# US 10,954,606 B2 · Methods for modeling the impurity concentration of a single crystal silicon ingot

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,606 B2
- Document ID: US10954606B2
- Status: Granted
- Kind: B2
- Application number: 16/020,707
- Filed: 2018-06-27
- Published: 2020-01-02
- Granted: 2021-03-23
- Earliest claimed: 2018-06-27
- Assignees: GlobalWafers Co., Ltd.
- Applicants: Global Wafers Co., Ltd.
- Inventors: Carissima Marie Hudson; JaeWoo Ryu
- Web page: https://patentgrep.com/patent/US10954606B2

## CPC

- C30B 15/20: Controlling or regulating (controlling or regulating in general G05)
- C30B 15/10: Crucibles or containers for supporting the melt
- C30B 29/06: Silicon
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

Methods for forming single crystal silicon ingots in which plural sample rods are grown from the melt are disclosed. A parameter related to the impurity concentration of the melt or ingot is measured. In some embodiments, the sample rods each have a diameter less than the diameter of the product ingot.

## Claims

### Claim 1

A method for modeling the impurity concentration of a single crystal silicon ingot, the method comprising:
pulling a first sample rod from a silicon melt disposed in a crucible, the first sample rod having a first sample rod diameter of less than 100 mm;
measuring a first sample rod parameter related to the impurity content of the first sample rod, the first sample rod parameter being selected from the group consisting of the phosphorous concentration, boron concentration, aluminum concentration, gallium concentration, arsenic concentration, indium concentration, antimony concentration, total impurity concentration, dopant concentration, and resistivity of the first sample rod;
pulling a second sample rod from the silicon melt, the second sample rod having a first sample rod diameter of less than 100 mm;
measuring a second sample rod parameter related to the impurity content of the second sample rod, the second sample rod parameter being selected from the group consisting of the phosphorous concentration, boron concentration, aluminum concentration, gallium concentration, arsenic concentration, indium concentration, antimony concentration, total impurity concentration, dopant concentration, and resistivity of the second sample rod; and
determining the impurity concentration of a single crystal silicon ingot based at least in part on a rate of change in the difference between the measured first sample rod parameter and the measured second sample rod parameter.

### Claim 2 (depends on 1)

The method as set forth in claim 1 wherein the first sample rod parameter and the second sample rod parameter is the same parameter.

### Claim 3 (depends on 1)

The method as set forth in claim 1 wherein the first sample rod diameter and the second sample rod diameter is each less than about 50 mm.

### Claim 4 (depends on 1)

The method as set forth in claim 1 wherein the first sample rod diameter and the second sample rod diameter is each less than about 25 mm.

### Claim 5 (depends on 1)

The method as set forth in claim 1 wherein the first sample rod diameter and the second sample rod diameter from about 5 mm to about 100 mm.

### Claim 6 (depends on 1)

The method as set forth in claim 1 further comprising:
pulling a third, fourth, fifth, sixth, seventh, eighth, ninth and/or tenth sample rod from the melt, the diameter of each sample rod being less than about 100 mm; and
measuring a sample rod parameter related to the impurity content for each sample rod pulled from the melt.

### Claim 7 (depends on 1)

The method as set forth in claim 1 wherein the impurity concentration of a single crystal silicon ingot is determined from a model, the first sample rod parameter and the second sample rod parameter being input into the model.

### Claim 8 (depends on 1)

The method as set forth in claim 1 further comprising pulling a product ingot from the melt, the single crystal silicon ingot in which the impurity concentration is determined being the product ingot pulled from the melt.

### Claim 9 (depends on 1)

The method as set forth in claim 1 wherein the melt is a first melt, the method further comprising:
pulling a first product ingot from the first melt; and
pulling a second product ingot from a second melt, the single crystal silicon ingot in which the impurity concentration is determined being the second product ingot pulled from the second melt.

### Claim 10 (depends on 9)

The method as set forth in claim 9 wherein the diameter of the first and second sample rods are each less than 0.75 times the diameter of the product ingot.

### Claim 11 (depends on 1)

The method as set forth in claim 1 wherein the impurity concentration is an impurity concentration of a portion of the single crystal silicon ingot.

### Claim 12 (depends on 1)

The method as set forth in claim 1 wherein the impurity concentration is concentration of one or more impurities over the length of the single crystal silicon ingot.

### Claim 13 (depends on 1)

The method as set forth in claim 1 further comprising annealing each sample rod in a thermal donor kill cycle prior to measuring the first and second sample rod parameters.

### Claim 14 (depends on 13)

The method as set forth in claim 13 wherein the sample rods are annealed at a temperature of at least about 500° C.

### Claim 15 (depends on 14)

The method as set forth in claim 14 wherein a length of the anneal is at least about 5 seconds.

### Claim 16 (depends on 13)

The method as set forth in claim 13 wherein a length of the anneal is from about 5 seconds to about 5 minutes.

### Claim 17 (depends on 13)

The method as set forth in claim 13 further wherein the sample rod is annealed at a temperature of at least about 650° C.