# US 10,954,578 B2 · High-strength steel sheet and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,578 B2
- Document ID: US10954578B2
- Status: Granted
- Kind: B2
- Application number: 15/520,236
- Filed: 2015-10-29
- Published: 2017-11-02
- Granted: 2021-03-23
- Earliest claimed: 2014-10-30
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Yoshiyasu Kawasaki; Hiroshi Matsuda; Takeshi Yokota; Takako Yamashita; Kazuhiro Seto
- Web page: https://patentgrep.com/patent/US10954578B2

## CPC

- C21D 9/46: for sheet metals
- B32B 15/012: {one layer being formed of an iron alloy or steel, another layer being formed of aluminium or an aluminium alloy}
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/0278: involving a particular surface treatment (C21D8/0294 takes precedence)
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/28: with titanium or zirconium
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/024: {by cleaning or etching}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/12: Aluminium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/40: Plates; Strips
- C23G 1/00: Cleaning or pickling metallic material with solutions or molten salts (with organic solvents C23G5/02)
- C25D 3/22: of zinc
- B32B 2255/06: on metal layer
- B32B 2255/205: Metallic coating
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Disclosed is a steel sheet having a predetermined chemical composition and a steel microstructure that contains, in area ratio, 35% or more and 80% or less of polygonal ferrite and 5% or more and 25% or less of martensite, and that contains, in volume fraction, 8% or more of retained austenite, in which the polygonal ferrite, the martensite, and the retained austenite have a mean grain size of 6 μm or less, 3 μm or less, and 3 μm or less, respectively, and each have a mean grain aspect ratio of 2.0 or less, and in which a value obtained by dividing an Mn content in the retained austenite in mass % by an Mn content in the polygonal ferrite in mass % equals 2.0 or more.

## Claims

### Claim 1

A high-strength steel sheet comprising:
a chemical composition consisting of, in mass %, C: 0.030% or more and 0.250% or less, Si: 0.01% or more and 3.00% or less, Mn: 3.15% or more and 4.20% or less, P: 0.001% or more and 0.100% or less, S: 0.0001% or more and 0.0200% or less, N: 0.0005% or more and 0.0100% or less, Ti: 0.003% or more and 0.200% or less,
optionally at least one selected from the group consisting of Al: 0.01% or more and 2.00% or less, Nb: 0.005% or more and 0.200% or less, B: 0.0003% or more and 0.0050% or less, Ni: 0.005% or more and 1.000% or less, Cr: 0.005% or more and 1.000% or less, V: 0.005% or more and 0.500% or less, Mo: 0.005% or more and 1.000% or less, Cu: 0.005% or more and 1.000% or less, Sn: 0.002% or more and 0.200% or less, Sb: 0.002% or more and 0.200% or less, Ta: 0.001 or more and 0.010% or less, Ca: 0.0005% or more and 0.0050% or less, Mg: 0.0005% or more and 0.0050% or less, and REM: 0.0005% or more and 0.0050% or less, and
the balance consisting of Fe and incidental impurities; and
a steel microstructure that contains, in area ratio, 35% or more and 80% or less of polygonal ferrite and 5% or more and 25% or less of martensite, and that contains, in volume fraction, 12.7% or more of retained austenite,
wherein the polygonal ferrite has a mean grain size of 6 μm or less, the martensite has a mean grain size of 3 μm or less, the retained austenite has a mean grain size of 3 μm or less, and the polygonal ferrite, the martensite, and the retained austenite each have a mean grain aspect ratio of 2.0 or less, and
wherein a value obtained by dividing an Mn content in the retained austenite in mass % by an Mn content in the polygonal ferrite in mass % equals 2.0 or more; and
a tensile strength TS of 590 MPa to 860 MPa.

### Claim 2 (depends on 1)

The high-strength steel sheet according to claim 1, wherein the retained austenite has a C content that satisfies the following formula in relation to the Mn content in the retained austenite:
0.09*[Mn content]−0.130−0.140≤[C content]≤0.09*[Mn content]−0.130+0.140
where
[C content] is the C content in the retained austenite in mass %, and
[Mn content] is the Mn content in the retained austenite in mass %.

### Claim 3 (depends on 1)

The high-strength steel sheet according to claim 1, wherein when the steel sheet is subjected to tensile working with an elongation value of 10%, a value obtained by dividing a volume fraction of the retained austenite after the tensile working by a volume fraction of the retained austenite before the tensile working equals 0.3 or more.

### Claim 4 (depends on 1)

The high-strength steel sheet according to claim 1, wherein the steel sheet further comprises a hot-dip galvanized layer, a hot-dip aluminum-coated layer or an electrogalvanized layer.

### Claim 5 (depends on 1)

The high-strength steel sheet according to claim 1, wherein N content of the chemical composition is 0.0010% or more and 0.0070% or less.

### Claim 6 (depends on 1)

The high-strength steel sheet according to claim 1, wherein C content of the chemical composition is 0.080% or more and 0.200% or less.

### Claim 7 (depends on 6)

The high-strength steel sheet according to claim 6, wherein N content of the chemical composition is 0.0010% or more and 0.0070% or less.

### Claim 8 (depends on 1)

The high-strength steel sheet according to claim 1, wherein Mn content of the chemical composition is 3.62% or more and 4.20% or less.

### Claim 9 (depends on 8)

The high-strength steel sheet according to claim 8, wherein N content of the chemical composition is 0.0010% or more and 0.0070% or less.

### Claim 10 (depends on 8)

The high-strength steel sheet according to claim 8, wherein C content of the chemical composition is 0.080% or more and 0.200% or less.

### Claim 11 (depends on 10)

The high-strength steel sheet according to claim 10, wherein N content of the chemical composition is 0.0010% or more and 0.0070% or less.

### Claim 12 (depends on 1)

A method for manufacturing the high-strength steel sheet according to claim 1, the method comprising:
subjecting a steel slab having the chemical composition according to claim 1 to hot rolling whereby the steel slab is heated to 1100° C. or higher and 1300° C. or lower, hot rolled with a finisher delivery temperature of 750° C. or higher and 1000° C. or lower, and coiled at a mean coiling temperature of 300° C. or higher and 750° C. or lower to obtain a hot-rolled sheet;
subjecting the hot-rolled sheet to pickling to remove scales;
subjecting the hot-rolled sheet to hot band annealing whereby the hot-rolled sheet is retained in a temperature range of Ac1 transformation temperature+20° C. to Ac1 transformation temperature+120° C. for 600 s to 21,600 s;
subjecting the hot-rolled sheet to cold rolling whereby the hot-rolled sheet is cold rolled at a rolling reduction of 30% or more to obtain a cold-rolled sheet; and
subjecting the cold-rolled sheet to cold-rolled sheet annealing whereby the cold-rolled sheet is retained in a temperature range of Ac1 transformation temperature to Ac1 transformation temperature+100° C. for more than 900 s to 21,600 s or less, and subsequently cooled.

### Claim 13 (depends on 12)

The method according to claim 12, further comprising: after the cold-rolled sheet annealing, subjecting the cold-rolled sheet to any one of the following:
galvanizing treatment, or to hot-dip galvanizing treatment followed by alloying treatment in a temperature range of 450° C. or higher and 600° C. or lower,
hot-dip aluminum-coating treatment, or
electrogalvanizing treatment.