# US 10,954,588 B2 · Oxidation controlled twin wire arc spray materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,588 B2
- Document ID: US10954588B2
- Status: Granted
- Kind: B2
- Application number: 15/347,516
- Filed: 2016-11-09
- Published: 2017-05-11
- Granted: 2021-03-23
- Earliest claimed: 2015-11-10
- Assignees: Oerlikon Metco (US) Inc.
- Applicants: Scoperta, Inc.
- Inventors: Justin Lee Cheney; David Jiang
- Web page: https://patentgrep.com/patent/US10954588B2

## CPC

- C23C 4/08: containing only metal elements (C23C4/073 takes precedence)
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/18: containing chromium
- C22C 38/40: with nickel
- C23C 4/131: Wire arc spraying
- C23C 4/18: After-treatment
- C23C 8/02: Pretreatment of the material to be coated (C23C8/04 takes precedence)
- C23C 8/20: Carburising
- C23C 8/24: Nitriding
- C23C 8/30: Carbo-nitriding
- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Disclosed herein are embodiments of alloys which can be particularly advantageous in twin wire arc spray methods for coating of a substrate. In some embodiments, a plurality of alloys can be used to form both hard and soft particles on a surface. In some embodiments, chromium can be minimized or eliminated.

## Claims

### Claim 1

An iron-based cored wire alloy feedstock configured for twin wire arc thermal spray applications, the cored wire alloy feedstock comprising:
a powder and a sheath, wherein the powder and sheath combination have a composition comprising Fe and, in wt. %:
0<Al≤2.5;
Cr: about 10-15;
0<Mn≤2;
Ni: about 15-25; and
Si: about 2.97-5.

### Claim 2 (depends on 1)

The cored wire alloy feedstock of claim 1, wherein the cored wire alloy feedstock is configured to form the coating after oxidation in a twin wire arc thermal spray application.

### Claim 3 (depends on 1)

The cored wire alloy feedstock of claim 1, wherein the sheath has a diameter of 1/16″ and a ratio of the powder to the sheath is about 20-40% by weight.

### Claim 4 (depends on 1)

The cored wire alloy feedstock of claim 1, wherein the microhardness of the coating is 200 Vickers or below.

### Claim 5 (depends on 1)

The cored wire alloy feedstock of claim 1, wherein the microhardness of the coating is 100 Vickers or below.

### Claim 6 (depends on 1)

The cored wire alloy feedstock of claim 1, wherein the weighted solute fraction is less than 6 wt. % at a melting temperature of the cored wire alloy feedstock.

### Claim 7 (depends on 1)

The cored wire alloy feedstock of claim 1, wherein the weighted solute fraction of the coating is less than 2 wt. % at a melting temperature of the cored wire alloy feedstock.

### Claim 8 (depends on 1)

The cored wire alloy feedstock of claim 1, wherein the composition comprises Fe and, in wt. %:
Al: about 1.5;
Cr: about 11.27;
Mn: about 1.03;
Ni: about 20; and
Si: about 3.3.

### Claim 9 (depends on 1)

The cored wire alloy feedstock of claim 1, wherein the composition comprises Fe and, in wt. %:
Al about 1.5, C about 1, Mn about 1, Si about 3.25; or
Al about 1.5, Cr about 11.27, Mn about 1.03, Ni about 20, and Si about 3.3.

### Claim 10 (depends on 1)

The cored wire alloy feedstock of claim 1, wherein the austenite ferrite transition temperature is below about 950K.

### Claim 11 (depends on 1)

A twin wire arc spray process using the cored wire alloy feedstock of claim 1 as a cored wire alloy feedstock.

### Claim 12

An iron-based cored wire alloy feedstock configured for twin wire arc thermal spray applications, the cored wire alloy feedstock comprising:
a powder and a sheath, wherein the powder and sheath combination have a composition comprising at least 50 wt. % Fe and, in wt. %:
Al: 1.35-1.65;
Cr: 10-12.397;
Ni: 18-22; and
Si: about 2.97-3.63.

### Claim 13 (depends on 12)

The iron-based cored wire alloy feedstock of claim 12, wherein the sheath has a diameter of 1/16″ and a ratio of the powder to the sheath is about 20-40% by weight.

### Claim 14 (depends on 12)

The iron-based cored wire alloy feedstock of claim 12, wherein the composition comprises Fe and, in wt. %
Mn: 0.927-1.133.

### Claim 15 (depends on 12)

The iron-based cored wire alloy feedstock of claim 12, wherein the composition comprises Fe and, in wt. %:
Al about 1.5, C about 1, Mn about 1, Si about 3.25; or
Al about 1.5, Cr about 11.27, Mn about 1.03, Ni about 20, and Si about 3.3.