# US 10,954,604 B2 · Methods and apparatuses for electroplating nickel using sulfur-free nickel anodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,604 B2
- Document ID: US10954604B2
- Status: Granted
- Kind: B2
- Application number: 15/641,053
- Filed: 2017-07-03
- Published: 2017-10-19
- Granted: 2021-03-23
- Earliest claimed: 2014-04-18
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Bryan L. Buckalew
- Web page: https://patentgrep.com/patent/US10954604B2

## CPC

- C25D 21/12: Process control or regulation (controlling or regulating in general G05)
- C25D 3/12: of nickel or cobalt
- C25D 7/123: {Semiconductors first coated with a seed layer or a conductive layer}
- C25D 17/001: {Apparatus specially adapted for electrolytic coating of wafers, e.g. semiconductors or solar cells}
- C25D 17/002: {Cell separation, e.g. membranes, diaphragms}
- C25D 17/10: Electrodes {, e.g. composition, counter electrode}
- C25D 21/04: Removal of gases or vapours {; Gas or pressure control}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Disclosed herein are systems and methods for electroplating nickel which employ substantially sulfur-free nickel anodes. The methods may include placing a semiconductor substrate in a cathode chamber of an electroplating cell having an anode chamber containing a substantially sulfur-free nickel anode, contacting an electrolyte solution having reduced oxygen concentration with the substantially sulfur-free nickel anode contained in the anode chamber, and electroplating nickel from the electrolyte solution onto the semiconductor substrate placed in the cathode chamber. The electroplating systems may include an electroplating cell having an anode chamber configured for holding a substantially sulfur-free nickel anode, a cathode chamber, and a substrate holder within the cathode chamber configured for holding a semiconductor substrate. The systems may also include an oxygen removal device arranged to reduce oxygen concentration in the electrolyte solution as it is flowed to the anode chamber.

## Claims

### Claim 1

An electroplating system for electroplating nickel onto a semiconductor substrate using a sulfur-free nickel anode, the system comprising:
an electroplating cell configured to hold an electrolyte solution during electroplating, the electroplating cell comprising:
a cathode chamber;
a substrate holder within the cathode chamber configured for holding the semiconductor substrate during electroplating;
an anode chamber comprising a sulfur-free nickel anode; and
a porous separator between the anode chamber and the cathode chamber permitting passage of ionic current during electroplating, but inhibiting the passage of electrolyte solution;
an oxygen removal device arranged to reduce oxygen concentration in the electrolyte solution as it is flowed to the anode chamber at least some during electroplating and at least some during idle times when the system is not electroplating; and
a pH sensor configured for measuring pH of the electrolyte solution.

### Claim 2 (depends on 1)

The system of claim 1, wherein the oxygen removal device is configured to reduce oxygen concentration of the electrolyte solution to about 1 PPM or less.

### Claim 3 (depends on 1)

The system of claim 1, wherein the oxygen removal device is configured to reduce oxygen concentration of the electrolyte solution to about 0.5 PPM or less.

### Claim 4 (depends on 1)

The system of claim 1, further comprising an oxygen sensor.

### Claim 5 (depends on 4)

The system of claim 4, wherein the system comprises a controller configured to reduce oxygen concentration in the electrolyte solution using the oxygen removal device prior to flowing the electrolyte solution into the anode chamber when the sensed oxygen concentration is more than about 1 PPM.

### Claim 6 (depends on 1)

The system of claim 1, wherein the system is configured for:
flowing the electrolyte solution to the cathode chamber;
wherein the oxygen concentration of the electrolyte solution flowed to the anode chamber is less than the oxygen concentration of the electrolyte solution flowed to the cathode chamber.

### Claim 7 (depends on 1)

The system of claim 1, wherein the oxygen removal device is a degasser.

### Claim 8 (depends on 1)

The system of claim 1, wherein the oxygen removal device is configured for reducing the oxygen concentration in the electrolyte solution by sparging the electrolyte solution with a gas substantially free of oxygen.

### Claim 9 (depends on 1)

The system of claim 1, wherein the system is configured for maintaining the electrolyte solution in the cathode chamber at a pH of between about 3.5 and 4.5 while electroplating nickel from the electrolyte solution onto the semiconductor substrate.

### Claim 10 (depends on 1)

The system of claim 1, further comprising a controller configured for:
sending an alert when sensed pH of the electrolyte solution is more than about 4.5.

### Claim 11 (depends on 1)

The system of claim 1, further comprising a controller configured for:
reducing oxygen concentration in the electrolyte solution prior to flowing it into the anode chamber when sensed pH of the electrolyte solution is more than about 4.5.

### Claim 12 (depends on 1)

The system of claim 1, wherein the porous separator is configured for maintaining a difference in oxygen concentration between the anode and cathode chambers.

### Claim 13 (depends on 12)

The system of claim 12, wherein the porous separator is a micro-porous membrane substantially free of ion exchange sites.

### Claim 14 (depends on 1)

The system of claim 1, wherein the system is configured for reducing oxygen concentration of the electrolyte solution during the idle time to a level such that the pH of the of electrolyte solution does not appreciably increase when contacting the sulfur-free nickel anode during idle time.

### Claim 15 (depends on 1)

The system of claim 1, wherein the concentration of sulfur in the sulfur-free nickel anode is about 0.0003% or less by weight.

### Claim 16 (depends on 1)

The electroplating system of claim 1, wherein the anode chamber further comprises a fluidic inlet configured for flowing electrolyte solution into the anode chamber at a flow rate of about 1 to 5 liters/min.