of greater than or equal to 60 mm, wherein 50 to 100 wt % of said spiral-crimped synthetic polymeric fibers are siliconized fibers;
20 to 50 wt % elastomeric fibers having a denier between 2.0 and 7.0, wherein the elastomeric fibers have a length of 55 to 80 mm; and
12 to 25 wt % synthetic binder fibers having a denier of 1.5 to 4.0, said binder fibers have a bonding temperature lower than the softening temperature of the first population of synthetic polymeric fibers and the second population of spiral-crimped synthetic polymeric fibers, the bonding temperature being between 80° C. and 150°,
wherein fibers in the fiber mixture are homogenously mixed such that the fiber mixture has a 90-100% uniform composition, and wherein said first and second surfaces comprise a cross-linked resin.

### Claim 2 (depends on 1)

The batting according to claim 1, wherein the first population of synthetic polymeric fibers have a length of 18 mm to 51 mm.

### Claim 3 (depends on 1)

The batting according to claim 1, wherein the second population of spiral-crimped synthetic polymeric fibers have a length of 60 to 75 mm.

### Claim 4 (depends on 1)

The batting according to claim 1, wherein the elastomeric fibers have a length of 58 to 71 mm.

### Claim 5 (depends on 1)

The batting according to claim 1, wherein the synthetic binder fibers have a length of 20 mm to 71 mm.

### Claim 6 (depends on 1)

The batting according to claim 1, wherein the first population of synthetic polymeric fibers have a non-spiral crimp.

### Claim 7 (depends on 1)

The batting according to claim 1, wherein the fiber mixture comprises:
40 to 55 wt % of the first population of synthetic polymeric fibers, said fibers having a non-spiral crimp;
15 to 25 wt % of the second population of spiral-crimped synthetic polymeric fibers;
20 to 35 wt % of the elastomeric fibers; and
12 to 15 wt % of the synthetic binder fibers.

### Claim 8 (depends on 1)

The batting according to claim 1, wherein 75 to 100 wt % of the first population of synthetic polymeric fibers are siliconized fibers.

### Claim 9 (depends on 1)

The batting according to claim 1, wherein 75 to 100 wt % of the second population of spiral-crimped synthetic polymeric fibers are siliconized fibers.

### Claim 10 (depends on 1)

The batting according to claim 1, wherein the first population of synthetic polymeric fibers and the second population of spiral-crimped synthetic polymeric fibers are polyester fibers.

### Claim 11 (depends on 1)

The batting according to claim 1, wherein the cross-linked resin comprises a cross-linked acrylate (co)polymer.

### Claim 12 (depends on 1)

The batting according to claim 1, having a density of 5.0 to 7.5 kg/m3.

### Claim 13 (depends on 1)

The batting according to claim 1, having a thermal performance rating of at least 0.75 clo/oz/yd2 when tested according to ISO 11092.

### Claim 14 (depends on 1)

The batting according to claim 1, having a water uptake of less than or equal to 30 wt %.

### Claim 15 (depends on 1)

The batting according to claim 1, having multidirectional stretch of 10-20% in machine, cross, and diagonal directions, under a load of 0.65 lbs, when tested according to ASTM D3107.

### Claim 16 (depends on 1)

The batting according to claim 1, having a migration resistance rating of 5.

### Claim 17 (depends on 1)

An article comprising the batting according to claim 1.

### Claim 18 (depends on 17)

The article according to claim 17, wherein said article is selected from the group consisting of an outerwear product, clothing, a sleeping bag, and bedding.

### Claim 19 (depends on 1)

The batting according to claim 1, wherein the fiber mixture comprises 25 wt % to 50 wt % elastomeric fibers.

### Claim 20 (depends on 1)

A method of making the batting according to claim 1, said method comprising:
preparing a fiber mixture by mixing:
35 to 65 wt % of a first population of synthetic polymeric fibers having a denier between 0.7 and 1.0, wherein 50 to 100 wt % of said synthetic polymeric fibers are siliconized fibers, and wherein the first population of synthetic polymeric fibers have a length of 18 mm to 59 mm;
10 to 30 wt % of a second population of spiral-crimped synthetic polymeric fibers having a length of greater than or equal to 60 mm, wherein 50 to 100 wt % of said spiral-crimped synthetic polymeric fibers are siliconized fibers;
20 to 50 wt % elastomeric fibers having a denier between 2.0 and 7.0, wherein the elastomeric fibers have a length of 55 to 80 mm; and
12 to 25 wt % synthetic binder fibers having a denier of 1.5 to 4.0, said binder fibers have a bonding temperature lower than the softening temperature of the first population of synthetic polymeric fibers and the second population of spiral-crimped synthetic polymeric fibers, the bonding temperature being between 80° C. and 150°,
wherein fibers in the fiber mixture are homogenously mixed such that the fiber mixture has a 90-100% uniform composition;
forming a nonwoven web from the fiber mixture, said nonwoven web comprising a first surface parallel to a second surface;
heating the non-woven web to or in excess of the bonding temperature of the binder fibers, thereby forming a bonded nonwoven web;
applying a cross-linker solution comprising a cross-linker compound to the first and second surfaces of the bonded nonwoven web; and
heating the bonded nonwoven web to a temperature in excess of the glass transition temperature of the cross-linker compound, thereby forming the batting.

### Claim 21 (depends on 20)

The method according to claim 20, wherein the cross-linker compound has a glass transition temperature (Tg) of less than 0° C.

### Claim 22 (depends on 20)

The method according to claim 20, wherein the cross-linker compound comprises an acrylate (co)polymer.

### Claim 23 (depends on 20)

The method according to claim 20, wherein coagulation of the cross-linker solution is minimized prior to applying the cross-linker solution to the first and second surfaces of the nonwoven web.

### Claim 24 (depends on 20)

The method according to claim 20, wherein the applying the cross-linker solution comprises spraying the solution onto the first and second surfaces of the nonwoven web, and wherein, during spraying, spray drops of the solution have an average median diameter of 150 to 250 μm.

### Claim 25 (depends on 24)

The method according to claim 24, wherein drop surface area density of the crosslinker solution on the first and second surfaces of the nonwoven web is 7 to 8 g/m2.

### Claim 26 (depends on 20)

The method according to claim 20, wherein said heating the bonded nonwoven web comprises two or more steps, including:
heating in an oven; and
heating in a calendaring process.

### Claim 27 (depends on 26)

The method according to claim 26, wherein said heating in a calendaring process utilizes a temperature of 150 to 175° C., and wherein calendaring production line speeds to not exceed 5 meters per minute.

### Claim 28 (depends on 20)

The method according to claim 20, wherein the fiber mixture comprises 25 wt % to 50 wt % elastomeric fibers.