# US 10,954,579 B2 · Partial radiation heating method for producing press hardened parts and arrangement for such production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,579 B2
- Document ID: US10954579B2
- Status: Granted
- Kind: B2
- Application number: 15/769,302
- Filed: 2016-10-14
- Published: 2018-09-20
- Granted: 2021-03-23
- Earliest claimed: 2015-10-15
- Assignees: Automation, Press and Tooling, AP & T AB
- Applicants: Automation, Press and Tooling, AP & T AB
- Inventors: Martin Skrikerud; Christian Koroschetz; Kent Eriksson
- Web page: https://patentgrep.com/patent/US10954579B2

## CPC

- C21D 9/46: for sheet metals
- C21D 1/34: Methods of heating (C21D1/06 takes precedence)
- C21D 1/673: for die quenching
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0247: characterised by the heat treatment
- C21D 8/0294: involving a localised treatment
- F27D 11/12: with electromagnetic fields acting directly on the material being heated
- C21D 2221/00: Treating localised areas of an article
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE

## Abstract

The present invention relates to a method, and system for performing such method, for producing a press hardened part (2′) of heat treatable material having zones of different structure by partially heating a blank (2) before the blank is processed. The method (100) comprises the steps of arranging (104) the blank in a furnace (10) for heating the blank to a temperature equal to or above the austenitization temperature of the material of the blank to get the blank into an austenitic phase, in a IR heating station (10) partially heating (106), by means of IR radiation (24), at least one first zone (2a) of the blank thereby keeping the at least one first zone of the blank in the austenitic phase, and arranging (108) the blank in a processing unit (30) for forming and quenching the blank to a press hardened part.

## Claims

### Claim 1

A method for producing a press hardened part of heat treatable material having zones of different structure by partially heating a blank before the blank is processed, comprising the steps of;
arranging the blank in a furnace for heating the blank to a temperature equal to or above the austenitization temperature of the material of the blank to get the blank into an austenitic phase,
arranging the heated blank in an infrared (IR) heating station comprising IR radiation sources configured to provide IR radiation towards an upper side of the blank, wherein the blank is arranged on a support providing shielding of a bottom side of the blank such that the bottom side of the blank is substantially free from radiation exposure from the IR radiation,
arranging a mask made of stainless steel or aluminum between the IR radiation sources and the upper side of the blank, in parallel with the blank, to block IR radiation from reaching outside at least one first zone of the blank,
partially heating, by means of IR radiation, said at least one first zone of the blank thereby keeping the at least one first zone of the blank in the austenitic phase and letting a second zone of the blank, outside said at least one first zone, to cool below the austenitization temperature, and
arranging the blank in a processing unit for forming and quenching the blank to a press hardened part.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the mask is provided with one or more opening or recess for radiation to pass through to reach the blank.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the mask is arranged in direct contact with the blank.

### Claim 4 (depends on 3)

The method according to claim 3, wherein a plane upper surface of the blank is arranged in contact with a plane bottom surface of the mask.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the infrared radiation is in the spectral range between 0.7 and 3 μm.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the infrared radiation is in the near-infrared (NIR) spectrum having a wavelength between 0.8 and 1.5 μm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the blank is kept in the IR heating station for a time between 8 and 100 seconds, providing a cooling of the second zone of the blank to between 550° C. and 750° C. depending on the cooling speed.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the infrared radiation is in the spectral range between 0.7 and 2 μm.