# US 10,954,383 B2 · Biofidelic skin simulant

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 10,954,383 B2
- Document ID: US10954383B2
- Status: Granted
- Kind: B2
- Application number: 15/940,098
- Filed: 2018-03-29
- Published: 2018-10-04
- Granted: 2021-03-23
- Earliest claimed: 2017-03-29
- Assignees: The Board of Trustees of The University of Alabama
- Applicants: The Board of Trustees of the University of Alabama
- Inventors: Arnab Chanda; Vinu Unnikrishnan; Zachary Flynn
- Web page: https://patentgrep.com/patent/US10954383B2

## CPC

- C08L 83/04: Polysiloxanes
- G09B 23/30: Anatomical models {(G09B23/281 - G09B23/288 take precedence)}
- C08G 77/12: containing silicon bound to hydrogen
- C08G 77/20: containing silicon bound to unsaturated aliphatic groups
- C08L 2203/02: for biomedical use
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- G09B: EDUCATIONAL OR DEMONSTRATION APPLIANCES; APPLIANCES FOR TEACHING, OR COMMUNICATING WITH, THE BLIND, DEAF OR MUTE; MODELS; PLANETARIA; GLOBES; MAPS; DIAGRAMS (devices for psychotechnics or for testing reaction times A61B5/16; games, sports, amusements A63; projectors, projector screens G03B)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Described are biofidelic skin simulants closely mimicking the biomechanical properties of natural human skin, including vaginal skin tissue. The simulant contains a crosslinked siloxane network.

## Claims

### Claim 1

A biofidelic skin simulant comprising a crosslinked siloxane network, wherein the skin simulant has a tensile strength from 1 to 30 MPa; and an elasticity modulus (E) (low stretch ratio) from 2 to 8 and an elasticity modulus (E) (high stretch ratio) from 6 to 90 MPa, wherein the low stretch elasticity modulus is less than the high stretch elasticity modulus,
wherein the tensile strength, elasticity modulus (E) (low stretch ratio) and elasticity modulus (E) (high stretch ratio) are measured at a strain rate of 0.012 s−1.

### Claim 2 (depends on 1)

The skin simulant according to claim 1, wherein the network comprises a first siloxane having a Shore Hardness of from 00-0 to 00-60, and a second siloxane having a Shore Hardness of from 10A to 40A.

### Claim 3 (depends on 2)

The skin simulant according to claim 2, wherein the first siioxane has a Shore Hardness of 00-0, 00-05, 00-10, or 00-15.

### Claim 4 (depends on 2)

The skin simulant according to claim 2, wherein the second siloxane has a Shore Hardness of 20A, 30A or 40A.

### Claim 5 (depends on 2)

The skin simulant according to claim 2, wherein the first siloxane is present in an amount of 2-20% by weight relative to the total weight of the crosslinked siloxane network.

### Claim 6 (depends on 2)

The skin simulant according to claim 2, wherein the first siloxane is present in an amount of 80-98% by weight relative to the total weight of the crosslinked siloxane network.

### Claim 7 (depends on 2)

The skin simulant according to claim 2, wherein the network comprises a first siloxane having a Shore Hardness of 00-10 which is present in an amount from 25-35% by weight, and a second siloxane having a Shore Hardness of 30A which is present in an amount from 65-75% by weight.

### Claim 8

A method for preparing a biofidelic skin simulant, comprising curing a combination of a first siloxane having a Shore Hardness of from 00-0 to 00-60 and a second siloxane having a Shore Hardness of from 20A to 40A in a mold, wherein the first and second siloxanes are different.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the first siloxane has a Shore Hardness of 00-0 or 00-10.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the second siloxane has a Shore Hardness of 30A.

### Claim 11 (depends on 8)

The method according to claim 8, wherein the first siloxane is present in an amount of 2-20% by weight relative to the total weight of the combination.

### Claim 12 (depends on 8)

The method according to claim 8, wherein the first siloxane is present in an amount of 80-98% by weight relative to the total weight of the combination.

### Claim 13 (depends on 8)

The method according to claim 8, wherein the combination comprises a first siloxane having a Shore Hardness of 00-10 which is present in an amount from 25-35% by weight, and a second siloxane having a Shore Hardness of 30A which is present in an amount from 65-75% by weight.

### Claim 14 (depends on 8)

The method according to claim 8, wherein the first siloxane has a Shore Hardness of 00-10, the second siloxane has a Shore Hardness of 30A, the first siloxane comprises 1-30% by weight of the combination, and the second siloxane comprises 70-99% by weight of the combination.

### Claim 15 (depends on 8)

The method according to claim 8, wherein the skin simulant is a vaginal skin simulant.