# US 10,954,580 B2 · Method for producing a high strength steel sheet having improved strength and formability, and obtained high strength steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,580 B2
- Document ID: US10954580B2
- Status: Granted
- Kind: B2
- Application number: 16/064,545
- Filed: 2016-12-21
- Published: 2019-01-03
- Granted: 2021-03-23
- Earliest claimed: 2015-12-21
- Assignees: ArcelorMittal
- Applicants: ArcelorMittal
- Inventors: Pavan Venkatasurya; Hyun Jo Jun
- Web page: https://patentgrep.com/patent/US10954580B2

## CPC

- C21D 9/46: for sheet metals
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0236: {Cold rolling}
- C21D 8/0247: characterised by the heat treatment
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- Y02P 10/20: Recycling
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing a steel sheet having a microstructure including 71% to 91% martensite and bainite, 9% to 13% retained austenite, and at most 20% ferrite is provided. The method includes providing a cold-rolled steel sheet including, in weight percent: 0.13%≤C≤0.22%, 1.2%≤Si≤2.3%, 0.02%≤Al≤1.0%, with 1.25%≤Si+Al≤2.35%, 2.4%≤Mn≤3%, Ti≤0.05%, Nb≤0.05% and a remainder of Fe and unavoidable impurities, annealing the steel sheet to obtain 80% to 100% austenite and 0% to 20% ferrite, quenching the steel sheet at a cooling rate between 20° C./s and 50° C./s to a quenching temperature between 240° C. and 310° C., heating the steel sheet to a partitioning temperature between 400° C. and 465° C. and maintaining the steel sheet at the partitioning temperature for 50 to 250 seconds, then immediately cooling the sheet to room temperature. Steel sheets are also provided.

## Claims

### Claim 1

A method for producing an uncoated steel sheet having a microstructure consisting of, in surface percentage, between 71% and 91% of a sum of martensite and bainite, between 9% and 13% retained austenite, and at most 20% ferrite, the method comprising the following successive steps:
providing a cold-rolled steel sheet, made of a steel having a chemical composition containing by weight:
0.13%≤C≤0.22%,
1.2%≤Si≤2.3%,
0.02%≤Al≤1.0%,
with 1.25%≤Si+Al≤2.35%,
2.4%≤Mn 3%,
Ti≤0.05%
Nb≤0.05%, and
a remainder, the remainder including Fe and unavoidable impurities;
annealing the steel sheet at an annealing temperature TA so as to obtain a structure comprising from 80% to 100% austenite and from 0% to 20% ferrite;
quenching the steel sheet at a cooling rate between 20° C./s and 50° C./s down to a quenching temperature QT between 240° C. and 270° C.;
heating the steel sheet up to a partitioning temperature PT between 440° C. and 460°;
maintaining the steel sheet at the partitioning temperature PT for a partitioning time Pt between 50 s and 250 s; and
immediately after the maintaining step, cooling the steel sheet down to room temperature,
wherein the retained austenite comprises blocky retained austenite having an aspect ratio between 2 and 4 and film-type retained austenite having an aspect ratio between 5 and 8,
the steel sheet having a yield strength between 850 and 1100 MPa, a tensile strength of at least 1180 MPa, a total elongation of at least 14% and a hole expansion ratio HER of at least 30%.

### Claim 2

A method for producing an uncoated steel sheet having a microstructure consisting of, in surface percentage, between 71% and 91% of a sum of martensite and bainite, between 9% and 13% retained austenite, and at most 20% ferrite, wherein the method comprises the following successive steps:
providing a cold-rolled steel sheet, made of a steel having a chemical composition containing by weight:
0.13%≤C≤0.22%,
1.2%≤Si≤2.3%,
0.02%≤Al≤1.0%,
with 1.25%≤Si+Al≤2.35%,
2.4%≤Mn 3%,
Ti≤0.05%,
Nb≤0.05%, and
a remainder, the remainder including Fe and unavoidable impurities;
annealing the steel sheet at an annealing temperature TA so as to obtain a structure comprising from 80% to 100% austenite and from 0% to 20% ferrite;
quenching the steel sheet at a cooling rate between 20° C./s and 50° C./s down to a quenching temperature QT between 290° C. and 320° C.;
heating the steel sheet up to a partitioning temperature PT between 400° C. and 425° C.;
maintaining the steel sheet at the partitioning temperature PT for a partitioning time Pt between 50 s and 250 s; and
immediately cooling the steel sheet down to room temperature,
wherein the retained austenite comprises blocky retained austenite having an aspect ratio between 2 and 4 and film-type retained austenite having an aspect ratio between 5 and 8,
the steel sheet having a yield strength between 850 and 1100 MPa, a tensile strength of at least 1180 MPa, a total elongation of at least 14% and a hole expansion ratio HER of at least 30%.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the step of providing the cold-rolled steel sheet comprises:
hot rolling a sheet made of said steel to obtain a hot rolled steel sheet;
coiling the hot-rolled steel sheet at a coiling temperature Tc between 500° C. and 730° C.; and
cold rolling the hot-rolled steel sheet to obtain the cold-rolled steel sheet.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the step of providing the cold-rolled steel sheet further comprises, between the coiling and the cold-rolling, performing a batch annealing at a batch annealing temperature between 500° C. and 650° C. for a batch annealing time between 300 seconds and 12 hours.

### Claim 5 (depends on 3)

The method according to claim 3, wherein the step of providing the cold-rolled steel sheet further comprises, between the coiling and the cold-rolling, performing a slow cooling of the hot-rolled steel sheet from the coiling temperature to a room temperature for a time between 5 and 7 days.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the steel sheet has, after the quenching and just before the heating to the partitioning temperature PT, a microstructure consisting of 10% and 40% austenite, between 60% and 90% martensite, and between 0% and 20% ferrite.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the chemical composition of the steel contains by weight:
0.13%≤C≤0.22%,
1.2%≤Si≤2.3%,
0.02%≤Al≤1.0%,
with 1.25%≤Si+Al≤2.35%,
2.4%≤Mn 3%,
Ti≤0.05%
Nb≤0.05%, and
a remainder, the remainder including Fe and unavoidable impurities;
and further satisfies at least one of the following conditions:
C≥0.16%;
C≤0.20%;
Si≥2.0%;
Si≤2.2%;
Mn≥2.6%; and
Mn≤2.8%.

### Claim 8 (depends on 1)

The method according to claim 1, wherein, after the steel sheet is quenched to the quenching temperature QT and before the steel sheet is heated to the partitioning temperature PT, the steel sheet is held at the quenching temperature QT for a holding time between 2 s and 8 s.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the partitioning time Pt is between 50 and 200 s.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the microstructure comprises between 5.5% and 10.5% of the film-type retained austenite.

### Claim 11

An uncoated steel sheet, wherein the uncoated steel sheet is made of a steel having a chemical composition containing by weight:
0.13%≤C≤0.22%,
1.2%≤Si≤2.3%,
0.02%≤Al≤1.0%,
with 1.25%≤Si+Al≤2.35%,
2.4%≤Mn 3%,
Ti≤0.05%,
Nb≤0.05%, and
a remainder, the remainder including Fe and unavoidable impurities;
the uncoated steel sheet having a microstructure consisting of, in surface percentage:
between 71% and 91% martensite and bainite;
between 9% and 13% retained austenite; and
at most 20% ferrite,
wherein the retained austenite comprises blocky retained austenite having an aspect ratio between 2 and 4 and film-type retained austenite having an aspect ratio between 5 and 8,
the uncoated steel sheet having a yield strength between 850 and 1100 MPa, a tensile strength of at least 1180 MPa, a total elongation of at least 14% and a hole expansion ratio HER of at least 30%.

### Claim 12 (depends on 11)

The uncoated steel sheet according to claim 11, wherein the hole expansion ratio HER is greater than 40%.

### Claim 13 (depends on 11)

The uncoated steel sheet according to claim 11, wherein the chemical composition of the steel contains by weight:
0.13%≤C≤0.22%,
1.2%≤Si≤2.3%,
0.02%≤Al≤1.0%,
with 1.25%≤Si+Al≤2.35%,
2.4%≤Mn 3%,
Ti≤0.05%,
Nb≤0.05%, and
a remainder, the remainder including Fe and unavoidable impurities;
and further satisfies at least one of the following conditions:
C≥0.16%;
C≤0.20%;
Si≥2.0%;
Si≤2.2%;
Mn≥2.6%; and
Mn≤2.8%.

### Claim 14 (depends on 11)

The uncoated steel sheet according to claim 11, wherein the retained austenite has a C content CRA% between 0.9% and 1.2%.

### Claim 15 (depends on 11)

The uncoated steel sheet according to claim 11, wherein the microstructure comprises between 5.5% and 10.5% of the film-type retained austenite.

### Claim 16

A steel sheet wherein the steel sheet is made of a steel having a chemical composition containing by weight:
0.13%≤C≤0.22%,
1.2%≤Si≤2.3%,
0.02%≤Al≤1.0%,
with 1.25%≤Si+Al≤2.35%,
2.4%≤Mn 3%,
Ti≤0.05%,
Nb≤0.05%, and
a remainder, the remainder including Fe and unavoidable impurities;
the steel sheet having a microstructure consisting of, in surface percentage:
between 71% and 91% martensite and bainite;
between 9% and 13% retained austenite; and
at most 20% ferrite,
wherein the retained austenite comprises blocky retained austenite having an aspect ratio between 2 and 4 and film-type retained austenite having an aspect ratio between 5 and 8,
the steel sheet having a yield strength between 850 and 1100 MPa, a tensile strength of at least 1180 MPa, a total elongation of at least 14% and a hole expansion ratio HER of at least 30%, and
the steel sheet being coated with a metallic coating fabricated by electroplating or vacuum deposition process.

### Claim 17 (depends on 16)

The steel sheet according to claim 16, wherein the hole expansion ratio HER is greater than 40%.

### Claim 18 (depends on 16)

The steel sheet according to claim 16, wherein the chemical composition of the steel contains by weight:
0.13%≤C≤0.22%,
1.2%≤Si≤2.3%,
0.02%≤Al≤1.0%,
with 1.25%≤Si+Al≤2.35%,
2.4%≤Mn 3%,
Ti≤0.05%,
Nb≤0.05%, and
a remainder, the remainder including Fe and unavoidable impurities;
and further satisfies at least one of the following conditions:
C≥0.16%;
C≤0.20%;
Si≥2.0%;
Si≤2.2%;
Mn≥2.6%; and
Mn≤2.8%.

### Claim 19 (depends on 16)

The steel sheet according to claim 16, wherein the retained austenite has a C content CRA% between 0.9% and 1.2%.

### Claim 20 (depends on 16)

The steel sheet according to claim 16, wherein the microstructure comprises between 5.5% and 10.5% of the film-type retained austenite.

### Claim 21 (depends on 2)

The method according to claim 2, wherein the step of providing the cold-rolled steel sheet comprises:
hot rolling a sheet made of said steel to obtain a hot rolled steel sheet;
coiling the hot-rolled steel sheet at a coiling temperature Tc between 500° C. and 730° C.; and
cold rolling the hot-rolled steel sheet to obtain the cold-rolled steel sheet.

### Claim 22 (depends on 21)

The method according to claim 21, wherein the step of providing the cold-rolled steel sheet further comprises, between the coiling and the cold-rolling, performing a batch annealing at a batch annealing temperature between 500° C. and 650° C. for a batch annealing time between 300 seconds and 12 hours.

### Claim 23 (depends on 21)

The method according to claim 21, wherein the step of providing the cold-rolled steel sheet further comprises, between the coiling and the cold-rolling, performing a slow cooling of the hot-rolled steel sheet from the coiling temperature to a room temperature for a time between 5 and 7 days.

### Claim 24 (depends on 2)

The method according to claim 2, wherein the steel sheet has, after the quenching and just before the heating to the partitioning temperature PT, a microstructure consisting of between 10% and 40% austenite, between 60% and 90% martensite, and between 0% and 20% ferrite.

### Claim 25 (depends on 2)

The method according to claim 2, wherein the chemical composition of the steel contains by weight:
0.13%≤C≤0.22%,
1.2%≤Si≤2.3%,
0.02%≤Al≤1.0%,
with 1.25%≤Si+Al≤2.35%,
2.4%≤Mn 3%,
Ti≤0.05%,
Nb≤0.05%, and
a remainder, the remainder including Fe and unavoidable impurities;
and further satisfies at least one of the following conditions:
C≥0.16%;
C≤0.20%;
Si≥2.0%;
Si≤2.2%;
Mn≥2.6%; and
Mn≤2.8%.

### Claim 26 (depends on 2)

The method according to claim 2, wherein, after the steel sheet is quenched to the quenching temperature QT and before the steel sheet is heated to the partitioning temperature PT, the steel sheet is held at the quenching temperature QT for a holding time between 2 s and 8 s.

### Claim 27 (depends on 2)

The method according to claim 2, wherein the partitioning time Pt is between 50 and 200 s.

### Claim 28 (depends on 2)

The method according to claim 2, wherein the microstructure comprises between 5.5% and 10.5% of the film-type retained austenite.